Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1650 °C | 3000 °F | Continuous |
Zircar Zirconia ZYZ-3 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
GBC Grade 98 Alumina Data provided by the manufacturer, GBC Materials Corporation. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Gouda Vuurvast CURAS 85 PD Moldable Refractory Material Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. This phosphate bonded material based on corundum and bauxite has a very go.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Gouda Vuurvast FI 65-12 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Gouda Vuurvast GOLITE 160 Refractory Insulating Castable Description: This castable can be used up to very high temperatures under reducing conditions.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Zircar Refractory Composites RS-99-45 Refractory Sheet ZRCI Refractory Sheet Type RS-99-45 is comprised of 99% alumina. This "All-Alumina" material is strong, uniform, rigid, refractory structure composed of alpha alumina fibers and high purity inorgani.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Zircar Refractory Composites RS-99-60 Refractory Sheet ZRCI Refractory Sheet Type RS-99-60 is comprised of 99% alumina. This "All-Alumina" material is strong, uniform, rigid, refractory structure composed of alpha alumina fibers and high purity inorgani.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Zircar Zirconia M-45 Alumina Boards, Discs & Cylinders Insulation Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Zircar Ceramics APA-1 Alumina Paper ZIRCAR Alumina Papers are uniform structures made principally of alumina fiber. APA-1 is a strong, flexible material with fibers held together with organic binder that is available in roll or sheet.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Zircar Ceramics APA-3 Alumina Paper ZIRCAR Alumina Papers are uniform structures made principally of alumina fiber. APA-3 is a thin uniformly rigidized sheet of alumina fiber and binder. Applications include thermal insulation in lo.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Zircar Refractory Composites Alumina Coat ZRCI ALUMINA COAT is an all-alumina liquid formulation used for hardening and increasing the refractoriness of the surfaces of alumina and alumina-silicate fiber products. ZRCI ALUMINA COAT is comp.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Zircar Refractory Composites RS-3000 ALUMINA FELT ZRCI Alumina Felt Type RS-3000 is 97% high purity alumina fiber, ceramic felt with less than 1% shot. Type RS-3000 is a strong, flexible material with fibers held together with an organic binder. It.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Cotronics Resbond™ 906 High Temperature Ceramic Adhesive, High Expansion |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | limited |
Chosun Refractories PT-165 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | limited |
Chosun Refractories TCH-175SV Torpedo Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Anderman Ceramics EZZ 66P Zircon Zirconia materials offer high temperature capability as well as excellent performance in areas of high wear and corrosion. Available in many shapes and sizes. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Aremco Ceramabind™ 642 High Temperature Inorganic Binder A basic solution which is highly compatible with most ceramic and metal powders. Good wettability and tack, and excellent acid resistance after curing. Extremely moisture resistant after a high temp.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Aremco Ceramabind™ 644-A High Temperature Inorganic Binder An acidic, colloidal alumina binder developed for mixing with sized refractory flours and grains to produce high temperature refractory coatings for ceramic fiber boards. Used as a superior standalo.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Aremco Ceramabind™ 875 High Temperature Inorganic Binder An acidic powdered binder system used to formulate high strength, hydraulic-setting cements for electrical potting or molding applications. A powder blend is typically formulated by adding one part .. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Aremco Ceramabond™ 835-MB High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Aremco Ceramacast™ 576-N High Temperature Potting & Casting Alumina Medium grain castable ceramic for large high temperature potting and tooling. Aremco offers a range of ceramic-based materials used for the assembly of high temperature, high power electrical devic.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Aremco Ceramacast™ 646-N High Temperature Potting & Casting Material Zirconia Castable ceramic with high dielectric and physical strength. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Aremco Ceramabond™ 503 High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Aremco Ceramabond™ 835-M High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Aremco Ceramacast™ 575 Alumina Fine Grain Potting Compound Hydraulic setting. Fine grain castable for potting and producing small tools. Used in the production of temperature probes, electrical feed-throughs, large heat treating fixtures, induction coils .. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | Continuous |
Zircar Zirconia ZYC Zirconia Cylinders Insulation Zircar Zirconia Cylinders Type ZYC are rigid, free standing refractory structures composed of yttria stabilized zirconia fibers that are bonded with silica. The material is evenly bonded, allowing .. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Pyrotek Pyrocast AL2 Abrasion-Resistant Refractory Castable Pyrocast AL2 refractory castable is a mullite-based refractory well suited for applications prone to erosion and abrasion. It exhibits excellent non-wetting properties when used in molten aluminum .. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | Continuous |
Zircar Zirconia ZYZ-6 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |