Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.10 W/m-K @Pressure 2.07 MPa |
7.63 BTU-in/hr-ft²-°F @Pressure 300 psi |
ASTM D5470 |
Parker Chomerics CHO-SEAL® 6371 Conductive Elastomer Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Molded onlyRoHS Compliant Information provided by C.. |
|||
Thermal Conductivity | 1.10 W/m-K | 7.63 BTU-in/hr-ft²-°F | MIL-I-49456a |
Parker Chomerics CHO-THERM® 1646 Non-Insulating Interface Material Description: CHO-THERM® 1646 pads offer the best available thermal performance, without the use of grease, in applications where electrical isolation is not required. The low thermal impedance of C.. |
|||
Thermal Conductivity | 1.10 W/m-K | 7.63 BTU-in/hr-ft²-°F | ASTM E 1530 |
SABIC Innovative Plastics LNP KONDUIT ITF2B PA 6/12 (Asia Pacific) LNP* Konduit* ITF2B is a compound based on Nylon 6/12 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Thermal Conductivity | 1.10 W/m-K | 7.63 BTU-in/hr-ft²-°F | ASTM E 1530 |
SABIC Innovative Plastics LNP KONDUIT PTF2BXXX PA 6 (Europe-Africa-Middle East) LNP KONDUIT* PTF2BXXX is a compound based on Nylon 6 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Thermal Conductivity | 1.10 W/m-K | 7.63 BTU-in/hr-ft²-°F | through-plane, ø80*3mm discs; ISO 22007-2 |
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 compound |
|||
Thermal Conductivity | 1.10 W/m-K | 7.63 BTU-in/hr-ft²-°F | through-plane, ø80*3mm discs; ISO 22007-2 |
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 (Europe-Africa-Middle East) Thermally conductive mineral filled PA6 compound |
|||
Thermal Conductivity | 1.10 W/m-K | 7.63 BTU-in/hr-ft²-°F | through-plane, ø80*3mm discs; ISO 22007-2 |
SABIC Innovative Plastics LNP KONDUIT PX11311U PA 6 (Europe-Africa-Middle East) Thermally conductive mineral and glass fiber filled PA6 compliant with ECO protocols, non-brominated, non chlorinated |
|||
Thermal Conductivity | 1.10 W/m-K | 7.63 BTU-in/hr-ft²-°F | Tested in accordance with ASTM F433; ASTM C177 |
LNP Konduit® OTF-212-11 Polyphenylene Sulfide, Proprietary Filler
(discontinued **) Features: Thermally ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades ar.. |
|||
Thermal Conductivity | 1.10 W/m-K @Temperature 25.0 °C |
7.63 BTU-in/hr-ft²-°F @Temperature 77.0 °F |
|
Mateck Cesium Iodide, CsI Optical crystals |
|||
Thermal Conductivity | 1.10 W/m-K @Temperature 127 °C |
7.63 BTU-in/hr-ft²-°F @Temperature 261 °F |
|
Schott AF 45 Thin Borosilicate Glass AF 45 is an alkali-free modified borosilicate glass with a high content of BaO and Al2O3. AF 45 with, its specific properties and large range of different thicknesses with tight tolerances, is exc.. |
|||
Thermal Conductivity | 1.10 W/m-K @Temperature 90.0 °C |
7.63 BTU-in/hr-ft²-°F @Temperature 194 °F |
|
Schott Glass 8253 Alkaline Earth Aluminosilicate Glass Alkaline earth aluminosilicate glass for high temperature application in electrical engineering, for sealing to molybdenum, for use at higher temperatures than glass 8252, free from alkali Bulb and.. |
|||
Thermal Conductivity | 1.10 W/m-K @Temperature 90.0 °C |
7.63 BTU-in/hr-ft²-°F @Temperature 194 °F |
|
Schott Glass 8516 Sealing Glass Sealing glass for Fe-Ni alloys, high IR-absorbing, lead-free, of poor evaporation Reed switches The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is below 10.. |
|||
Thermal Conductivity | 1.10 W/m-K @Temperature 90.0 °C |
7.63 BTU-in/hr-ft²-°F @Temperature 194 °F |
|
Schott Glass 8625 Biocompatible Glass Biocompatible glass, high IR-absorbing, Transponders (implantable) The heavy metal content of the elements lead, cadmium, mercury, and hexavalent chromium is below 100 ppmInformation provided by S.. |
|||
Thermal Conductivity | 1.10 W/m-K | 7.63 BTU-in/hr-ft²-°F | |
Sharadaa Ceramics REFINSUL 15 Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Thermal Conductivity | 1.10 W/m-K | 7.63 BTU-in/hr-ft²-°F | |
Sharadaa Ceramics REFINSUL 9 Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Thermal Conductivity | 1.10 W/m-K @Temperature 90.0 °C |
7.63 BTU-in/hr-ft²-°F @Temperature 194 °F |
|
Schott Glass 8252 Alkaline Earth Aluminosilicate Glass Alkaline earth aluminosilicate glass for high temperature applications in electrical engineering, for sealing to molybdenum, free from alkali Bulb and exhaust tube for halogen lamps for automotive,.. |
|||
Thermal Conductivity | 1.10 W/m-K @Temperature 121 °C |
7.63 BTU-in/hr-ft²-°F @Temperature 250 °F |
|
Tra-Con Tra-Bond 7560D Hydrolytically Stable Adhesive TRA-BOND 7560D is an electrically insulating epoxy adhesive. This material has a 10 day work life and a medium viscosity for easy usage. There are also multiple cure options that make this product i.. |
|||
Thermal Conductivity | 1.10 - 1.50 W/m-K @Temperature 25.0 - 300 °C |
7.63 - 10.4 BTU-in/hr-ft²-°F @Temperature 77.0 - 572 °F |
|
China-Yixing Longly Refractories Cordierite Ceramics (Heat Resistance Ceramics) LONGLY's cordierite ceramics' main crystal phrase is 2MgO-2Al2O2-5SiO2, this composition has low thermal expansion coefficient and excellent thermal shock resistance. Maximum service temperature is.. |
|||
Thermal Conductivity | 1.10 W/m-K | 7.63 BTU-in/hr-ft²-°F | |
Epoxy Technology EPO-TEK® H31 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H31 is a single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and opto-electronic.. |
|||
Thermal Conductivity | 1.10 W/m-K | 7.63 BTU-in/hr-ft²-°F | z |
Arlon TC600 Glass, PTFE and Micro-Dispersed Ceramic High Thermal Conductivity, Excellent Dielectric Constant Control and Phase Stability with TemperatureInformation provided by Arlon Materials for Electronics (MED). |
|||
Thermal Conductivity | 1.10 - 1.40 W/m-K | 7.63 - 9.72 BTU-in/hr-ft²-°F | |
AGY ZenTron® S-2 Generic S-Glass Fiber S-2 glass and S-glass have the same composition. S-glass is no longer made by AGY, but used to have a reactive epoxy size. Various silanes and starch oil are used as binders. Acid resistant. Mod.. |
|||
Thermal Conductivity | 1.10 W/m-K @Temperature 90.0 °C |
7.63 BTU-in/hr-ft²-°F @Temperature 194 °F |
|
Schott Glass 8241 Alkaline Earth Aluminosilicate Glass Alkaline earth aluminosilicate glass for high temperature application in electrical engineering, for sealing to molybdenum, free from alkali, blue colored, defined absorption Bulb and exhaust tube .. |
|||
Thermal Conductivity | 1.10 W/m-K | 7.63 BTU-in/hr-ft²-°F | Longitudinal |
LATI Laticonther 62 CEG/500-V0HF1 PA 6, Glass/Mineral Reinforced, Flame Retardant High thermal conductivity product based on Polyamide 6 (PA6). Glass fibers / Mineral filler. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Mid.. |
|||
Thermal Conductivity | 1.10 - 1.20 W/m-K | 7.63 - 8.33 BTU-in/hr-ft²-°F | Average value: 1.13 W/m-K Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Black Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Black Filled". Each property range of values reported is minimu.. |