Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 182 °C | 360 °F | Cured |
Parker Chomerics Tecknit TeckBond™-C Silver-Plated Copper-Filled Adhesive Description: TECKBOND-C is a silicone rubber base filled with silver-plated copper particles to produce a highly conductive one-component adhesive sealant. The system is an RTV moisture-cured compou.. |
|||
Maximum Service Temperature, Air | 182 °C | 360 °F | |
Fujipoly Industries Sarcon® 30GHR Thin-Film GHR Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of .. |
|||
Maximum Service Temperature, Air | 182 °C | 360 °F | |
Fujipoly Industries Sarcon® 30GSR Thin-Film GSR Sarcon GSR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GSR is a composite of.. |
|||
Maximum Service Temperature, Air | 182 °C | 360 °F | |
Fujipoly Industries Sarcon® 30GTR Thin-Film GTR Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of .. |
|||
Maximum Service Temperature, Air | 182 °C | 360 °F | |
Fujipoly Industries Sarcon® 30U Thin-Film UR Sarcon UR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov.. |
|||
Maximum Service Temperature, Air | 182 °C | 360 °F | |
Fujipoly Industries Sarcon® 45H Thin-Film HR Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of .. |
|||
Maximum Service Temperature, Air | 182 °C | 360 °F | |
Fujipoly Industries Sarcon® 45T Thin-Film TR Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of .. |
|||
Maximum Service Temperature, Air | 182 °C | 360 °F | |
Fujipoly Industries Sarcon® 45U Thin-Film UR Sarcon UR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov.. |
|||
Maximum Service Temperature, Air | 182 °C | 360 °F | |
Fujipoly Industries Sarcon® 85T Thin-Film TR Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of .. |
|||
Maximum Service Temperature, Air | 182 °C | 360 °F | Short Term |
TriStar Ultracomp UC-400 Composite Bearing Ultracomp UC-400 - Designed for high loads, low speeds, impact and vibration applications. UC-400 has a MOS2 additive for salt water applications where cathodic reactions could occur. Excellent dry .. |
|||
Maximum Service Temperature, Air | 182 °C | 360 °F | Short Term |
TriStar Ultracomp UC-500 Composite Bearing Ultracomp UC-500 - Multiple sources of lubrication make this Ultracomp an excellent choice for full rotary or higher speed linear applications. High strength, high impact resistance and long wear li.. |
|||
Maximum Service Temperature, Air | 182 °C | 360 °F | Intermittent |
Ensinger TECASON™ P MT Polyphenylsulfone (PPSU) TECASON™ P MT is a polyphenylsulfone suited primarily to applications in the medical industry. It has improved performance in terms of temperature, impact strength and chemical resistance, as well.. |
|||
Maximum Service Temperature, Air | 182 °C | 360 °F | Intermittent |
Ensinger RADEL® R-5500 Polyphenylsulfone (PPSU) RADEL® R is a Polyphenysulfone produced by Solvay Advanced Polymers. RADEL® R is in the same performance category as products like Polysulfone and ULTEM® (PEI). RADEL® R has increased performa.. |
|||
Maximum Service Temperature, Air | 182 °C | 360 °F | Short term, cured 14 days @ 50% RH |
3M AC-240 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-240 Class B is a two-part, polysulfide-based, long application life, quick cure product for use as a sealant for integral fuel tanks and fuselages. This tow-component, mangan.. |
|||
Maximum Service Temperature, Air | 182 °C | 360 °F | AMS-S-8802, cured 14 days @ 50% RH |
3M AC-251 Black Class B-1 Aerospace Sealant 3M Aerospace Sealant AC-251 Black Class B are two-part, quick curing, polysulfide based canopy and windshield sealants. These products are formulated for sealing acrylic, glass, and polycarbonate ai.. |
|||
Maximum Service Temperature, Air | 182 °C | 360 °F | AMS-S-8802, cured 14 days @ 50% RH |
3M AC-251 Black Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-251 Black Class B are two-part, quick curing, polysulfide based canopy and windshield sealants. These products are formulated for sealing acrylic, glass, and polycarbonate ai.. |
|||
Maximum Service Temperature, Air | 182 °C | 360 °F | Short term, cured 14 days @ 50% RH |
3M AC-275 Class B-1/2 Aerospace Sealant 3M Aerospace Sealant AC-275 Class B is a high temperature two-component manganese dioxide cured, liquid polysulfide polymer sealants providing excellent fuel tank and fuselage seals. They have outst.. |
|||
Maximum Service Temperature, Air | 182 °C | 360 °F | Short term, cured 14 days @ 50% RH |
3M AC-275 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-275 Class B is a high temperature two-component manganese dioxide cured, liquid polysulfide polymer sealants providing excellent fuel tank and fuselage seals. They have outst.. |
|||
Maximum Service Temperature, Air | 182 °C | 360 °F | Short term, cured 14 days @ 50% RH |
3M AC-350 Class A-2 Aerospace Sealant 3M Aerospace Sealant AC-350 Class A are fast-cure, intermediate density two-component, manganese dioxide cure, brushable, polysulfide fuel tank and fuselage sealants. 3M AC-350 Class A Sealants have.. |
|||
Maximum Service Temperature, Air | 182 °C | 360 °F | Short term, cured 14 days @ 50% RH |
3M AC-350 Class C-2 Aerospace Sealant 3M Aerospace Sealant AC-350 Class C are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant hav.. |
|||
Maximum Service Temperature, Air | 182 °C | 360 °F | Short term, cured 14 days @ 50% RH |
3M AC-360 Class B-1/2 Aerospace Sealant 3M Aerospace Sealant AC-360 Class B are fast cure, intermediate density two-component, manganese dioxide cure, polysulfide fuel tank and fuselage sealant. 3M AC-360 Class B Sealants have outstanding.. |
|||
Maximum Service Temperature, Air | 182 °C | 360 °F | Short term, cured 14 days @ 50% RH |
3M AC-360 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-360 Class B are fast cure, intermediate density two-component, manganese dioxide cure, polysulfide fuel tank and fuselage sealant. 3M AC-360 Class B Sealants have outstanding.. |
|||
Maximum Service Temperature, Air | 182 °C | 360 °F | Short term, cured 14 days @ 50% RH |
3M AC-730 Class C-4 (168) Aerospace Sealant 3M Aerospace Sealant AC-730 Class C are two-part, manganese-cured, non-chromate corrosion inhabiting sealants. These Sealants provide an effective barrier against the common causes of corrosion on a.. |
|||
Maximum Service Temperature, Air | 182 °C | 360 °F | Short term, cured 14 days @ 50% RH |
3M AC-370 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-370 Class B are fast cure, low density polysulfide sealants suitable for fuel tank and fuselage applications. These two-component, manganese dioxide cured sealants are solven.. |
|||
Maximum Service Temperature, Air | 182 °C | 360 °F | Short term, cured 14 days @ 50% RH |
3M AC-730 Class B-1/2 Aerospace Sealant 3M Aerospace Sealant AC-730 Class B are fast cure, two-part, manganese-cured, non-chromate containing corrosion inhabiting sealants. These Sealants provide an effective barrier against the common ca.. |
|||
Maximum Service Temperature, Air | 182 °C | 360 °F | Short term, cured 14 days @ 50% RH |
3M AC-730 Class C-8 (24) Aerospace Sealant 3M Aerospace Sealant AC-730 Class C are two-part, manganese-cured, non-chromate corrosion inhabiting sealants. These Sealants provide an effective barrier against the common causes of corrosion on a.. |
|||
Maximum Service Temperature, Air | >= 182 °C | >= 360 °F | |
Saint-Gobain Rulon® ACM Bearing/Seal PTFE
(discontinued **) Saint Gobain Rulon® ACM is now produced as a part of the TriStar Plastics Corp. product line under the Ultracomp trade name.Description: This family of materials offers the combination of high comp.. |
|||
Maximum Service Temperature, Air | 182 °C | 360 °F | Heat Resistance; ASTM D570D |
Plenco 3557 Phenolic, Granular, Transfer Molded PLENCO 03557 is a woodflour and mineral filled phenolic molding compound offering excellent dielectric strength values at elevated temperatures while maintaining mechanical strength properties. UL r.. |
|||
Maximum Service Temperature, Air | 182 °C | 360 °F | Short term, cured 14 days @ 50% RH |
3M AC-240 Class B-4 Aerospace Sealant 3M Aerospace Sealant AC-240 Class B is a two-part, polysulfide-based, long application life, quick cure product for use as a sealant for integral fuel tanks and fuselages. This tow-component, mangan.. |