Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 104 °C | 220 °F | Long Term |
Quadrant EPP Nylatron® GF30 Nylon Type 66, 30% Glass-Reinforced Black Color (ASTM Product Data Sheet) |
|||
Maximum Service Temperature, Air | 104 °C | 220 °F | Long Term |
Quadrant EPP Nylatron® GS Nylon, Extruded MoS2 Filled Type 66 (ASTM Product Data Sheet) |
|||
Maximum Service Temperature, Air | 104 °C | 220 °F | Long Term |
Quadrant EPP Nylatron® LFG (ASTM Product Data Sheet) |
|||
Maximum Service Temperature, Air | 104 °C | 220 °F | Long Term |
Quadrant EPP Nylatron® LIG Oil Filled Cast 6 Nylon (ASTM Product Data Sheet) |
|||
Maximum Service Temperature, Air | 104 °C | 220 °F | Long Term |
Quadrant EPP TIVAR® SuperPlus UHMW-PE, Glass-filled Cross-linked & Heat Stabilized Extreme Wear Resistant (ASTM Product Data Sheet) |
|||
Maximum Service Temperature, Air | 104 °C | 219 °F | Modified ISO 2796-1980; Typical maximum temperature to which parts can be exposed short term (1 hour) without significant deformation (<1%). |
NOVA Chemicals Dytherm® 150R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Maximum Service Temperature, Air | 104 °C | 219 °F | Modified ISO 2796-1980; Typical maximum temperature to which parts can be exposed short term (1 hour) without significant deformation (<1%). |
NOVA Chemicals Dytherm® 170F Expandable Polystyrene This is a special flame retardant grade consisting of spherical beads of a blend of polystyrene and polyphenylene ether containing pentane as expansion agent, and a internal flame-retardant additive.. |
|||
Maximum Service Temperature, Air | 104 °C | 220 °F | |
Quantum Nylon 6/6 Information provided by Quantum Advanced Engineering Plastics |
|||
Maximum Service Temperature, Air | 104 °C | 220 °F | |
Quantum Nylon 6/6 MoS2 Filled Information provided by Quantum Advanced Engineering Plastics |
|||
Maximum Service Temperature, Air | 104 °C | 220 °F | |
Quantum PBT Information provided by Quantum Advanced Engineering Plastics |
|||
Maximum Service Temperature, Air | 104 °C | 220 °F | |
Quantum PET Information provided by Quantum Advanced Engineering Plastics |
|||
Maximum Service Temperature, Air | 104 °C | 220 °F | |
Master Bond EP30-D10 Abrasion Resistant, Flexible Adhesive Compound Description: Master Bond Polymer System EP30-D10 is a versatile two component, abrasion resistant elastomer featuring superior strength, toughness and chemical resistance for high performance bondin.. |
|||
Maximum Service Temperature, Air | 104 °C | 220 °F | |
Loctite® 4014 Cyanoacrylate Adhesive Medical Grade BondersLoctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant products are designe.. |
|||
Maximum Service Temperature, Air | 104 °C | 220 °F | Long Term |
Ensinger NORYL® Polyphenylene oxide (PPO) NORYL®, due to its inherent chemical composition, exhibits unusually low moisture absorption. Therefore, good electrical insulating properties are realized over a wide range of humidity and temper.. |
|||
Maximum Service Temperature, Air | 104 °C | 219 °F | Service |
3M FP017802 Matte White Polypropylene Label Product 3M™ Matte White Polypropylene Label Products FP010602, FP010609 and FP017802 are matte white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3.. |
|||
Maximum Service Temperature, Air | 104 °C | 219 °F | Deflection Temp at unknown load |
Abatron AboCast 8103-13 One-Component Epoxy AboCast 8103-13 is the low-viscosity one-component clear epoxy system with deep impregnation that offers high performance at relatively high temperatures. It is best for thin-wall casting. Suggested.. |
|||
Maximum Service Temperature, Air | 104 °C | 219 °F | Long Term |
3M 4004 Double Coated Urethane Foam Tape 3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst.. |
|||
Maximum Service Temperature, Air | 104 °C | 219 °F | Long Term |
3M 4008 Double Coated Urethane Foam Tape 3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst.. |
|||
Maximum Service Temperature, Air | 104 °C | 219 °F | Long Term |
3M 4016 Double Coated Urethane Foam Tape 3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst.. |
|||
Maximum Service Temperature, Air | 104 °C | 219 °F | Long Term |
3M 4026 Double Coated Urethane Foam Tape 3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst.. |
|||
Maximum Service Temperature, Air | 104 °C | 219 °F | Long Term |
3M 4032 Double Coated Urethane Foam Tape 3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst.. |
|||
Maximum Service Temperature, Air | 104 °C | 219 °F | Long Term |
3M 4052 Double Coated Urethane Foam Tape 3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst.. |
|||
Maximum Service Temperature, Air | 104 °C | 219 °F | Long Term |
3M 4085 Double Coated Urethane Foam Tape 3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst.. |
|||
Maximum Service Temperature, Air | 104 °C | 219 °F | Service |
3M FP010609 Matte White Polypropylene Label Product 3M™ Matte White Polypropylene Label Products FP010602, FP010609 and FP017802 are matte white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3.. |
|||
Maximum Service Temperature, Air | 104 °C | 220 °F | |
Quantum Nylon 6/6 30% Glass Fiber Filled Information provided by Quantum Advanced Engineering Plastics |