Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.950 W/m-K @Temperature 80.0 °C |
6.59 BTU-in/hr-ft²-°F @Temperature 176 °F |
Z Direction; ASTM C518 |
Rogers Corporation RO3010 Ceramic-Filled PTFE Composite, High Frequency Circuit Material Features and Benefits: |
|||
Thermal Conductivity | 0.950 W/m-K | 6.59 BTU-in/hr-ft²-°F | ASTM D5470 |
Parker Chomerics THERM-A-FORM 1642 Cure-in-Place Potting and Underfill Material Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co.. |
|||
Thermal Conductivity | 0.950 W/m-K | 6.59 BTU-in/hr-ft²-°F | Average; ISO 22007-4 |
Victrex® PEEK 150CA30 30% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, FDA food contact c.. |
|||
Thermal Conductivity | 0.950 W/m-K | 6.59 BTU-in/hr-ft²-°F | Average; ISO 22007-4 |
Victrex® PEEK 450CA30 30% Carbon Fiber Reinforced General purpose, 30% carbon fiber reinforced, pelletized grade for injection molding.Information provided by Victrex. |
|||
Thermal Conductivity | 0.950 W/m-K | 6.59 BTU-in/hr-ft²-°F | Average; ISO 22007-4 |
Victrex® PEEK 650CA30 30% Carbon Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, FDA food contact compliant.. |
|||
Thermal Conductivity | 0.950 W/m-K @Temperature 23.0 °C |
6.59 BTU-in/hr-ft²-°F @Temperature 73.4 °F |
Average; ISO/CD 22007-4 |
Victrex® PEEK 90CA30 Polyetheretherketone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food cont.. |
|||
Thermal Conductivity | 0.950 W/m-K @Temperature 23.0 °C |
6.59 BTU-in/hr-ft²-°F @Temperature 73.4 °F |
Average; ISO/CD 22007-4 |
Victrex® PEEK -HT™ 22CA30 PolyEtherKetone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact com.. |
|||
Thermal Conductivity | 0.950 W/m-K | 6.59 BTU-in/hr-ft²-°F | |
Schott N-K5 Glass Information Provided by SCHOTT North America, Inc. |
|||
Thermal Conductivity | 0.950 W/m-K | 6.59 BTU-in/hr-ft²-°F | |
Schott N-SF11 Glass Information Provided by SCHOTT North America, Inc. |
|||
Thermal Conductivity | 0.950 W/m-K | 6.59 BTU-in/hr-ft²-°F | |
Schott N-SF4 Glass Information Provided by SCHOTT North America, Inc. |
|||
Thermal Conductivity | 0.950 W/m-K | 6.59 BTU-in/hr-ft²-°F | |
Dow Corning SE 4430 KIT Two-part, thermally conductive elastomer, soft, good thermal conducitvity, UL 94 V-0 rating, low viscosity.Information provided by Dow Corning |
|||
Thermal Conductivity | 0.950 W/m-K | 6.59 BTU-in/hr-ft²-°F | |
Schott N-KZFS5 Glass Information Provided by SCHOTT North America, Inc. |