Thermal Properties | Metric | English | Comments |
---|---|---|---|
Hot Ball Pressure Test | <= 100 °C | <= 212 °F | IEC 60695-10-2 |
SABIC Innovative Plastics Cycolac® G360 ABS (Europe-Africa-Middle East) CYCOLAC G360 is a high flow, high impact, medium to high heat resistant injection moulding ABS grade. It is recommended for large or complex parts in the automotive or electrical power tool segments.. |
|||
Hot Ball Pressure Test | <= 100 °C | <= 212 °F | IEC 60695-10-2 |
SABIC Innovative Plastics Cycoloy® C1000 PC+ABS (Europe-Africa-Middle East) CYCOLOY C1000 is a PC+ABS blend developed with emphasis on excellent processing efficiency while maintaining good heat resistance and impact ductility. It is an excellent material choice for a wide .. |
|||
Hot Ball Pressure Test | <= 100 °C | <= 212 °F | IEC 60695-10-2 |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties |
|||
Hot Ball Pressure Test | <= 100 °C | <= 212 °F | IEC 60695-10-2 |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Europe-Africa-Middle East) CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of propertiesThis data was supplied by.. |
|||
Hot Ball Pressure Test | <= 100 °C | <= 212 °F | IEC 60695-10-2 |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties. |
|||
Hot Ball Pressure Test | <= 100 °C | <= 212 °F | IEC 60695-10-2 |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Asia Pacific) Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties. |
|||
Hot Ball Pressure Test | <= 100 °C | <= 212 °F | IEC 60695-10-2 |
SABIC Innovative Plastics Cycoloy® XCY620HS PC+ABS PC+ ABS General Purpose Non-FR |
|||
Hot Ball Pressure Test | <= 100 °C | <= 212 °F | IEC 60695-10-2 |
SABIC Innovative Plastics Cycoloy® XCY620S PC+ABS PC+ ABS Automotive applications |
|||
Hot Ball Pressure Test | <= 100 °C | <= 212 °F | IEC 60695-10-2 |
SABIC Innovative Plastics Cycoloy® XCY620S PC+ABS (Asia Pacific) PC+ ABS Automotive applications |
|||
Hot Ball Pressure Test | <= 100 °C | <= 212 °F | IEC 60695-10-2 |
SABIC Innovative Plastics Cycoloy® XCY620S PC+ABS (Europe-Africa-Middle East) PC+ ABS automotive applications, excellent flow/impact balance, high heat resistance temperature and excellent properties retention after hydrolytic and heat aging. |
|||
Hot Ball Pressure Test | <= 100 °C | <= 212 °F | IEC 60695-10-2 |
SABIC Innovative Plastics Cycolac® CRT3370 ABS (Europe-Africa-Middle East) CYCOLAC CRT3370 is a 17% glass reinforced injection moulding grade of ABS. It exhibits high rigidity and excellent dimensional stability combined with medium/high heat performance and good flow char.. |
|||
Hot Ball Pressure Test | <= 100 °C | <= 212 °F | IEC 60695-10-2 |
SABIC Innovative Plastics Cycoloy® C1000HF PC+ABS (Europe-Africa-Middle East) CYCOLOY C1000HF is a general purpose PC+ABS blend specially developed for thin wall applications requiring a high flow with a good balance of properties. It is suitable for applications in the autom.. |
|||
Hot Ball Pressure Test | <= 100 °C | <= 212 °F | IEC 60695-10-2 |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Europe-Africa-Middle East) Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties.This .. |
|||
Hot Ball Pressure Test | <= 100 °C | <= 212 °F | IEC 60695-10-2 |
SABIC Innovative Plastics Geloy XTPM302 ASA+PC (Europe-Africa-Middle East) XTPM302 is a general purpose ASA/PC injection moulding grade, available in various colors.Typical properties measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Mid.. |
|||
Hot Ball Pressure Test | <= 100 °C | <= 212 °F | IEC 60695-10-2 |
SABIC Innovative Plastics Lexan® DMX6014 PC Copolymer (Asia Pacific) DMX6014 is an injection moldable PC copolymer ABS blend. This resin combines excellent scratch resistance (F-pencil hardness) with ductility.This data was supplied by SABIC-IP for the Asia Pacific r.. |
|||
Hot Ball Pressure Test | <= 100 °C | <= 212 °F | IEC 60695-10-2 |
SABIC Innovative Plastics NORYL SE90 PPE+HIPS (Europe-Africa-Middle East) NORYL SE90 is an unfilled, flame retardant material with a Vicat B/120 of 110°C according ISO 306. NORYL SE90 is V1 at 1.6 mm according UL94 and halogen free according VDE/DIN 472 part 815. |
|||
Hot Ball Pressure Test | <= 100 °C | <= 212 °F | IEC 60695-10-2 |
SABIC Innovative Plastics LNP LUBRICOMP NL001 PC+ABS (Europe-Africa-Middle East) LNP LUBRICOMP* NL001 is a wear resistant PC+ABS blend, suitable for thin wall applications. |
|||
Hot Ball Pressure Test | >= 100 °C | >= 212 °F | BS 3456, IEC 335 |
EPICHEM Epiblend PC/ABS nero Polycarbonate/ABS |
|||
Hot Ball Pressure Test | >= 100 °C | >= 212 °F | BS 3456, IEC 335 |
EPICHEM Epilac T ABS Acrylonitrile Butadiene Styrene |
|||
Hot Ball Pressure Test | >= 100 °C | >= 212 °F | BS 3456, IEC 335 |
EPICHEM Epiryl PPO V0 Polyphenylene oxide Characteristics: self-extinguishing V0 at 1,6 mm |
|||
Hot Ball Pressure Test | >= 100 °C | >= 212 °F | BS 3456, IEC 335 |
EPICHEM Epiblend PC/ABS nero Polycarbonate/ABS Characteristics: Thermic resistant |
|||
Hot Ball Pressure Test | <= 100 °C | <= 212 °F | IEC 60695-10-2 |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Asia Pacific) CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties |
|||
Hot Ball Pressure Test | <= 100 °C | <= 212 °F | IEC 60695-10-2 |
SABIC Innovative Plastics Cycolac® CRT3370F ABS (Europe-Africa-Middle East) CYCOLAC CRT3370F is a 17% glass reinforced injection moulding grade of ABS. It exhibits high rigidity and excellent dimensional stability combined with medium/high heat performance and good flow cha.. |