| Category | Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) |
| Manufacturer | Quantum Advanced Engineering Plastics |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Quantum PET.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.34 g/cc | 1.34 g/cc | ASTM D792 |
| Water Absorption | 0.10 % | 0.10 % | ASTM D570 |
| Water Absorption at Saturation | 0.70 % | 0.70 % | ASTM D570 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 95 | 95 | ASTM D785 |
| Hardness, Rockwell R | 120 | 120 | ASTM D785 |
| Hardness, Shore D | 86 | 86 | ASTM 2240 |
| Tensile Strength | 79.3 MPa | 11500 psi | ASTM D638 |
| Elongation at Break | 50 % | 50 % | ASTM D638 |
| Tensile Modulus | 2.76 GPa | 400 ksi | ASTM D638 |
| Flexural Strength | 103 MPa | 15000 psi | ASTM D790 |
| Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
| Compressive Strength | 103 MPa | 15000 psi | ASTM D695 |
| Compressive Modulus | 2.90 GPa | 420 ksi | ASTM D695 |
| Shear Strength | 55.2 MPa | 8000 psi | ASTM D732 |
| Izod Impact, Notched | 0.267 J/cm | 0.500 ft-lb/in | ASTM D256 |
| Coefficient of Friction | 0.20 | 0.20 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 59.4 µm/m-°C | 33.0 µin/in-°F | ASTM D696 |
| Thermal Conductivity | 0.259 W/m-K | 1.80 BTU-in/hr-ft²-°F | ASTM C177 |
| Melting Point | 254 °C | 490 °F | ASTM D3417 |
| Maximum Service Temperature, Air | 104 °C | 220 °F | |
| Deflection Temperature at 0.46 MPa (66 psi) | 116 °C | 240 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 79.4 °C | 175 °F | ASTM D648 |
| Flammability, UL94 | HB | HB |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
| Dielectric Constant | 3.0 @Frequency 1.00e+6 Hz |
3.0 @Frequency 1.00e+6 Hz |
ASTM D150 |
| Dielectric Strength | 15.4 kV/mm | 390 kV/in | ASTM D149 |
| Dissipation Factor | 0.020 @Frequency 1.00e+6 Hz |
0.020 @Frequency 1.00e+6 Hz |
ASTM D150 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| FDA Compliance | yes |