Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 232 °C | 450 °F | |
Arlon A3020-R004-12 0.020" (0.508 mm) Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate
  1 inch width and 36 inches long. Design/Construction: Side 1: Cured Fusible Silicone Rubber Substrate: 25% sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester Film Prod.. |
|||
Maximum Service Temperature, Air | 232 °C | 450 °F | |
Arlon R36772R008 0.008" (0.203 mm) Fully Cured, Unsupported, Silicone Rubber with Fiberglass Substrate
( Design/Construction:Side 1: Fully Cured, Unsupported, Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, material .. |
|||
Maximum Service Temperature, Air | 232 °C | 450 °F | |
Master Bond EP13 High Temperature Resistant One Component Epoxy System Master Bond Polymer System EP13 is a one component heat curing epoxy featuring high shear strength and very high temperature resistance. EP13 forms rigid and dimensionally stable bonds with minimal .. |
|||
Maximum Service Temperature, Air | 232 °C | 450 °F | |
Master Bond Supreme 45HTND Toughened Epoxy for Structural Bonding Description: Master Bond Polymer Adhesive SUPREME 45HTND is a two component epoxy adhesive featuring a balance of shear and peel strengths for high performance structural bonding suitable for applic.. |
|||
Maximum Service Temperature, Air | 232 °C | 450 °F | |
Master Bond EP34 Room Temperature Curing Two Component Epoxy System Master Bond Polymer System EP34 is a unique room temperature curing two component epoxy compound for high temperature potting and encapsulating applications. Adhesion to metals, glass, ceramics, woo.. |
|||
Maximum Service Temperature, Air | 232 °C | 450 °F | |
Arlon 19146R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1523 FiberglassSide 2: Uncured Silicone RubberInterleave: PolyethyleneAppearance: Black silicone gum and rubber on fiberglass clothT.. |
|||
Maximum Service Temperature, Air | 232 °C | 450 °F | |
Arlon 30560R015 0.015" (0.381 mm) Uncured/Unsupported Silicone Rubber on a Release Carrier Design/Construction:Side 1: Uncured/Unsupported Silicone Rubber on a Release Carrier Appearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The.. |
|||
Maximum Service Temperature, Air | 232 °C | 450 °F | |
Arlon 32580R020 0.020" (0.508 mm) Uncured Silicone Rubber on Polyester Film Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmAppearance: Red silicone gum on polymer linerThis data represents typical values for the production.. |
|||
Maximum Service Temperature, Air | 232 °C | 450 °F | |
Arlon 51576B015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone RubberInterleave: Polyethylene This data represents typical values for the production mate.. |
|||
Maximum Service Temperature, Air | 232 °C | 450 °F | |
Arlon 55572R030 0.030" (0.762 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Appearance: Red silicone rubber on fiberglass clothThis data Represents typical values for the production material. T.. |
|||
Maximum Service Temperature, Air | 232 °C | 450 °F | |
Arlon 55759R028 0.029" (0.737 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 162 Style Fiberglass This data represents typical values for the production ma.. |
|||
Maximum Service Temperature, Air | 232 °C | 450 °F | |
Arlon 56596R045 0.045" (1.14 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone RubberProduct Use: Flexible heater insulationAppearance: Red silicone gum and rubber on fiberglass with polymer release lin.. |
|||
Maximum Service Temperature, Air | 232 °C | 450 °F | |
Arlon 70011B016 0.016" (0.406 mm) Uncured Silicone Rubber with Prime Coated Polyester Fabric Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Maximum Service Temperature, Air | 232 °C | 450 °F | |
Arlon CP-310G Bulk Compound Appearance: Green silicone gumThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by A.. |
|||
Maximum Service Temperature, Air | 232 °C | 450 °F | |
Arlon R34172W008 0.008" (0.203 mm) Cured, Unsupported Silicone Rubber on a Mylar Carrier Design/Construction:Side 1: Cured, Unsupported Silicone Rubber on a Mylar Carrier This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Maximum Service Temperature, Air | 232 °C | 450 °F | |
Arlon 49100R010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 1681 FiberglassProduct Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass fabricTh.. |
|||
Maximum Service Temperature, Air | 232 °C | 450 °F | |
Arlon 51268R020P 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured Silicone RubberThickness:Side 1: Skim CoatSide 2: Skim Coat + 0.010" uncuredThis data Represents typical values for the product.. |
|||
Maximum Service Temperature, Air | 232 °C | 450 °F | |
Arlon 51976R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothThis data Represents typical values for the production mat.. |
|||
Maximum Service Temperature, Air | 232 °C | 450 °F | |
Arlon 55149R062 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Layer 2: uncured silicone rubber; Layer 1: cured silicone rubber; Substrate: 162 fiberglass |
|||
Maximum Service Temperature, Air | 232 °C | 450 °F | |
Arlon 55273R060 0.060" (1.52 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, .. |
|||
Maximum Service Temperature, Air | 232 °C | 450 °F | |
Arlon 99202R008 0.008" (0.203 mm) Cured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction: Interleave: FEP FilmSide 1: Cured Silicone Rubber Carrier: PTFE Coated FiberglassProduct Use: Adhesive. Bonds without primer.Appearance: Off-white, High viscosity gum on release.. |
|||
Maximum Service Temperature, Air | 232 °C | 450 °F | |
Arlon R31961R019 0.019" (0.483 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place.. |
|||
Maximum Service Temperature, Air | 232 °C | 450 °F | |
Arlon R33991R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Maximum Service Temperature, Air | 232 °C | 450 °F | |
Arlon 44141R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Clear PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 Fiberglass Side 2: Uncured Silicone RubberInterleave 2: Blue PolyethyleneThis data represent.. |
|||
Maximum Service Temperature, Air | 232 °C | 450 °F | |
Arlon 44580R010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. The data should not be used to wri.. |
|||
Maximum Service Temperature, Air | 232 °C | 450 °F | |
Arlon 30600R010 0.010" (0.254 mm) Uncured/Unsupported Silicone Rubber on a Release Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on a Release Carrier Product Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass with polymer release linersThis.. |
|||
Maximum Service Temperature, Air | 232 °C | 450 °F | |
Arlon 32210A005 0.005" (0.127 mm) Uncured Fluorosilicone Rubber on Polyester Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Fluorosilicone RubberCarrier: PolyesterThis data represents typical values for the production material. The data should not be used to wr.. |
|||
Maximum Service Temperature, Air | 232 °C | 450 °F | |
Arlon 47581R007 0.007" (0.178 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: PESide 1: Uncured Silicone RubberSubstrate: 2113 Style FiberglassSide 2: Uncured Silicone RubberInterleave 2: PE This data represents typical values for the produc.. |
|||
Maximum Service Temperature, Air | 232 °C | 450 °F | |
Arlon 48B10R005 0.005" (0.127 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1080 FiberglassThis data represents typical values for the production material. The data should not be us.. |
|||
Maximum Service Temperature, Air | 232 °C | 450 °F | |
Henkel Hysol EA 9394/C-2 Paste Adhesive System Elevated cure, thixotropic adhesive with structural properties to 450°F / 232°C.Application: Structural Repair |