Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 99.0 °C @Load 1.02 kg |
210 °F @Load 2.25 lb |
ISO 306/A 120 |
Polimeri Europa Sinkral® PD L 322 ABS Resin Sinkral PD L 322 by continuous mass, is a general purpose, high flow injection molding grade having good impact resistance coupled with an excellent gloss.Applications: Widely used in the small and.. |
|||
Vicat Softening Point | 99.0 °C @Load 5.001 kg |
210 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH 150DNH Polypropylene Homopolymer, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
Vicat Softening Point | 99.0 °C @Load 1.02 kg |
210 °F @Load 2.25 lb |
50°C per hour; ISO 306A50 |
Total Polystyrene Impact 8260 Improved Environmental Stress Crack Resistance High Impact Polystyrene POLYSTYRENE IMPACT 8260 is a high impact polystyrene for extrusion and injection applications. This grade has an improved environmental stress crack resistance in comparison with standard high impa.. |
|||
Vicat Softening Point | 99.0 °C @Load 0.999 kg |
210 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTASTIR HI 0408 V0 Flame Retardant Polystyrene Flame retardant class V0, PBDE free, good impact resistance, good thermal resistance, high light resistance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 99.0 °C @Load 0.999 kg |
210 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTASTIR HI 0508 V0 Flame Retardant Polystyrene Flame retardant class V0, PBDE free, good impact resistance, good thermal resistance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 99.0 °C @Load 0.999 kg |
210 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTASTIR HI 10 V0 Flame Retardant Polystyrene Flame retardant class V0, with PBDE, for injection molding or extrusionInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 99.0 °C @Load 5.00 kg |
210 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
Chi Mei Polylac® PA-717C ABS Medium impact |
|||
Vicat Softening Point | 99.0 °C @Load 1.00 kg |
210 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
Chi Mei Polylac® PA-737 ABS - High Flow High flow, medium impact |
|||
Vicat Softening Point | 99.0 °C @Load 5.00 kg |
210 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
Chi Mei Polyrex® PH-60 Polystyrene - High Impact Medium impact |
|||
Vicat Softening Point | 99.0 °C @Load 1.00 kg |
210 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
Chi Mei Kibiton® PB-5900 Styrene-Butadiene Copolymer Injection Molding, High rigidity |
|||
Vicat Softening Point | 99.0 °C @Load 1.00 kg |
210 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
Chi Mei Polylac® PA-764 ABS - Flame Retardant F.R. Weather Resistant |
|||
Vicat Softening Point | 99.0 °C @Load 1.00 kg |
210 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
Chi Mei Polylac® PA-764B ABS - Flame Retardant F.R. Weather Resistant |
|||
Vicat Softening Point | 99.0 °C @Load 1.00 kg |
210 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
Chi Mei Polylac® PA-764B ABS - Flame Retardant F.R. Weather Resistant |
|||
Vicat Softening Point | 99.0 °C @Load 5.00 kg |
210 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
Chi Mei Wonderloy® PC-540 PC/ABS Alloy - Flame Retardant High Heat |