Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1350 °C | 2460 °F | |
Gouda Vuurvast B 1 Dense Refractory Brick Description: B 1 is a fireclay quality for general applications up to 1350°CRemarks: This data represents average values, obtained from samples that were cut from standard bricks.Information prov.. |
|||
Maximum Service Temperature, Air | 1350 °C | 2460 °F | |
Gouda Vuurvast FI 35-15 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Maximum Service Temperature, Air | 1350 °C | 2460 °F | |
Gouda Vuurvast FLUCON 150 G (R) Dense Self Flowing Refractory Castable Description: Flucon 150 G (R) is a self-flowing low cement castable based on sintered South-American bauxite. Especially suitable for direct contact with liquid aluminum metal.Remarks: These values .. |
|||
Maximum Service Temperature, Air | 1350 °C | 2460 °F | |
Gouda Vuurvast GOLITE 135 RL C Refractory Insulating Castable Description: Golite 135 RL C is a coarse low iron light weight castable and combines a good mechanical strength with a low density and a low thermal conductivity.Remarks: These values apply to cast .. |
|||
Maximum Service Temperature, Air | 1350 °C | 2460 °F | |
Gouda Vuurvast VIBRON 135 Dense Vibrating Refractory Castable Description: Vibron 135 is a vibrating castable, specially fit for the production of prefab elements. The very low cement content (1%) and the abrasion resistant spinel grains give this material exc.. |
|||
Maximum Service Temperature, Air | 1350 °C | 2460 °F | |
Gouda Vuurvast VIBRON 150 G Dense Vibrating Refractory Castable Description: Vibron 150 G is a low cement castable based on sintered South-American bauxite. Especially suited for direct contact with liquid aluminum metal.Remarks: Indicated values apply to vibrat.. |
|||
Maximum Service Temperature, Air | 1350 °C | 2460 °F | |
Gouda Vuurvast VIBRON 150 G RAPID Dense Vibrating Refractory Castable Description: Vibron 150 G Rapid is a low cement castable based on sintered South-American bauxite. Because of special additives this material is suited for direct contact with liquid aluminum and al.. |
|||
Maximum Service Temperature, Air | 1350 °C | 2460 °F | |
Sharadaa Ceramics PCF40 Precast Prefired Brick Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Castin.. |
|||
Maximum Service Temperature, Air | 1350 °C | 2460 °F | |
Sharadaa Ceramics REFCAST SPECIAL Dense Castables Description: We offer a range of Dense Castables that are conventional castable and extensively used in boiler work, general furnace and burner blocks. Made as per international standards, our range.. |
|||
Maximum Service Temperature, Air | 1350 °C | 2460 °F | |
Sharadaa Ceramics REFCAST SPL Dense Castables Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Maximum Service Temperature, Air | 1350 °C | 2460 °F | |
Sharadaa Ceramics Sharada LTM 1.2 Insulating Castable Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Maximum Service Temperature, Air | 1350 °C | 2460 °F | Extended periods if cycles remain above 300°C |
Saint-Gobain Spectrosil® 1000 Optical Fused Quartz Spectrosil® 1000 grade is used for non-transmissive mirrors and substrates, and other high purity components which do not require specified optical transmission.Spectrosil® is a synthetic fuse.. |
|||
Maximum Service Temperature, Air | 1350 °C | 2460 °F | |
Saint-Gobain Spectrosil® 1000 Optical Fused Quartz Spectrosil® 1000 grade is used for non-transmissive mirrors and substrates, and other high purity components which do not require specified optical transmission.Spectrosil® is a synthetic fuse.. |
|||
Maximum Service Temperature, Air | 1350 °C | 2460 °F | Extended periods if cycles remain above 300°C |
Saint-Gobain Spectrosil® 2100 Optical Fused Quartz Spectrosil® 2100 has improved refractive index homogeneity.Spectrosil® is a synthetic fused silica manufactured using a patented, environmentally friendly process that results in a virtually c.. |
|||
Maximum Service Temperature, Air | 1350 °C | 2460 °F | |
Saint-Gobain Spectrosil® 2100 Optical Fused Quartz Spectrosil® 2100 has improved refractive index homogeneity.Spectrosil® is a synthetic fused silica manufactured using a patented, environmentally friendly process that results in a virtually c.. |
|||
Maximum Service Temperature, Air | 1350 °C | 2460 °F | Extended periods if cycles remain above 300°C |
Saint-Gobain Spectrosil® 2200 Optical Fused Quartz Spectrosil® 2200 grade is an excimer laser grade developed for maximum transmission and prolonged life in microlithography and other critical deep UV applications using KrF (248 nm) and ArF (193 .. |
|||
Maximum Service Temperature, Air | 1350 °C | 2460 °F | |
Saint-Gobain Spectrosil® 2200 Optical Fused Quartz Spectrosil® 2200 grade is an excimer laser grade developed for maximum transmission and prolonged life in microlithography and other critical deep UV applications using KrF (248 nm) and ArF (193 .. |
|||
Maximum Service Temperature, Air | 1350 °C | 2460 °F | Extended periods if cycles remain above 300°C |
Saint-Gobain Vitreosil® 065 066 Optical Fused Quartz Vitreosil® 065, for use in the near UV and visible, has a less rigorous bubble specification. It has a useful transmission range from 270 nm in the near UV to 2000 nm in the IR.Vitreosil® opt.. |
|||
Maximum Service Temperature, Air | 1350 °C | 2460 °F | Extended periods if cycles remain above 300°C |
Saint-Gobain Vitreosil® Clear Fused Quartz Tubing Electrically fused quartz is recognized for its combination of purity, chemical inertness, physical stability, thermal shock resistance, high electrical resistivity, and high operating temperatures... |
|||
Maximum Service Temperature, Air | 1350 °C | 2460 °F | |
Skamol Group SICAL Mortar Silicon Carbide Mortar Sical mortar has the following characteristics: Max. service temperature 1350°C (2462°F)Good adherence to SiC bricksHigh SiC contentHigh content of finesEasy to handleInformation provided by S.. |
|||
Maximum Service Temperature, Air | 1350 °C | 2460 °F | |
Saint-Gobain Puropsil® B Infrared Grade Low [OH] Optical Fused Quartz Puropsil® B optical infrared fused quartz is manufactured from naturally occurring quartz crystal using a plasma process to ensure a low OH. It has excellent IR transmission with a useful IR tra.. |
|||
Maximum Service Temperature, Air | 1350 °C | 2460 °F | Extended periods if cycles remain above 300°C |
Saint-Gobain Vitreosil® CFQ/TSC Optical Fused Quartz Vitreosil® CFQ/TSC grades are for use in less demanding applications including viewing windows for use in corrosive and high temperature environments and non-optical components such as spacers, i.. |
|||
Maximum Service Temperature, Air | 1350 °C | 2460 °F | |
CeramTec Rocar® SiG Silicon Carbide, SiSiC Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch.. |
|||
Maximum Service Temperature, Air | 1350 °C | 2460 °F | limited |
Chosun Refractories INCT-135N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | >= 1350 °C | >= 2460 °F | |
China-Yixing Longly Refractories ASM-130 Cordierite-Mullite Featured mullite, cordierite as the main raw material, the use of advanced production technology, professionally manufacturing the kiln furniture of ceramic and powder metallurgy with load bearing b.. |
|||
Maximum Service Temperature, Air | 1350 °C | 2460 °F | limited |
Chosun Refractories GUN-135L Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1350 °C | 2460 °F | |
BNZ Materials Color A Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Maximum Service Temperature, Air | 1350 °C | 2460 °F | |
BNZ Materials Color B Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Maximum Service Temperature, Air | 1350 °C | 2460 °F | |
BNZ Materials Color CA Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |