SINTIMID™ V polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an idea choice for the most demanding applications. SINTIMID™ V is characterized by its long-term thermal stability, outstanding wear resistance, high creep resistance, and strength up to its continuous use temperature of 572°F.Superior high temperature characteristicsExcellent long-term thermal stabilityOutstanding bearing and wear properties (at elevated temperatures, SINTIMID™ V formulations offer superior wear rates)Excellent creep resistanceHigh strength and stiffness properties (SINTIMID™ V has a tensile strength of 20,000 psi at room temperature)High purity characteristics (only extremely low levels of extractables and ionic impurities are apparent in SINTIMID™ V)Good chemical resistance (SINTIMID™ V is not attacked by common solvents or fuels and is acceptable for use in contact with many acids)SINTIMID™ V with its superior physical properties, is ideal for applications in the aerospace, nuclear, automotive, electrical/electronic, and chemical processing industries. It is an excellent candidate for high purity applications in the semiconductor processing industry. Typical components produced from SINTIMID™ V include seals, thrust washers, bushings and wear pads in transportation/off-highway equipment, insulating and support elements in electrical welding and brazing equipment, and wafer-handling components in the harsh environment of semiconductor plasma ovens. Pump and valve seals, vanes, and piston rings are also commonly produced from SINTIMID™ V.Information Provided by Ensinger Industries, Inc.Sintimid has been replaced with Tecasint in the Ensinger product line.
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
ASTM D792
Density 1.34 g/cc
0.0484 lb/in³
ASTM D792
Water Absorption 0.62 %

@Temperature 22.8 °C,
Time 86400 sec
0.62 %

@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 120
120
ASTM D785
Tensile Strength, Yield 140 MPa

@Temperature 22.8 °C
20300 psi

@Temperature 73.0 °F
ASTM D638
Elongation at Break 9.0 %

@Temperature 22.8 °C
9.0 %

@Temperature 73.0 °F
ASTM D638
Flexural Strength 205 MPa

@Temperature 22.8 °C
29700 psi

@Temperature 73.0 °F
ASTM D790
Flexural Modulus 4.00 GPa

@Temperature 22.8 °C
580 ksi

@Temperature 73.0 °F
ASTM D790
Izod Impact, Notched 0.320 J/cm

@Temperature 22.8 °C
0.600 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 50.4 µm/m-°C
28.0 µin/in-°F
ASTM D696
Maximum Service Temperature, Air 280 °C
536 °F
Long Term
330 °C
626 °F
Intermittent
Deflection Temperature at 1.8 MPa (264 psi) 316 °C
600 °F
ASTM D648