Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 50.0 °C | 122 °F | UL-746 ABC |
Plaskolite Optix® CP - 61 General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | UL-746 ABC |
Plaskolite West Optix® CA - 41 FDA General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | UL-746 ABC |
Plaskolite West Optix® CP - 41 UVA General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | UL-746 ABC |
Plaskolite West Optix® CP - 61 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | UL-746 ABC |
Plaskolite Optix® CP - 924 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | Deflection temperature; load unknown. |
Abatron AboCast 8-8/Abocure 8-8 Epoxy
(discontinued **) 2-part solvent-free dielectric epoxy casting compound.Processing: 100/50 ratio (pbw); Gel time, 1 lb. (2.2 kg): 135 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°C (212°F)... |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | |
Natural Rubber, Not Vulcanized (NR, IR, Polyisoprene) Natural rubber is polyisoprene. Chemical and environmental resistance and mechanical properties are improved through crosslinking (vulcanizing), usually through treatment with sulfur.Natural rubber.. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | RTI |
Sylvin Technologies 9077-70 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | RTI |
Sylvin Technologies 9077-75 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | RTI |
Sylvin Technologies 9077-90 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | RTI |
Sylvin Technologies 916V0 Black PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | RTI |
Sylvin Technologies 9604-80 Clear PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | RTI |
Sylvin Technologies 9604-80C Clear PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | RTI |
Sylvin Technologies 9604-95 Clear PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | RTI |
Sylvin Technologies 9812A-95 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | Application |
3M 2000+ Fire Barrier Silicone Sealant 3M Fire Barrier Silicone Sealant 2000+ is a ready-to-use, gun-grade, one-component silicone elastomer that cures upon exposure to atmospheric humidity to form a flexible firestop seal. This material.. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | Application; ASTM C1299 |
3M CP 25WB+ Fire Barrier Sealant 3M Fire Barrier Sealant CP 25WB+ is a high-performance, ready-to-use, gun-grade, latex-based, intumescent sealant that dries to form a monolithic fire-stop seal that also acts as a barrier to airbor.. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | Long term |
3M 9576 Splicing Tape 3M™ Splicing Tape offers excellent flying splice and core starting wet grab characteristics. They are typically used in the printing industry and perform well at process speeds in excess of 2000 fe.. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | |
3M SS100 Smoke and Sound Sealant 3M Smoke and Sound Sealant SS 100 is an economical, ready to use, gun-grade, elastomeric sealant that drives to form a monolithic flexible seal that helps prevent unwanted noise infiltration and mit.. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | |
Abatron 8311-8A/82033B Filled Potting Compound
(discontinued **) Gray and colors casting, potting, embedding, and adhesive epoxy system. 40% filled. 100/8 ratio.Information provided by Abatron. |
|||
Maximum Service Temperature, Air | 50.0 - 90.0 °C | 122 - 194 °F | Average value: 72.9 °C Grade Count:14 |
Overview of materials for Acrylic, Impact Modified, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | RTI |
Sylvin Technologies 9604-95 LMW Clear PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Maximum Service Temperature, Air | 50.0 - 125 °C | 122 - 257 °F | Average value: 95.1 °C Grade Count:23 |
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Elastomer, Unreinforced". Each property range of values reported is minimum and .. |