Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Ryton® R-4-280BL Polyphenylene Sulfide (PPS), Glass Fiber

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Manufacturer Solvay Specialty Polymers
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Solvay Specialty Polymers Ryton® R-4-280BL Polyphenylene Sulfide (PPS), Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Ryton® R-4-280BL 40% glass fiber reinforced polyphenylene sulfide compound provides a combination of enhanced mechanical strength and good flow for injection molding.Features: Good Chemical Resistance; Good Processability; High StrengthAdditional Properties: Heat Deflection Temperature - ASTM D648 265 °C; Insulation Resistance - (90°C): 1.00E+12 ohm; Mold Shrinkage - 0.20 %; Mold Shrinkage - 0.50 %; Temperature Index - UL 746B 200 to 220 °CInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.68 g/cc
0.0607 lb/in³
ISO 1183
Water Absorption 0.020 %

@Time 86400 sec
0.020 %

@Time 24.0 hour
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength 195 MPa
28300 psi
ASTM D638
Elongation at Break 1.6 %
1.6 %
ASTM D638
Flexural Strength 280 MPa
40600 psi
ASTM D790
Flexural Modulus 14.0 GPa
2030 ksi
ISO 178
Compressive Strength 285 MPa
41300 psi
ASTM D695
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
Notch A; ISO 180
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
16.7 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 10.0 µm/m-°C

@Temperature 100 - 200 °C
5.56 µin/in-°F

@Temperature 212 - 392 °F
2; ISO 11359-2
15.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
8.33 µin/in-°F

@Temperature -58.0 - 122 °F
2; ISO 11359-2
CTE, linear, Transverse to Flow 40.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
22.2 µin/in-°F

@Temperature -58.0 - 122 °F
ISO 11359-2
90.0 µm/m-°C

@Temperature 100 - 200 °C
50.0 µin/in-°F

@Temperature 212 - 392 °F
ISO 11359-2
Thermal Conductivity 0.320 W/m-K
2.22 BTU-in/hr-ft²-°F
ISO 8302
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
5VA

@Thickness 1.60 mm
5VA

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Constant 3.9

@Frequency 1.00e+6 Hz
3.9

@Frequency 1.00e+6 Hz
ASTM D150
4.0

@Frequency 1000 Hz
4.0

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 22.0 kV/mm
559 kV/in
ASTM D149
Dissipation Factor 0.0020

@Frequency 1000 Hz
0.0020

@Frequency 1000 Hz
ASTM D150
0.0020

@Frequency 1.00e+6 Hz
0.0020

@Frequency 1.00e+6 Hz
ASTM D150
Arc Resistance 130 sec
130 sec
ASTM D495
Comparative Tracking Index 150 V
150 V
UL 746
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
Latin America
North America
Color Black
Form Pellets
RoHS Compliance RoHS Compliant