Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
GBC Grade 96 Alumina Data provided by the manufacturer, GBC Materials Corporation. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Gouda Vuurvast AK 55 S Dense Refractory Brick Description: This andalusite based brick is characterized by a low porosity and a good creep resistance (After 24 hours at 1350°C under a load of 0.2 MPa gives between 14th and 24th hour a creep .. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Gouda Vuurvast CURAS 85 PD REPAIR Moldable Refractory Material Description: Curas 85 PD Repair is a phosphate bonded moldable based on sintered bauxite. It has been specially developed for aluminum melting and holding furnaces. However, it can be applied on any.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Gouda Vuurvast CURON 160 H SIC GM Dense Refractory Castable Description: This gunning castable has an extremely good thermal shock resistance and very good resistance against aggressive slags. Application among others in the copper industry.Remarks: These va.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Gouda Vuurvast CURON 160 HF Dense Refractory Castable Description: This castable has a high volume stability and keeps its strength up to high temperatures. In addition, Curon 160 HF has an excellent thermal shock resistance. It is largely used in the .. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Gouda Vuurvast CURON 160 HS GM Dense Refractory Castable Description: This gunning castable has a high volume stability up to high temperatures. In addition Curon 160 HS GM has an excellent thermal shock resistance and abrasion resistance (9-12 cm3 accord.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Gouda Vuurvast VIBRON 160 Dense Vibrating Refractory Castable Description: Vibron 160 is a low cement vibrating castable on andalusite base, characterized by a high strength and excellent thermal shock resistance.Remarks: Indicated values apply to vibrated pro.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Gouda Vuurvast VIBRON 160 H Dense Vibrating Refractory Castable Description: Vibron 160 H is a low cement castable based on high fired high alumina grog and characterized by a high strength and good thermal shock resistance.Remarks: Indicated values apply to vib.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Gouda Vuurvast VIBRON 165 Dense Vibrating Refractory Castable Description: Vibron 165 is a low cement castable based on andalusite and especially fit for the production of prefab elements.Remarks: Indicated values apply to vibrated products.Information provide.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Gouda Vuurvast AK 85 M Dense Refractory Brick Description: A bauxite based brick with a mullite bond. Application: torpedo ladles, electric arc furnace roofs, cement kilns.Remarks: This data represents average values, obtained from samples that.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Gouda Vuurvast CURAS 60 SD Moldable Refractory Material Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. Because this material contains a high percentage of sillimanite, it has a .. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Gouda Vuurvast CURON 160 H Dense Refractory Castable Description: Because of the selection of raw materials this castable has a high volume stability and keeps its strength up to high temperatures. In addition Curon 160 H has an excellent thermal shoc.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Gouda Vuurvast VIBRON 160 H RAPID Dense Vibrating Refractory Castable Description: Vibron 160 H Rap is a low cement castable based on high fired high alumina grog and characterized by a high strength and good thermal shock resistance. Because of special additives, thi.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Sharadaa Ceramics PCF80 Precast Prefired Brick Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Castin.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Sharadaa Ceramics REFCAST LC60ABR Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Sharadaa Ceramics REFCAST LC70 Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Sharadaa Ceramics Saber Block, Pyroblock Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Sharadaa Ceramics ZAP 009 Smart Cast Application Special Properties: Thermal Shock, Lesser Dross Formation, Non-wetting To AluminumIndustry: Non-FerrousApplication: Aluminum Melting/Holding Furnace, Launders, Risers, Transfer LaddlesInformation pr.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | Deformation temp |
SPHERE ONE EXTENDOSPHERESâ„¢ HA Hollow Spheres EXTENDOSPHERESâ„¢ HA are off white, low-cost, low-density, high alumina, ceramic hollow spheres.Applications: Hollow spheres are ideal for use in coatings, sealants, caulks and other applications.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Zircar Zirconia Buster Blanket Alumina Blanket Insulation Buster Blanket and Buster Mat are flexible, Hi-Alpha alumina fiber insulation materials. The mat is 100% fibers while the blanket has been needled into a durable blanket with the addition of an orga.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | No Load |
CoorsTek SC-DSG (SC-35) Graphite Loaded Sintered Silicon Carbide Thermal Shock Delta Tc = 600°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Chosun Refractories 1600BLANKET Blanket Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | limited |
Chosun Refractories HSC-16H-W2 Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | limited |
Chosun Refractories HSC-16RA Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | limited |
Chosun Refractories PT-160 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | limited |
Chosun Refractories HACT-160 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | Intermittent |
Zircar Ceramics AL-30AA Alumina Insulation AL-30 and AL-30AA are rigid alumina fiber boards characterized by uniform open porosity and high machinability. Alumina bonded AL-30AA is used in fuel cell reformers.Information provided by Zircar C.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Sinotek Materials PMF Board Heat Insulation Material Ceramic Fiber Board, White Ceramic Fiber Board is used for the following applications: sealing for furnace doors, thermal and electric insulation for heaters, glass and ceramics, high temperature and thermal insulation, and i.. |