Polymer Property : Maximum Service Temperature, Air = 2550 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1400 °C
2550 °F
GBC Grade 90 Alumina
Data provided by the manufacturer, GBC Materials Corporation.
Maximum Service Temperature, Air 1400 °C
2550 °F
Gouda Vuurvast A Vuurvast Dense Refractory Brick
Description: A general purpose high quality fireclay brick for use up to 1400°C. Reasonably good thermal shock resistance.Remarks: This data represents average values, obtained from samples that ..
Maximum Service Temperature, Air 1400 °C
2550 °F
Gouda Vuurvast CURON 140 Dense Refractory Castable
Description: Because of its relatively low Fe2O3 content and its high alumina percentages, this castable can be applied up to 1400°C in slightly reducing atmospheres. Up to high temperatures Curo..
Maximum Service Temperature, Air 1400 °C
2550 °F
Gouda Vuurvast CURON 140 GM Dense Refractory Castable
Description: Because of its relatively low Fe2O3 content and its high alumina percentages, this gunning castable can be applied up to 1400°C in slightly reducing atmospheres.Remarks: These values..
Maximum Service Temperature, Air 1400 °C
2550 °F
Gouda Vuurvast FLUCON 140 Dense Self Flowing Refractory Castable
Description: Flucon 140 is a self flowing low cement castable, based on a high quality chamotte grog.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Maximum Service Temperature, Air 1400 °C
2550 °F
Gouda Vuurvast VIBRON 140 C RAPID Dense Vibrating Refractory Castable
Description: Vibron 140 C Rapid is a low cement castable, based on high quality coarse chamotte grog. Because of special additives this castable is special suited for a faster heating schedule.Remar..
Maximum Service Temperature, Air 1400 °C
2550 °F
Gouda Vuurvast VIBRON 140 Dense Vibrating Refractory Castable
Description: Vibron 140 is a low cement castable, based on high quality chamotte.Remarks: Indicated values apply to vibrated products.Information provided by Gouda Vuurvast.
Maximum Service Temperature, Air 1400 °C
2550 °F
Gouda Vuurvast CURON 14 S Dense Refractory Castable
Description: Curon 14 S is a dense, strong and abrasion resistant castable. Because of the very low percentage of Fe2O3 and SiO2 it is used for highly abrasive conditions in reducing atmospheres.Rem..
Maximum Service Temperature, Air 1400 °C
2550 °F
Sharadaa Ceramics HH 40 Normal Medium and High Heat and Super Duty Brick
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Maximum Service Temperature, Air 1400 °C
2550 °F
Sharadaa Ceramics HH 40D Normal Medium and High Heat and Super Duty Brick
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Maximum Service Temperature, Air 1400 °C
2550 °F
Sharadaa Ceramics REFCAST Dense Castables
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Maximum Service Temperature, Air 1400 °C
2550 °F
Sharadaa Ceramics Sharada LTM 1.5 Insulating Castable
Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd.
Maximum Service Temperature, Air 1400 °C
2550 °F
Sharadaa Ceramics THERMO PATCH Dense Castables
Description: We offer a range of Dense Castables that are conventional castable and extensively used in boiler work, general furnace and burner blocks. Made as per international standards, our range..
Maximum Service Temperature, Air 1400 °C
2550 °F
Sharadaa Ceramics HICCS Insulation Brick
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Maximum Service Temperature, Air 1400 °C
2550 °F
CeramTec Rocar® ST Silicon Carbide, SSiC
Silicon carbide is extremely hard and displays excellent corrosion and thermal shock resistance. Its outstanding sliding properties and high thermal conductivity make useful in tribological applicat..
Maximum Service Temperature, Air 1400 °C
2550 °F
CeramTec Rubalit® 708 Alumina, 96%
Based on 96% aluminum oxide, Rubalit® 708 was developed specifically for making heavy-duty resistors and miniature metal layer resistors. Because of its outstanding strength, this same material is ..
Maximum Service Temperature, Air 1400 °C
2550 °F
CeramTec Rubalit® A 1999.5 Alumina, 99.7%
Rubalit® A 1999.5 (99.7%) is mechanically stronger, features a higher heat conductivity, and is more corrosion resistant than other aluminas. This high-purity aluminum oxide ceramic with carbon mat..
Maximum Service Temperature, Air 1400 °C
2550 °F
No Load
CoorsTek AD-85 Alumina (nom. 85% Al2O3)
Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Maximum Service Temperature, Air 1400 °C
2550 °F
Du-Co Ceramics S-470 Aluminum Silicate
Du-Co Ceramics Company manufactures a variety of crushable ceramic materials for use worldwide in cartridge heaters, thermocouples, and mineral insulated cable. The crushable ceramic products are cu..
Maximum Service Temperature, Air 1400 °C
2550 °F
Du-Co Ceramics S-570 Silica
Du-Co Ceramics Company manufactures a variety of crushable ceramic materials for use worldwide in cartridge heaters, thermocouples, and mineral insulated cable. The crushable ceramic products are cu..
Maximum Service Temperature, Air 1400 °C
2550 °F
Chosun Refractories CFS-1 Ceramic Foam
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Maximum Service Temperature, Air 1400 °C
2550 °F
limited
Chosun Refractories CT-140 Fireclay Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Maximum Service Temperature, Air 1400 °C
2550 °F
limited
Chosun Refractories CT-140S Fireclay Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Maximum Service Temperature, Air 1400 °C
2550 °F
Chosun Refractories CFA-1 Ceramic Foam
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Maximum Service Temperature, Air 1400 °C
2550 °F
limited
Chosun Refractories PT-140 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Maximum Service Temperature, Air 1400 °C
2550 °F
BNZ Materials BNZP-26 Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Maximum Service Temperature, Air 1400 °C
2550 °F
BNZ Materials BNZP-26A Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Maximum Service Temperature, Air 1400 °C
2550 °F
Anderman Ceramics EM60P Sillimanite
Porous synthetic mullite with high thermal shock. Available as tube up to 10 ft (3 m) long with diameters 0.6" to 2.4".Information provided by Anderman Ceramics.
Maximum Service Temperature, Air 1400 °C
2550 °F
Aremco Pyro-Paint™ 634-SIC High Temperature Refractory Coating
This advanced silicon carbide, water-based coating reduces significantly the oxidation of graphite and carbon components and structures at temperatures to 2550 °F (1400 °C). Provides a hard surfac..
Maximum Service Temperature, Air 1400 °C
2550 °F
CeramTec B 40 Alumina, 99.1%
B 40 is the ideal sliding mate with the same properties as Rubalit® A 1896. It contains a larger share of Al2O3 for superior chemical stability.