Polymer Property : Maximum Service Temperature, Air = 280 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 280 °C
536 °F
Temperature Index (Burning); NES 715
Solvay Specialty Polymers Cogegum® AFR/720 Polyolefin, Unspecified  (discontinued **)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
Maximum Service Temperature, Air 280 °C
536 °F
Temperature Index (Burning); NES 715
Solvay Specialty Polymers Cogegum® AFR/920-UV Polyolefin, Unspecified  (Unverified Data**)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
Maximum Service Temperature, Air 280 °C
536 °F
Long Term
Ensinger Sintimid™ V Unfilled Polyimide (PI)  (discontinued **)
SINTIMID™ V polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an idea choice for the most demanding applications. SINTIMID™ V..
Maximum Service Temperature, Air 280 °C
536 °F
Long Term
Ensinger Sintimid™ V 40% graphite Polyimide (PI)  (discontinued **)
SINTIMID™ V polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an idea choice for the most demanding applications. SINTIMID™ V..
Maximum Service Temperature, Air 280 °C
536 °F
Long Term
Ensinger Sintimid™ V-HP high-purity Polyimide (PI)  (discontinued **)
SINTIMID™ V polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an idea choice for the most demanding applications. SINTIMID™ V..
Maximum Service Temperature, Air 280 °C
536 °F
short term
Lehmann & Voss LUVOCOM® 1105-7192 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
Maximum Service Temperature, Air 280 °C
536 °F
short term
Lehmann & Voss LUVOCOM® 1105-7678 PEEK, with carbon fiber, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m..
Maximum Service Temperature, Air 280 °C
536 °F
short term
Lehmann & Voss LUVOCOM® 1105-7766 PEEK, with carbon fiber, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
Maximum Service Temperature, Air 280 °C
536 °F
short term
Lehmann & Voss LUVOCOM® 1105-7916 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts.High chemical resistance parts, hydrolysis resi..
Maximum Service Temperature, Air 280 °C
536 °F
short term
Lehmann & Voss LUVOCOM® 1105-7938/GY PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
Maximum Service Temperature, Air 280 °C
536 °F
short term
Lehmann & Voss LUVOCOM® 1105-8167 PEEK, with carbon fiber, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m..
Maximum Service Temperature, Air 280 °C
536 °F
short term
Lehmann & Voss LUVOCOM® 1105-8234 PEEK, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Dynam..
Maximum Service Temperature, Air 280 °C
536 °F
short term
Lehmann & Voss LUVOCOM® 1105-8422 PEEK, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m..
Maximum Service Temperature, Air 280 °C
536 °F
short term
Lehmann & Voss LUVOCOM® 1105-8476 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precisio..
Maximum Service Temperature, Air 280 °C
536 °F
short term
Lehmann & Voss LUVOCOM® 1105-8513 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
Maximum Service Temperature, Air 280 °C
536 °F
short term
Lehmann & Voss LUVOCOM® 1105/CF/15/TF/15 PEEK, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m..
Maximum Service Temperature, Air 280 °C
536 °F
short term
Lehmann & Voss LUVOCOM® 1105/GF/30/BK-1 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
Maximum Service Temperature, Air 280 °C
536 °F
short term
Lehmann & Voss LUVOCOM® 1105/GF/30/TF/15 PEEK, with glass fiber and PTFE
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,..
Maximum Service Temperature, Air 280 °C
536 °F
short term
Lehmann & Voss LUVOCOM® 1105-0706 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch..
Maximum Service Temperature, Air 280 °C
536 °F
short term
Lehmann & Voss LUVOCOM® 1105-0923/GY2 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera..
Maximum Service Temperature, Air 280 °C
536 °F
short term
Lehmann & Voss LUVOCOM® 1105-0948/YL2 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch..
Maximum Service Temperature, Air 280 °C
536 °F
short term
Lehmann & Voss LUVOCOM® 1105-7781/BK PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
Maximum Service Temperature, Air 280 °C
536 °F
short term
Lehmann & Voss LUVOCOM® 1105-7914 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts.High chemical resistance parts, hydrolysis resi..
Maximum Service Temperature, Air 280 °C
536 °F
short term
Lehmann & Voss LUVOCOM® 1105-7916-1 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts.High chemical resistance parts, hydrolysis resi..
Maximum Service Temperature, Air 280 °C
536 °F
short term
Lehmann & Voss LUVOCOM® 1105-8389/BL PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
Maximum Service Temperature, Air 280 °C
536 °F
Heat Resistance; DIN 53772
Karina 1000/0080 IE MBPEB Antisplit Color Concentrate
LDPE carrier based antisplit MB for PP woven tape used on a dosage between 2% and 4%.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Maximum Service Temperature, Air 280 °C
536 °F
Short Periods
Hippe PA 46 Nylon 46
PA 46 is primarily used in higher temperature ranges where stiffness, creep resistance, continuous heat stability and fatigue strength are required. Therefore PA 46 is suitable for high quality app..
Maximum Service Temperature, Air 280 °C
536 °F
Short term
3M 9085UV Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
Maximum Service Temperature, Air 280 °C
536 °F
Highly Temperature Resistant Quality, Opaque, Grey, Blue
BIW ASTM Class 2D2 Silicone Foam
Products are a closed cell foam and there fore good for use in damp or liquid applications. A variety of physical properties and foam qualities are available by adjusting the processing parameters...