Polymer Property : CTE, linear, Parallel to Flow = 15.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature 23.0 - 150 °C
8.33 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM 2410EPR PEI (Asia Pacific)
40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing.
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature -40.0 - 150 °C
8.33 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics ULTEM 2410EPR PEI (Europe-Africa-Middle East)
40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. Resin is RoHS compliant. UL94 V0 listing.
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature -40.0 - 150 °C
8.33 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Asia Pacific)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature 100 - 200 °C
8.33 µin/in-°F

@Temperature 212 - 392 °F
2
Solvay Specialty Polymers Amodel® A-4133 HH Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® A-4133 HH is a 33% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation ..
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature 100 - 200 °C
8.33 µin/in-°F

@Temperature 212 - 392 °F
2
Solvay Specialty Polymers Amodel® AE-4133 Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® AE-4133 is a 33% glass reinforced, hot-water moldable polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Good Chemical Resistance; Good Cree..
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature 23.0 - 150 °C
8.33 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM HU2400 PEI
40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food..
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature -40.0 - 150 °C
8.33 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics ULTEM SF2350 PEI Blend
High flow Ultem blends for thin wall application
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature -40.0 - 150 °C
8.33 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics Ultem SF2350 PEI Blend (Europe-Africa-Middle East)
High flow Ultem blends for thin wall applicationThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
8.33 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON DEL22P PC
LNP STAT-KON* DEL22P is a compound based on Polycarbonate resin containing 10% Carbon Fiber, 10% PTFE. Added features of this material include: Electrically Conductive. Exceptional Processing, Wear..
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
8.33 µin/in-°F

@Temperature -58.0 - 122 °F
2
Solvay Specialty Polymers Ryton® BR111 Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® BR111 is a natural-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outstanding chemical..
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
8.33 µin/in-°F

@Temperature -58.0 - 122 °F
2
Solvay Specialty Polymers Ryton® BR111BL Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® BR111BL Ryton® BR111 is a black-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outs..
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
8.33 µin/in-°F

@Temperature -58.0 - 122 °F
2
Solvay Specialty Polymers Ryton® BR42B Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® BR42B 40% glass fiber reinforced polyphenylene sulfide compound is specially formulated to provide low coefficient of friction and reduced wear rate for use in applications requiring low s..
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature 100 - 200 °C
8.33 µin/in-°F

@Temperature 212 - 392 °F
2
Solvay Specialty Polymers Ryton® R-4-02 Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4 and R-4-02 40% glass fiber reinforced polyphenylene sulfide compounds provide a good combination of mechanical and electrical properties with outstanding chemical resistance, even at e..
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature 100 - 200 °C
8.33 µin/in-°F

@Temperature 212 - 392 °F
2
Solvay Specialty Polymers Ryton® R-4-220BL Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-220NA and R-4-220BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength after constant or repeated exposure to high temperature water.Featur..
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
8.33 µin/in-°F

@Temperature -58.0 - 122 °F
2
Solvay Specialty Polymers Ryton® R-4-230NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-230NA and R-4-230BL 40% glass fiber reinforced polyphenylene sulfide compounds provide reduced flash and improved processability compared to other polyphenylene sulfide injection moldi..
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature 100 - 200 °C
8.33 µin/in-°F

@Temperature 212 - 392 °F
2
Solvay Specialty Polymers Ryton® R-4-232NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-232NA 40% glass fiber reinforced polyphenylene sulfide compound complies with United States Food and Drug Administration (FDA) and European Union (EU 10/2011 and 1183/2012) regulations..
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
8.33 µin/in-°F

@Temperature -58.0 - 122 °F
2
Solvay Specialty Polymers Ryton® R-4-232NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-232NA 40% glass fiber reinforced polyphenylene sulfide compound complies with United States Food and Drug Administration (FDA) and European Union (EU 10/2011 and 1183/2012) regulations..
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature 100 - 200 °C
8.33 µin/in-°F

@Temperature 212 - 392 °F
2
Solvay Specialty Polymers Ryton® R-4-240NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-240NA and R-4-240BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and toughness compared to other polyphenylene sulfide compounds.Feat..
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
8.33 µin/in-°F

@Temperature -58.0 - 122 °F
2; ISO 11359-2
Solvay Specialty Polymers Ryton® R-4-280BL Polyphenylene Sulfide (PPS), Glass Fiber
Ryton® R-4-280BL 40% glass fiber reinforced polyphenylene sulfide compound provides a combination of enhanced mechanical strength and good flow for injection molding.Features: Good Chemical Resis..
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
8.33 µin/in-°F

@Temperature -58.0 - 122 °F
2
Solvay Specialty Polymers Ryton® R-7-120BL Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® R-7-120NA and R-7-120BL glass fiber and mineral filled polyphenylene sulfide compounds provide good strength and low maintenance molding using conventional molding equipment.Features: Good..
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature 100 - 200 °C
8.33 µin/in-°F

@Temperature 212 - 392 °F
2
Solvay Specialty Polymers Ryton® R-7-120NA Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® R-7-120NA and R-7-120BL glass fiber and mineral filled polyphenylene sulfide compounds provide good strength and low maintenance molding using conventional molding equipment.Features: Good..
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
8.33 µin/in-°F

@Temperature -58.0 - 122 °F
2
Solvay Specialty Polymers Ryton® R-7-120NA Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® R-7-120NA and R-7-120BL glass fiber and mineral filled polyphenylene sulfide compounds provide good strength and low maintenance molding using conventional molding equipment.Features: Good..
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature 100 - 200 °C
8.33 µin/in-°F

@Temperature 212 - 392 °F
2
Solvay Specialty Polymers Ryton® R-7-121BL Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin..
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
8.33 µin/in-°F

@Temperature -58.0 - 122 °F
2
Solvay Specialty Polymers Ryton® R-7-121BL Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin..
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature 100 - 200 °C
8.33 µin/in-°F

@Temperature 212 - 392 °F
2
Solvay Specialty Polymers Ryton® R-7-121NA Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin..
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
8.33 µin/in-°F

@Temperature -58.0 - 122 °F
2
Solvay Specialty Polymers Ryton® R-7-121NA Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin..
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature 100 - 200 °C
8.33 µin/in-°F

@Temperature 212 - 392 °F
2; ISO 11359-2
Solvay Specialty Polymers Ryton® R-7-190NA Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® R-7-190NA glass fiber and mineral filled polyphenylene sulfide compound provides enhanced strength and low maintenance molding using conventional molding equipment.Features: Good Chemical ..
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
8.33 µin/in-°F

@Temperature -58.0 - 122 °F
2
Solvay Specialty Polymers Ryton® R-4-220NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-220NA and R-4-220BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength after constant or repeated exposure to high temperature water.Featur..
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
8.33 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM HU2410 PEI (Asia Pacific)
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP..
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
8.33 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Ultem HU2410 PEI (Europe-Africa-Middle East)
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP..