Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 80.0 °C @Time 1.80e+7 sec |
176 °F @Time 5000 hour |
|
Murtfeldt Original Material ”S”® Natural Polyethylene Material ”S”® is based on virgin, ultrahigh molecular weight low pressure polyethylene and significantly exceeds the requirements of DIN 16972. In particular, Material ”S”® natural has excell.. |
|||
Maximum Service Temperature, Air | 80.0 °C | 176 °F | |
Okulen® 500 - REG PE Colored OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Maximum Service Temperature, Air | 80.0 °C | 176 °F | Glass |
Parker Chomerics Tecknit Teckshield®-F 100 OPI 0.0022" Diameter Wire, High Performance EMC Window Description: TECKSHIELD-F high-performance fully laminated flat windows are specially designed to provide optimum optical transmission and EMI shielding in severe interference environments. TECKSHIE.. |
|||
Maximum Service Temperature, Air | 80.0 °C | 176 °F | Continuous Service |
NOVA Chemicals Dylite® F271T Specialty Expandable Polystyrene Features: Highly consistent bead size; high gloss characteristics; low energy consumption; fast cyclingApplications: Drinking cups -hot and cold, noodle bowls, take-out and ice cream containers, and.. |
|||
Maximum Service Temperature, Air | 80.0 °C | 176 °F | |
Okulen® 2000 PE-UHMW, W OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Maximum Service Temperature, Air | 80.0 °C | 176 °F | Continuous; FRISETTA Test Method |
Nilit FRIANYL B63 D Nylon 6., std. viscosity for injection molding Nylon 6., std. viscosity for injection molding, permanently flexible, developed for dowels.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Maximum Service Temperature, Air | 80.0 - 200 °C | 176 - 392 °F | Average value: 128 °C Grade Count:4 |
Overview of materials for Nylon 66, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Maximum Service Temperature, Air | 80.0 - 180 °C | 176 - 356 °F | Average value: 126 °C Grade Count:4 |
Overview of materials for Nylon 66, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Maximum Service Temperature, Air | 80.0 - 160 °C | 176 - 320 °F | Average value: 126 °C Grade Count:19 |
Overview of materials for Nylon 12, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |
|||
Maximum Service Temperature, Air | 80.0 °C | 176 °F | |
Lehmann & Voss LUVOCOM® 3-8363 Polyamide 6, unreinforced Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce.. |
|||
Maximum Service Temperature, Air | 80.0 °C | 176 °F | short term |
Lehmann & Voss LUVOCOM® 1200-7116-1 ABS, with carbon fiber Applications: Office communication.Reduced moment of inertia compared with metal parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Strong, stiff .. |
|||
Maximum Service Temperature, Air | 80.0 - 105 °C | 176 - 221 °F | Softening point |
Mitsui MILEXâ„¢ XL-225MB Phenol Aralkyl Resin, Standard Grade The MILEXâ„¢ Family of products is widely featured in brake systems of automobiles made by automakers through Mitsui Chemicals'. The phenolic material is primarily used as binders in brake pad.. |
|||
Maximum Service Temperature, Air | 80.0 °C | 176 °F | |
LATI Latan 13 S/30 POM, 30% Glass Bead Reinforced Polyoxymethylene (POM) based compound. Glass beads. Medium viscosity. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro.. |
|||
Maximum Service Temperature, Air | 80.0 °C | 176 °F | UL temperature rating; UL 1581 |
SABIC Innovative Plastics NORYL WCD891B PPE-TPE (Europe-Africa-Middle East) Non-halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications. Strong flame retardant performance capable of meeting VW-1 and 80°C end use tempera.. |
|||
Maximum Service Temperature, Air | 80.0 °C | 176 °F | |
Styrolution Luran® S 797 S UV White 33999 Q455 ASA Description: Grade with especially high notched impact strengthApplications: Lighting covers and lawn mower housings.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |
|||
Maximum Service Temperature, Air | 80.0 °C | 176 °F | UL temperature rating; UL 1581 |
SABIC Innovative Plastics NORYL WCD841U PPE-TPE Flexible, UV stabilized, halogen free extrusion grade for applications such as wire insulation and cable jacket. Good color stability after UV weathering per ASTM D4459. Light color capable. Flame r.. |
|||
Maximum Service Temperature, Air | 80.0 °C | 176 °F | Short Term (3h) |
Wolf Kunststoff ZEDEX® ZX-100EL55 A1F Polymer Alloy, Elastomer Modified Main Characteristics: Rubbery; Soft; High shock absorption; High impact resistance; Elongation > 300%Applications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automitve Technol.. |
|||
Maximum Service Temperature, Air | 80.0 °C | 176 °F | |
Trelleborg R448 Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Maximum Service Temperature, Air | 80.0 °C | 176 °F | Continuous use |
Polyram PlusTek PB841 Nylon 6 for Injection Molding, Impact Modified Impact modified Nylon 6 for injection molding applications.Information provided by Polyram. |
|||
Maximum Service Temperature, Air | 80.0 - 110 °C | 176 - 230 °F | long term; EMS |
EMS-Grivory Grivory® BG-25 HM PA6-GF25 Product description: Grilon BG-25 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 25% glass fibers. Grilon BG-25 HM has the following important prop.. |
|||
Maximum Service Temperature, Air | 80.0 - 110 °C | 176 - 230 °F | long term; EMS |
EMS-Grivory Grivory® BRZ 347 W PA6 Product description: Grilon BRZ 347 W is a heat stabilized, high viscosity, impact modified and plasticized PA6 extrusion grade. Grilon BRZ 347 W has the following important properties: High flexibi.. |
|||
Maximum Service Temperature, Air | 80.0 - 110 °C | 176 - 230 °F | long term; EMS |
EMS-Grivory Grivory® L 16 W 20 black 9995 PA12 Product Description: Grilamid L 16 W 20 is a semi-flexible low viscosity, heat stabilized PA12 injection molding grade. The main characteristics of this product are: Easy flowing?High impact streng.. |
|||
Maximum Service Temperature, Air | 80.0 °C | 176 °F | |
Elmer's Products Aron Alpha® 252F Cyanoacrylate Adhesive (Industrial Krazy Glue™) Surface insensitive adhesives, ultra-fast setting for porous, soft or tough-to-bond substrates. Series 200TX & Gel: No run, no stringing, excellent gap filling characteristics with good strength on.. |
|||
Maximum Service Temperature, Air | 80.0 °C | 176 °F | |
Alliance N-38 Neodymium Iron Boron Magnetic Material |