Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.50 - 2.00 W/m-K | 10.4 - 13.9 BTU-in/hr-ft²-°F | ASTM E1461 |
PolyOne Trilliant™ HC HC6200-5002 XR Grey Polyamide 12 (Nylon 12) The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead.. |
|||
Thermal Conductivity | 1.51 W/m-K @Temperature 500 °C |
10.4 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Potters Industries Spheriglass® 2429 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Thermal Conductivity | 1.51 W/m-K @Temperature 500 °C |
10.4 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Potters Industries Spheriglass® 3000 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Thermal Conductivity | 1.50 W/m-K | 10.4 BTU-in/hr-ft²-°F | through-plane, 10*10*3mm sample; ASTM E 1461-07 |
SABIC Innovative Plastics LNP KONDUIT PX09322 PA 6 (Asia Pacific) White colored thermally conductive mineral filled PA6 FR compound |
|||
Thermal Conductivity | 1.50 - 4.69 W/m-K @Pressure 30.0 - 30.0 MPa |
10.4 - 32.5 BTU-in/hr-ft²-°F @Pressure 4350 - 4350 psi |
Average value: 1.94 W/m-K Grade Count:4 |
Overview of materials for Silicone, Molded, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
Thermal Conductivity | 1.50 - 4.69 W/m-K @Temperature 50.0 - 50.0 °C |
10.4 - 32.5 BTU-in/hr-ft²-°F @Temperature 122 - 122 °F |
Average value: 2.08 W/m-K Grade Count:4 |
Overview of materials for Silicone Rubber This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Thermal Conductivity | 1.50 - 4.69 W/m-K @Pressure 30.0 - 30.0 MPa |
10.4 - 32.5 BTU-in/hr-ft²-°F @Pressure 4350 - 4350 psi |
Average value: 2.08 W/m-K Grade Count:4 |
Overview of materials for Silicone Rubber This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Thermal Conductivity | 1.50 W/m-K | 10.4 BTU-in/hr-ft²-°F | 60°C for 1,000 hrs with 90% RH; JIS-R-2618 |
Fujipoly Industries Sarcon® 25G-Td Thin-Film GR-TD Sarcon 25G-Td is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary.Information provided by Fujipoly Industries |
|||
Thermal Conductivity | 1.50 W/m-K | 10.4 BTU-in/hr-ft²-°F | 60°C for 1,000 hrs with 90% RH; JIS-R-2618 |
Fujipoly Industries Sarcon® GR-d Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary.Information provided by Fujipoly Industries |
|||
Thermal Conductivity | 1.50 W/m-K | 10.4 BTU-in/hr-ft²-°F | 70°C for 1,000 hrs; JIS-R-2618 |
Fujipoly Industries Sarcon® GR-Fd Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-Fd has a mesh embedded overall.Information provided b.. |
|||
Thermal Conductivity | 1.50 W/m-K | 10.4 BTU-in/hr-ft²-°F | 70°C for 1,000 hrs; JIS-R-2618 |
Fujipoly Industries Sarcon® GR-Hd Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-Hd has a hardened top surface.Information provided by.. |
|||
Thermal Conductivity | 1.50 W/m-K @Temperature 90.0 °C |
10.4 BTU-in/hr-ft²-°F @Temperature 194 °F |
DIN 51936, ASTM E 1461-01 |
Schott Nextrema® 712-8 Glass Ceramic The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal.. |
|||
Thermal Conductivity | 1.50 W/m-K | 10.4 BTU-in/hr-ft²-°F | |
Tra-Con Tra-Duct 2916 Room Temperature Conductive Silver Epoxy Adhesive TRA-DUCT 2916 is an electrically conductive, silver-filled epoxy formulation recommended for electronic bonding, coating, and sealing applications that require high flexibility coupled with good ele.. |
|||
Thermal Conductivity | 1.50 W/m-K | 10.4 BTU-in/hr-ft²-°F | |
Tra-Con Tra-Duct 2916T Room Temperature Conductive Silver Epoxy Adhesive TRA-DUCT 2916T is an electrically conductive, silver-filled epoxy formulation recommended for electronic bonding, coating, and sealing applications that require high flexibility coupled with good el.. |
|||
Thermal Conductivity | 1.50 W/m-K | 10.4 BTU-in/hr-ft²-°F | |
Tra-Con Tra-Duct 2958 Snap Cure Conductive Silver Epoxy Adhesive TRA-DUCT 2958 is a two-part, smooth paste of specially refined and processed epoxy and silver components, recommended for electronic, microelectronic and die-attach bonding and sealing applications .. |
|||
Thermal Conductivity | 1.50 W/m-K | 10.4 BTU-in/hr-ft²-°F | |
Tra-Con Tra-Duct 2924 Conductive Silver Epoxy Adhesive TRA-DUCT 2924 is a two part electrically conductive composition developed for low shrinkage, low resistivity bonding applications where good electrical and physical properties over a wide temperatur.. |
|||
Thermal Conductivity | 1.50 W/m-K | 10.4 BTU-in/hr-ft²-°F | |
Tra-Con Tra-Duct 2956 Low Ion Snap Cure Silver Epoxy Adhesive TRA-DUCT 2956 is recommended for the bonding and sealing of electronic components where a combination of electrical and mechanical properties are required. This two-part, smooth, paste system of sil.. |
|||
Thermal Conductivity | 1.50 W/m-K | 10.4 BTU-in/hr-ft²-°F | |
Epoxy Technology EPO-TEK® H35-175MPLV Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H35-175MPLV is a single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and opto-el.. |
|||
Thermal Conductivity | 1.50 W/m-K | 10.4 BTU-in/hr-ft²-°F | Silicone Property; ASTM E 1530 |
Arlon Thermabond® R36300W015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Primers: Dow Corning S2260Appearance: White silicone gumThis data represents typical val.. |
|||
Thermal Conductivity | 1.50 W/m-K @Temperature 20.0 - 100 °C |
10.4 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
Anderman Ceramics EM60P Sillimanite Porous synthetic mullite with high thermal shock. Available as tube up to 10 ft (3 m) long with diameters 0.6" to 2.4".Information provided by Anderman Ceramics. |
|||
Thermal Conductivity | >= 1.50 W/m-K | >= 10.4 BTU-in/hr-ft²-°F | COLORA |
Aptek 2313-PMF Hybrid Epoxy Adhesive Snap-cure, silver-filled; long pot-life/stable viscosity-excellent for robotics. Thermal shock resistant.Production-oriented, snap-cure technology for surface mount applications-allows cure during s.. |
|||
Thermal Conductivity | 1.50 W/m-K | 10.4 BTU-in/hr-ft²-°F | |
Atom Adhesives AA-DUCT 916 Epoxy Adhesive AA-DUCT 916 is an electrically conductive, silver-filled epoxy formulation recommended for electronic bonding, coating, and sealing applications that require high flexibility coupled with good elect.. |
|||
Thermal Conductivity | 1.50 W/m-K | 10.4 BTU-in/hr-ft²-°F | HOT-DISK || 60x60x3 mm |
Lehmann & Voss LUVOCOM® 1301-0824 PPS, linear, with carbon fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc.. |