Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 81.0 µm/m-°C

@Temperature -40.0 - 95.0 °C
45.0 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
SABIC Innovative Plastics Lexan® 4704 PPC
High heat resistant polycarbonate copolymer, provides DTUL of 300F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with ..
CTE, linear, Parallel to Flow 81.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® OQ1022 PC
Standard Flow OQ Resin
CTE, linear, Parallel to Flow 81.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® OQ1022 PC (Asia Pacific)
Standard Flow OQ Resin
CTE, linear, Parallel to Flow 81.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® OQ1022 PC (Europe-Africa-Middle East)
Standard Flow OQ Resin
CTE, linear, Parallel to Flow 81.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® 303 PC (Asia Pacific)
Clear, high viscosity material designed to service severe environments of HID lighting.This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Parallel to Flow 81.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Noryl RF1132 PPE+PP
PPE+PP blend for high frequency applications. Good heat resistance and low DK.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 81.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® 195 PBT
PELLET FORM. For compounding only (not for injection molding). Unreinforced PBT. Melt viscosity between 740 and 900 poise. Natural Color (1001) Only.
CTE, linear, Parallel to Flow 81.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® 195HP PBT
PELLET FORM. For compounding only (not for injection molding). Unreinforced PBT. FDA 21CFR177.1660 compliant. Melt viscosity between 740 and 900 poise. Natural Color (1001) Only.
CTE, linear, Parallel to Flow 81.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® 215HPR PBT
Unreinforced PBT with mold release. FDA food contact compliant in limited colors. Effective March 2008 this grade will no longer be supported with biocompatibility data. Alternative grade Valox HX21..
CTE, linear, Parallel to Flow 81.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® 295 PBT
Unreinforced PBTThis data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 81.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® 310 PBT
Unreinforced, general purpose. Typical viscosity 5000-7000.
CTE, linear, Parallel to Flow 81.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® 310 PBT (Asia Pacific)
Unreinforced, general purpose. Typical viscosity 5000-7000.
CTE, linear, Parallel to Flow 81.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® 310HP PBT
PBT for compounding/fibers only. Not intended for injection molding. FDA compliant. Available in Natural color (1001) only.
CTE, linear, Parallel to Flow 81.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® 311 PBT
Unreinforced, improved resistance to UV. Medium viscosity.
CTE, linear, Parallel to Flow 81.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® 312 PBT
Unreinforced, For compounding only (not for injection molding), FDA (21 CFR 177.1660) compliant. Medium viscosity.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 81.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® 312 PBT (Asia Pacific)
Unreinforced, For compounding only (not for injection molding), Medium viscosity.
CTE, linear, Parallel to Flow 81.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® 315 PBT
Unreinforced, For extrusion/compounding only (not for injection molding). High viscosity. Melt viscosity between 7500 and 9500 poise.
CTE, linear, Parallel to Flow 81.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® 325 PBT
General purpose, unreinforced, improved processing. Applications like sprinklers and nozzles, pumps, door handle, tank covers, pens, pencils etc.
CTE, linear, Parallel to Flow 81.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® 325 PBT (Asia Pacific)
General purpose, unreinforced, improved processing. Applications like sprinklers and nozzles, pumps, door handle, tank covers, pens, pencils etc.
CTE, linear, Parallel to Flow 81.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Stat-kon PE002 PA 6
LNP* Stat-kon* PE002 is a compound based on Nylon 6 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americ..
CTE, linear, Parallel to Flow 81.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Stat-kon PE002 PA 6 (Asia Pacific)
LNP* Stat-kon* PE002 is a compound based on Nylon 6 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Asia P..
CTE, linear, Parallel to Flow 81.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL NH5120 PPE+PS
Noryl* NH5120 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated V1 flame re..
CTE, linear, Parallel to Flow 81.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL NH5120 PPE+PS
Noryl* NH5120 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated V1 flame re..
CTE, linear, Parallel to Flow 81.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
45.0 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics NORYL GTX GTX673 PPE+PA
Conductive Noryl GTX* resin designed for profile extrusion. This grade can be electrostatic or powder coat painted without the need for a primer. In addition, its high heat capability allows it to ..
CTE, linear, Parallel to Flow 81.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
45.0 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics NORYL GTX GTX674PC PPE+PA6
A conductive PPE/PA blend designed to have improved surface appearance and elevated heat resistance for powder coating. The material is suitable for injection molding. The material is only availab..
CTE, linear, Parallel to Flow 81.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
45.0 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics NORYL GTX GTX674PC PPE+PA6 (Europe-Africa-Middle East)
A conductive PPE/PA blend designed to have improved surface appearance and elevated heat resistance for powder coating. The material is suitable for injection molding. The material is only availab..