Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 1400 °C | 2550 °F | |
Kennametal Stellite Hydroloy® HQ913® Information provided by Deloro Stellite, Inc. Typical data, not guaranteed as a maximum or minimum. Proprietary stainless steel with low Co and Mn contents, formulated to resist cavitation and dro.. |
|||
Solidus | 1400 °C | 2550 °F | |
Special Metals BRIGHTRAY® Alloy B Electrical Resistance Alloy A nickel-iron-chromium electrical-resistance alloy for use at operating temperatures up to 2010°F (1100°C). It contains rare-earth additions for increased oxidation resistance, especially und.. |
|||
Solidus | 1400 °C | 2550 °F | |
Special Metals BRIGHTRAY® Alloy S Electrical Resistance Alloy A nickel-chromium electrical-resistance alloy for use at temperatures up to 2100°F (1150°C) under continuous operating conditions. It is similar to BRIGHTRAY alloy C but does not contain rare.. |
|||
Solidus | 1400 °C | 2550 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed and Aged Rod and Bar Tensile strength (ultimate and yield), compressive strength, hardness, and elongation values reported here are typical for Annealed and Aged Rod and Bar specifically. Other property values are typic.. |
|||
Solidus | 1400 °C | 2550 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed and Aged Wire Tensile strength (ultimate) and elongation values reported here are typical for Annealed and Aged Wire specifically. Other property values are typical of aged DURANICKEL® alloy 301 or the alloy i.. |
|||
Solidus | 1400 °C | 2550 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed Rod and Bar Tensile strength (ultimate and yield), compressive strength, hardness, and elongation values reported here are typical for Annealed Rod and Bar specifically. Other property values are typical of ann.. |
|||
Solidus | 1400 °C | 2550 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed Strip Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Annealed Strip specifically. Other property values are typical of annealed DURANICKEL® alloy 3.. |
|||
Solidus | 1400 °C | 2550 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Cold-Drawn and Aged Rod and Bar Tensile strength (ultimate and yield), compressive strength, hardness, and elongation values reported here are typical for Cold-Drawn and Aged Rod and Bar specifically. Other property values are typ.. |
|||
Solidus | 1400 °C | 2550 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Cold-Drawn Rod and Bar Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Cold-Drawn Rod and Bar specifically. Other property values are typical of annealed DURANICKEL®.. |
|||
Solidus | 1400 °C | 2550 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Half-Hard Strip Tensile strength (ultimate), hardness, and elongation values reported here are typical for Half-Hard Strip specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the.. |
|||
Solidus | 1400 °C | 2550 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Hot-Finished and Aged Rod and Bar Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Hot-Finished and Aged Rod and Bar specifically. Other property values are typical of aged DURANIC.. |
|||
Solidus | 1400 °C | 2550 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Hot-Finished Rod and Bar Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Hot-Finished Rod and Bar specifically. Other property values are typical of annealed DURANICKELÂ.. |
|||
Solidus | 1400 °C | 2550 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Spring Strip Tensile strength (ultimate), hardness, and elongation values reported here are typical for Spring Strip specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the al.. |
|||
Solidus | 1400 °C | 2550 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Spring Strip, Aged Tensile strength (ultimate), hardness, and elongation values reported here are typical for Spring Strip, Aged specifically. Other property values are typical of aged DURANICKEL® alloy 301 or the .. |
|||
Solidus | 1400 °C | 2550 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Spring Wire Tensile strength (ultimate) and elongation values reported here are typical for Spring Wire specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the alloy in gener.. |
|||
Solidus | 1400 °C | 2550 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Spring Wire, Aged Tensile strength (ultimate) and elongation values reported here are typical for Spring Wire, Aged specifically. Other property values are typical of aged DURANICKEL® alloy 301 or the alloy in gen.. |
|||
Solidus | 1400 °C | 2550 °F | |
Goodfellow Iron 55/Nickel 45 Alloy Low Nickel magnetic alloy. Most applications are based on the requirements of moderately high saturation and permeabilities greater than silicon irons. Uses include the manufacture of sensitive rela.. |
|||
Solidus | 1400 °C | 2550 °F | |
Crucible Steel 303 Plus Chromium-Nickel Steel Crucible 303 Plus is a non-hardenable austenitic chromium-nickel steel to which elements have been added to improve machinability and non-galling characteristics. Better machinability than that of.. |
|||
Solidus | 1400 °C | 2550 °F | |
Crucible Steel 303 SE Chromium-Nickel Steel Crucible 303 SE is a non-hardenable austenitic chromium-nickel steel to which selenium has been added to improve machinability and non-galling characteristics. This grade is non-magnetic in the anne.. |
|||
Solidus | 1400 °C | 2550 °F | |
ATI Allegheny Ludlum Stainless Steel Type 201, 10% Cold Work (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
Solidus | 1400 °C | 2550 °F | |
ATI Allegheny Ludlum Stainless Steel Type 201, 40% Cold Work (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
Solidus | 1400 °C | 2550 °F | |
ATI Allegheny Ludlum Stainless Steel Type 201, 5% Cold Work (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
Solidus | 1400 °C | 2550 °F | |
ATI Allegheny Ludlum Stainless Steel Type 201, 60% Cold Work (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
Solidus | 1400 °C | 2550 °F | |
ATI Allegheny Ludlum Stainless Steel Type 201L, 10% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |
|||
Solidus | 1400 °C | 2550 °F | |
ATI Allegheny Ludlum Stainless Steel Type 201L, 5% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |
|||
Solidus | 1400 °C | 2550 °F | |
ATI Allegheny Ludlum Stainless Steel Type 201L, Annealed (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |
|||
Solidus | 1400 °C | 2550 °F | |
ATI Allegheny Ludlum Stainless Steel Type 201, 30% Cold Work (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
Solidus | 1400 °C | 2550 °F | |
ATI Allegheny Ludlum Stainless Steel Type 201, Annealed (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
Solidus | 1400 °C | 2550 °F | |
ATI Allegheny Ludlum Stainless Steel Type 201L, 30% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |
|||
Solidus | 1400 °C | 2550 °F | |
ATI Allegheny Ludlum Stainless Steel Type 201L, 40% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |