Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 148 °C @Load 1.00 kg |
298 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PP CQX30030 RTX Polypropylene, Mineral Reinforced, Scratch Resistant Information provided by Polykemi AB |
|||
Vicat Softening Point | 148 °C @Load 1.00 kg |
298 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PP CQX8025 R2 Polypropylene, Mineral Reinforced, Scratch Resistant Information provided by Polykemi AB |
|||
Vicat Softening Point | 148 °C @Load 1.00 kg |
298 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PP HGX500707 Polypropylene, Multifiller Information provided by Polykemi AB |
|||
Vicat Softening Point | 148 °C @Load 1.00 kg |
298 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH T15040CR Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 148 °C @Load 1.00 kg |
298 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH T20020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 148 °C @Load 1.00 kg |
298 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH T2020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 148 °C @Load 1.00 kg |
298 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH T4020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 148 °C @Load 1.00 kg |
298 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH T8040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 148 °C @Load 1.00 kg |
298 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYlux 104 HF PC/PBT-Blend, High Flow Information provided by Polykemi AB |
|||
Vicat Softening Point | 148 °C @Load 5.001 kg |
298 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB SCANBLEND P AP2060 F30 PBT/ASA, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 148 °C @Load 1.00 kg |
298 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH T1040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 148 °C @Load 1.00 kg |
298 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH T15020 H4 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 148 °C @Load 1.00 kg |
298 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH T5020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 148 °C @Load 1.02 kg |
298 °F @Load 2.25 lb |
50°C per hour; ISO 306 |
Total PPC 10641 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 10641 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 44 g/10 min.Polypropylene PPC 10641 is characterized by high fluidity with good mechanical prope.. |
|||
Vicat Softening Point | 148 °C @Load 1.02 kg |
298 °F @Load 2.25 lb |
50°C per hour; ISO 306 |
Total PPC 12642 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 12642 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 70 g/10 min and good mechanical properties.Polypropylene PPC 10641 has been developed for high s.. |
|||
Vicat Softening Point | 148 °C @Load 1.02 kg |
298 °F @Load 2.25 lb |
50°C per hour; ISO 306 |
Total PPM H250 Polypropylene, Homopolymer Medical Grade Polypropylene PPM H250 is a narrow molecular weight distribution homopolymer with a Melt Flow Index of 25 g/10 min recommended for the manufacture of medical packaging and medical devices, to the ex.. |
|||
Vicat Softening Point | 148 °C @Load 0.999 kg |
298 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTABLEND 4501 V0/D Flame Retardant PC - ABS PC - ABS BlendFlame retardant class V0, PBDE and antimony free, with halogens, high impact resistance, very high thermal resistance, high gloss, good processabilityInformation provided by Cossa Poli.. |
|||
Vicat Softening Point | 148 °C @Load 0.999 kg |
298 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTACARB 1560 V0 Flame Retardant Polycarbonate Flame retardant class V0, antimony and PBDE free, opaque, high melt flow, high impact strength, high thermal resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 148 °C @Load 0.999 kg |
298 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTACARB 2060 V0 Flame Retardant Polycarbonate Flame retardant class V0, antimony and PBDE free, opaque, high melt flow, high impact strength, high thermal resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 148 °C @Load 5.10 kg |
298 °F @Load 11.2 lb |
120°C/h; ISO 306 |
Covestro Makrolon® 2400 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Vicat Softening Point | 148 °C @Load 5.10 kg |
298 °F @Load 11.2 lb |
120°C/h; ISO 306 |
Covestro Makrolon® 2408 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
Vicat Softening Point | 148 °C @Load 5.10 kg |
298 °F @Load 11.2 lb |
120°C/h; ISO 306 |
Covestro Makrolon® 2800 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Vicat Softening Point | 148 °C @Load 5.10 kg |
298 °F @Load 11.2 lb |
120°C/h; ISO 306 |
Covestro Makrolon® 3152 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•.. |
|||
Vicat Softening Point | 148 °C @Load 5.10 kg |
298 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Covestro Makrolon® 3258 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
Vicat Softening Point | 148 °C @Load 1.00 kg |
298 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
Chi Mei Wonderlite® PC-108U Polycarbonate - UV Stabilized UV Stabilized |
|||
Vicat Softening Point | 148 °C @Load 1.00 kg |
298 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
Chi Mei Wonderlite® PC-122U Polycarbonate - UV Stabilized UV Stabilized |
|||
Vicat Softening Point | 148 °C @Load 1.00 kg |
298 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH T20040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 148 °C @Load 1.00 kg |
298 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH T5038 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 148 °C @Load 1.00 kg |
298 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH T5040DS Polypropylene Homopolymer, Mineral Reinforced, Detergent Resistant Information provided by Polykemi AB |
|||
Vicat Softening Point | 148 °C @Load 1.00 kg |
298 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH T8030 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |