Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 100 °C | 212 °F | Recommended |
Nye Lubricants 748C (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | Maximum operating temperature continuously for 5000 hours based on a tensile stress of 50% at 23° C. (dry sample) |
Omnia Plastica Akulon® PA6 G.Oil - Omniamid Oil - at 50% RH Cast Nylon 6 with the addition of 6% of special lubricating oil which remains in solution in the material. The unique method of production results in a micro distribution of oil particles with a hom.. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | Continuous; 20,000 h |
Quadrant EPP Ertalyte® PET, cast (ISO Data) The specific properties of this virgin crystalline PET make it especially suitable for the manufacture of mechanical precision parts which have to sustain high loads and/or are subject to wear. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | ISO.75 DN.53461 |
Polimersan Plastics POLIPA® (PA 6) Polyamide POLIPA® PA6 (POLYAMIDE) is produced by poly condensation of e-aminoacid and by the help of d-carbon acid and d-amine poly condensation. Its characteristics depend upon the numbers of the main struc.. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | 20,000 hr; IEC 216 |
Nilit Nilamid B3 H G3 15% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 6. These products combine good overall mechanical performance and impact strength with ease of processing. Key cha.. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | |
Parker Chomerics CHO-SEAL® 6435 Conductive Elastomer Description: Material of choice for high shielding effectiveness where NBC fluid resistance is needed; good performance in corrosive environments.Molded onlyRoHS CompliantInformation provided by Cho.. |
|||
Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | Long Term |
Kolon Kocetal® CL704 Reinforced Grade Acetal Copolymer
(discontinued **) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | |
Lehmann & Voss LUVOCOM® 1-1109 Polyamide 66, with glass fiber and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | |
Lehmann & Voss LUVOCOM® 80-7112/BK Polyacetal-copolymer, with glass fiber and carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically .. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | |
Lehmann & Voss LUVOCOM® 80-7580 Polyacetal-copolymer, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | |
Lehmann & Voss LUVOCOM® 80-7653 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Antistatic.No change of electric potential at bearings in case of separation of charge caused b.. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | |
Lehmann & Voss LUVOCOM® 80-8106 Polyacetal-copolymer, with carbon fiber, PTFE, easy flowing Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | |
Lehmann & Voss LUVOCOM® 80-8222 Polyacetal-copolymer, with mineral filler, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | |
Manifattura Cattaneo PP H Polypropylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | |
Lehmann & Voss LUVOCOM® 80-8003 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically .. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | |
Lehmann & Voss LUVOCOM® NSB 90 BK Polyamide 66, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | |
GEHR Plastics PP-30GF Polypropylene, 30% Glass Fiber Polypropylene shows a high mechanical strength and a tensile strength, but a low notched impact strength. PP resists stress cracking and it is easy to weld. At minus temperatures it can get brittle... |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | |
Zotefoams Plastazote® LD33 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | |
Tra-Con Tra-Bond FS163 Medium Viscosity Epoxy/Polyamide Adhesive TRA-BOND FS163 is a medium viscosity polyamide/epoxy adhesive recommended for industrial bonding and sealing applications where toughness, impact resistance, and superior mechanical properties are r.. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | |
Trelleborg Commercial Neoprene® C653 Chloroprene CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade.. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | |
Zotefoams Plastazote® LD29 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | 5000 h; VDE 0304/P2-1, IEC 216 |
EPICHEM PA 66 GF 30 Polyamide 66, 30% Glass Characteristics: 30% glass fibre filled |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | Continuous |
Epoxy Technology EPO-TEK® 302 Fast Setting, Optical Epoxy Product Description: EPO-TEK® 302 is a two component, fast-gelling, room temperature curing epoxy, designed for electronic, optical, medical, and general applications. Advantages & Application No.. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | |
Alliance N-40M Neodymium Iron Boron Magnetic Material |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | |
BASF Ultraform® N2640 Z2 POM + PUR Description: Elastomer-modified injection molding grade with high impact strength for clips, snap and fastening elements, and also for components subject to impact stress.Information provided by BAS.. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | |
BASF Ultraform® W2320 U035 LEV POM Description: Is a POM, UV-stabilized, very free-flowing, rapidly solidifying grade for injection molding, with reduced emission potential.Information provided by BASF |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | Dry |
3M Scotchkote™ GP 830 WB Epoxy Primer 3M Scotchkote WB Epoxy Primer GP 830 is a member of a range of Scotchkote waterborne coatings and has been specifically developed as a primer/tie coat for use on sealed mineral surfaces and existing.. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | Long Term |
CENTROPLAST CENTRODAL LF Polyoxymethylene conductive This material is electrically conductive, with high mechanical strength and dimensional stability. Applications include structural components in potentially explosive areas, components for divertin.. |
|||
Maximum Service Temperature, Air | 100 - 130 °C | 212 - 266 °F | long term; EMS |
EMS-Grivory Grivory® XE 4192 black 9992 PA610-GF30 Information provided by EMS Grivory |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | long term; EMS |
EMS-Grivory Grivory® TS FR PA666 FR Information provided by EMS Grivory |