Thermal Properties Metric English Comments
Thermal Conductivity 1.10 W/m-K
7.63 BTU-in/hr-ft²-°F
Resinlab® EP1285HD-16 Highly Filled, Medium Viscosity Casting Resin
Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C..
Thermal Conductivity 1.10 W/m-K
7.63 BTU-in/hr-ft²-°F
MIL-I-49456a
Parker Chomerics CHO-THERM® 1646 Non-Insulating Interface Material
Description: CHO-THERM® 1646 pads offer the best available thermal performance, without the use of grease, in applications where electrical isolation is not required. The low thermal impedance of C..
Thermal Conductivity 1.10 W/m-K
7.63 BTU-in/hr-ft²-°F
ASTM E 1530
SABIC Innovative Plastics LNP KONDUIT MT00E PP
LNP KONDUIT* MT00E is a compound based on Polypropylene resin containing 70% Proprietary Thermal Filler. Added features of this material include: Thermally Conductive.
Thermal Conductivity 1.10 W/m-K
7.63 BTU-in/hr-ft²-°F
ASTM E 1530
SABIC Innovative Plastics LNP KONDUIT MT00E PP (Europe-Africa-Middle East)
LNP KONDUIT* MT00E is a compound based on Polypropylene resin containing Proprietary Thermal Filler. Added features of this material include: Thermally Conductive.
Thermal Conductivity 1.10 W/m-K
7.63 BTU-in/hr-ft²-°F
ASTM E 1530
SABIC Innovative Plastics LNP KONDUIT PTF2BXXX PA 6
LNP KONDUIT* PTF2BXXX is a compound based on Nylon 6 resin containing 10% Glass Fiber, 55% Proprietary Thermal Filler. Added features of this material include: Thermally Conductive.
Thermal Conductivity 1.10 W/m-K
7.63 BTU-in/hr-ft²-°F
ASTM E 1530
SABIC Innovative Plastics LNP KONDUIT PTF2BXXX PA 6 (Asia Pacific)
LNP KONDUIT* PTF2BXXX is a compound based on Nylon 6 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive.
Thermal Conductivity 1.10 W/m-K
7.63 BTU-in/hr-ft²-°F
through-plane, ø80*3mm discs; ISO 22007-2
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6
LNP* Konduit* PX08321 a compound based on PA6 resins containing mineral. Added features include: Thermally Conductive.
Thermal Conductivity 1.10 W/m-K
7.63 BTU-in/hr-ft²-°F
through-plane, ø80*3mm discs; ISO 22007-2
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 (Asia Pacific)
Thermally conductive mineral filled PA6 compound
Thermal Conductivity 1.10 W/m-K
7.63 BTU-in/hr-ft²-°F
through-plane, ø80*3mm discs; ISO 22007-2
SABIC Innovative Plastics LNP KONDUIT PX11311U PA 6 (Europe-Africa-Middle East)
Thermally conductive mineral and glass fiber filled PA6 compliant with ECO protocols, non-brominated, non chlorinated
Thermal Conductivity 1.10 W/m-K
7.63 BTU-in/hr-ft²-°F
HOT-DISK || 60x60x3 mm
Lehmann & Voss LUVOCOM® 1301/CF/20 PPS, linear, with carbon fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
Thermal Conductivity 1.10 W/m-K

@Temperature 25.0 °C
7.63 BTU-in/hr-ft²-°F

@Temperature 77.0 °F
Mateck Cesium Iodide, CsI
Optical crystals
Thermal Conductivity 1.10 W/m-K

@Temperature 127 °C
7.63 BTU-in/hr-ft²-°F

@Temperature 261 °F
Schott AF 45 Thin Borosilicate Glass
AF 45 is an alkali-free modified borosilicate glass with a high content of BaO and Al2O3. AF 45 with, its specific properties and large range of different thicknesses with tight tolerances, is exc..
Thermal Conductivity 1.10 W/m-K

@Temperature 90.0 °C
7.63 BTU-in/hr-ft²-°F

@Temperature 194 °F
Schott Glass 8271 Borosilicate Glass
Borosilicate glass, highly UV-blocked, stabilized against solarization. Used for sealing glass to KOVAR metal and backlights. The heavy metal content for the elements lead, cadmium, mercury, and hex..
Thermal Conductivity 1.10 W/m-K

@Temperature 90.0 °C
7.63 BTU-in/hr-ft²-°F

@Temperature 194 °F
Schott Glass 8516 Sealing Glass
Sealing glass for Fe-Ni alloys, high IR-absorbing, lead-free, of poor evaporation Reed switches The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is below 10..
Thermal Conductivity 1.10 W/m-K

@Temperature 90.0 °C
7.63 BTU-in/hr-ft²-°F

@Temperature 194 °F
Schott Glass 8625 Biocompatible Glass
Biocompatible glass, high IR-absorbing, Transponders (implantable) The heavy metal content of the elements lead, cadmium, mercury, and hexavalent chromium is below 100 ppmInformation provided by S..
Thermal Conductivity 1.10 W/m-K
7.63 BTU-in/hr-ft²-°F
Sharadaa Ceramics REFINSUL 15 Insulating Castables Medium/High Purity
Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan..
Thermal Conductivity 1.10 W/m-K
7.63 BTU-in/hr-ft²-°F
Sharadaa Ceramics REFINSUL 9 Insulating Castables Medium/High Purity
Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan..
Thermal Conductivity 1.10 W/m-K

@Temperature 90.0 °C
7.63 BTU-in/hr-ft²-°F

@Temperature 194 °F
Schott Glass 8252 Alkaline Earth Aluminosilicate Glass
Alkaline earth aluminosilicate glass for high temperature applications in electrical engineering, for sealing to molybdenum, free from alkali Bulb and exhaust tube for halogen lamps for automotive,..
Thermal Conductivity 1.10 - 1.50 W/m-K

@Temperature 25.0 - 300 °C
7.63 - 10.4 BTU-in/hr-ft²-°F

@Temperature 77.0 - 572 °F
China-Yixing Longly Refractories Cordierite Ceramics (Heat Resistance Ceramics)
LONGLY's cordierite ceramics' main crystal phrase is 2MgO-2Al2O2-5SiO2, this composition has low thermal expansion coefficient and excellent thermal shock resistance. Maximum service temperature is..
Thermal Conductivity 1.10 W/m-K
7.63 BTU-in/hr-ft²-°F
Epoxy Technology EPO-TEK® H31 Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® H31 is a single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and opto-electronic..
Thermal Conductivity 1.10 W/m-K
7.63 BTU-in/hr-ft²-°F
z
Arlon TC600 Glass, PTFE and Micro-Dispersed Ceramic
High Thermal Conductivity, Excellent Dielectric Constant Control and Phase Stability with TemperatureInformation provided by Arlon Materials for Electronics (MED).
Thermal Conductivity 1.10 - 1.40 W/m-K
7.63 - 9.72 BTU-in/hr-ft²-°F
AGY ZenTron® S-2 Generic S-Glass Fiber
S-2 glass and S-glass have the same composition. S-glass is no longer made by AGY, but used to have a reactive epoxy size. Various silanes and starch oil are used as binders. Acid resistant. Mod..
Thermal Conductivity 1.10 W/m-K
7.63 BTU-in/hr-ft²-°F
Tested in accordance with ASTM F433; ASTM C177
LNP Konduit® ITF-212-11 Polyamide 6/12 Copolymer  (discontinued **)
Features: Thermally ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades ar..
Thermal Conductivity 1.10 W/m-K

@Temperature 90.0 °C
7.63 BTU-in/hr-ft²-°F

@Temperature 194 °F
Schott Glass 8241 Alkaline Earth Aluminosilicate Glass
Alkaline earth aluminosilicate glass for high temperature application in electrical engineering, for sealing to molybdenum, free from alkali, blue colored, defined absorption Bulb and exhaust tube ..
Copyright © lookpolymers.com All Rights Reserved