Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 250 °C | 482 °F | Recommended |
Nye Lubricants UniFlor 8771R (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
Precision Polymer Engineering S40H Silicone Rubber White Silicone Rubber, 35-45 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Formulated using only those ingredients determined by the United States F.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
Precision Polymer Engineering S60K Silicone Rubber Silicone Rubber, 56-65 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Formulated using only those ingredients determined by the United States Federal.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
Precision Polymer Engineering S60N Silicone Rubber Red Silicone Rubber, 56-65 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. To meet UK Ministry of Defence Aircraft Materials Specification DTD5582A Gr.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
Precision Polymer Engineering S70Z Silicone Rubber Grey Silicone Rubber, 66-75 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Formulated using only those ingredients determined by the United States Fe.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
Precision Polymer Engineering S80Y Silicone Rubber Yellow Silicone Rubber, 76-85 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applications: Excellent heat resistance and.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | Continuous use |
Pyrotek NAD-250 Structural Insulation Board NAD-250 is a general purpose cement board. It is suitable for low-voltage electrical insulation in dry conditions.ApplicationsOven shelves Platen insulators Coil boxes Foundry core plates Heat guar.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | Continuous |
Quadrant EPP Duratron® PAI T4501 PAI + graphite + PTFE, compression moulded (ISO Data) Compression moulded Duratron T4501 PAI is similar in composition to Duratron T4301 PAI, and is selected when larger shapes are required Very high maximum allowable service temperature in air (250°C.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | Continuous |
Quadrant EPP Symalit® 1000 PFA unfilled, lining industries (ISO Data) Symalit 1000 PFA is made from a fluoropolymer resin that is a copolymer of tetrafluoroethylene and perfluorovinylether. It exhibits good mechanical properties combined with excellent electrical prop.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
Lehmann & Voss LUVOCOM® 1105-7185 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
Lehmann & Voss LUVOCOM® 1105-7568/GY PEEK, with PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Superheated steam sterilizable.High chemical resistance parts, hydrolysis resistance, non .. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
Lehmann & Voss LUVOCOM® 1105-8135/VI PEEK, unreinforced, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
Lehmann & Voss LUVOCOM® 1105-8417 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | short term |
Lehmann & Voss LUVOCOM® 21-8015 Polyamide 6/6T, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
Lehmann & Voss LUVOCOM® 1105/BK7308 PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Suitable for biocompatible application.Not f.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
Lehmann & Voss LUVOCOM® 1105/GN7348 PEEK, unreinforced, laser markable Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Not flammable.Especially suitable for medica.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
Lehmann & Voss LUVOCOM® 1105-0923/GY2 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
Lehmann & Voss LUVOCOM® 1105-7141 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Chemical and hydrolys.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
Lehmann & Voss LUVOCOM® 1105-7876-1 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Low warpage.Emergency running property.Information provided by Lehmann.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
Lehmann & Voss LUVOCOM® 1105/TF/20/BN PEEK, with PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | Continuous Use |
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | short term; EMS |
EMS-Grivory Grivory® HTV-3H1 black 9205 PA6T/6I-GF30 Product description: Grivory HTV-3H1 black 9205 is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I... |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | short term; EMS |
EMS-Grivory Grivory® HTV-45H1 black 9205 PA6T/6I-GF45 Product description: Grivory HTV-45H1 black 9205 is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation a.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | Continuous |
Epoxy Technology EPO-TEK® 431 Copper Filled Epoxy A two component, copper-filled, electrically and thermally conductive epoxy for adhesive bonding in electronics. It may be used at the PCB level for interconnecting, grounding and EMI RF shielding... |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | Intermittent |
Epoxy Technology EPO-TEK® 730 Unfilled Black General and Structural Grade Epoxy Material Description: A two component, room temperature curing, general and structural grade epoxy. It can be used for adhesive, sealing, and encapsulating applications in medical, xray device, fil.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | Continuous |
Epoxy Technology EPO-TEK® E2036 Epoxy Product Description: A two component, slightly flexible, silver-filled, electrically conductive adhesive for semiconductor and electronic assemblies. It is a low Tg epoxy, intended for many kinds o.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | short term; EMS |
EMS-Grivory Grivory® XE 4216 black 9233 PA6T/66-GF30 Product description: Grivory XE 4216 black 9233 is a high heat stabilized, 30% glass fiber reinforced, semicrystalline, thermoplastic engineering material for injection molding. Polymer designation .. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
BASF Ultramid® KR 4350 BK 00464 PA6/6T (Dry) Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
Lehmann & Voss LUVOCOM® 1105-7096 PEEK, with carbon fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
Lehmann & Voss LUVOCOM® 1105-7251 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera.. |