Material Notes:
Two-part, thermally conductive elastomer, soft, good thermal conducitvity, UL 94 V-0 rating, low viscosity.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 2.20 g/cc

@Temperature 25.0 °C
2.20 g/cc

@Temperature 77.0 °F
Viscosity 5600 cP
5600 cP
dynamic
Mechanical Properties Metric English Comments
Hardness, Shore OO 70
70
Tensile Strength, Ultimate 0.414 MPa
60.0 psi
Penetration P(0), 1/10 mm 35
35
Thermal Properties Metric English Comments
CTE, linear 174 µm/m-°C
96.7 µin/in-°F
Thermal Conductivity 0.950 W/m-K
6.59 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.90e+14 ohm-cm
1.90e+14 ohm-cm
Dielectric Constant 4.0

@Frequency 1.00e+6 Hz
4.0

@Frequency 1.00e+6 Hz
4.6

@Frequency 100 Hz
4.6

@Frequency 100 Hz
4.6

@Frequency 100000 Hz
4.6

@Frequency 100000 Hz
Dielectric Strength 17.9 kV/mm
455 kV/in
Dissipation Factor 0.00015

@Frequency 100000 Hz
0.00015

@Frequency 100000 Hz
0.0020

@Frequency 100 Hz
0.0020

@Frequency 100 Hz
Processing Properties Metric English Comments
Cure Time 1.90 min

@Temperature 150 °C
0.0317 hour

@Temperature 302 °F
2.50 min

@Temperature 125 °C
0.0417 hour

@Temperature 257 °F
3.50 min

@Temperature 100 °C
0.0583 hour

@Temperature 212 °F
420 min

@Temperature 22.0 °C
7.00 hour

@Temperature 71.6 °F
Shelf Life 8.00 Month
8.00 Month
Descriptive Properties Value Comments
Color grey
Hydrophobic yes
Self Leveling yes
Water Resistant yes
Working Time (min) 240