Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | |
Quadrant EPP Duratron® PAI T4203 PAI, unfilled, extruded (ISO Data) Duratron T4203 PAI offers the best toughness and impact strength of all Duratron PAI grades. This extruded Duratron PAI grade is very popular for precision parts in high-tech equipment. In addition,.. |
|||
Thermal Conductivity | 0.259 - 0.331 W/m-K | 1.80 - 2.30 BTU-in/hr-ft²-°F | |
Polygon Polylube™ Fiber Series Epoxy Composite Bearings Low friction coupled with high load carrying capacity are natural benefits. Teflon® superfilaments, which exhibit tensile strength twenty times greater than PTFE resins are integrated into the bea.. |
|||
Thermal Conductivity | 0.259 - 0.540 W/m-K | 1.80 - 3.75 BTU-in/hr-ft²-°F | Average value: 0.392 W/m-K Grade Count:6 |
Overview of materials for Polyamide-Imide, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Molded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Torlon® 4200 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4200 is an unreinforced, unpigmented grade of polyamide-imide (PAI) resin for extrusion. This grade is designed for applications in the semiconductor industry which cannot tolerate particulat.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Torlon® 4203L Polyamide-imide (PAI)
(Unverified Data**) Torlon 4203L is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin. It has the best impact resistance and greatest elongation of all the Torlon grades. Torlon PAI has the hi.. |
|||
Thermal Conductivity | 0.259 - 1.26 W/m-K | 1.80 - 8.72 BTU-in/hr-ft²-°F | Average value: 0.795 W/m-K Grade Count:7 |
Overview of materials for Epoxy, Encapsulating, Glass or Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Glass or Mineral Filled". Each property range of values reported is minimum and ma.. |
|||
Thermal Conductivity | 0.259 - 0.576 W/m-K | 1.80 - 4.00 BTU-in/hr-ft²-°F | Average value: 0.398 W/m-K Grade Count:26 |
Overview of materials for Nylon 612, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of .. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 20-0778 Polyphthalamide, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | |
Ineos Barex® 218 E Acrylonitrile-Methyl Acrylate Copolymer Extrusion Grade. Barex® Resins are available in either natural or blue tint. Barex® 218E is most commonly used for thermoformed sheet applications in which high impact performance is require.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV511 White Extreme Low Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM 1100F PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant. Effective June, 2007 this grade will no longer be supported with b.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM 1110F PEI (Europe-Africa-Middle East) Enhanced flow PolyetherimiEnhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant. Effective June, 2007 this grade will no long.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Ultem 1110R PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Ultem 1110R PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | |
Styron CALIBRE™ 200 4 Polycarbonate, General Purpose CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins .. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS (Europe-Africa-Middle East) Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL GTX GTX830 PPE+PA (Europe-Africa-Middle East) NORYL GTX830 a 30% glass reinforced grade which offers an excellent combination of chemical/heat resistance in combination with stiffness. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Noryl HB1525 PPE+HIPS (Europe-Africa-Middle East) NORYL HB1525 is a 15 % short glass fibre reinforced material with a HDT/A of 115°C according ISO 75. NORYL HB1525 is an easy flow material designed for applications where dimensional stability an.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | |
Trelleborg Offshore Vikotherm™ 73780 Insulative Elastomer Vikotherm™ is a rubber elastomer chemically modified to provide very high insulating characteristics while maintaining its inherent rubber properties in respect of seawater resistance, pressure res.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | of melt |
DuPont Performance Polymers Zytel® FE5382 BK276 Nylon 612
(Unverified Data**) 33% Glass Reinforced Polyamide 612 Developed for Electrical and Electronics Applications Zytel FE5382 BK276 is a 33% glass fiber reinforced heat stabilized black polyamide 612 resin developed for el.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | of melt |
DuPont Performance Polymers Zytel® RS 30G30HSL BK038A Nylon 610 30% Glass Reinforced Renewably Sourced Polyamide 610 Developed for Extrusion Information provided by DuPont Performance Polymers |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Torlon® 4203 Polyamide-imide (PAI)
(discontinued **) Torlon 4203 is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin for extrusion. It has the best impact resistance and greatest elongation of all the Torlon grades. Torlon P.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ASTM C-177 |
Glastic GLASGUARD Scuff and Bulkhead Liners GlasGuard Scuff and Bulkhead Liners serve as a method of protecting trailer walls from damage caused by forklift trucks and careless loading and unloading of freight. Manufactured of 1/4" thick fib.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Valox® VX4930 PBT (Europe-Africa-Middle East) VALOX VX4930 is a 30% glass reinforced nucleated PBT/ASA blend with excellent mechanical properties, high dimensional stability and low density. Applications: connectors and automotive industry. |
|||
Thermal Conductivity | 0.259 W/m-K | 1.80 BTU-in/hr-ft²-°F | ASTM C177 |
Quantum PEI - Ultem® 30% Glass Fiber Filled Information provided by Quantum Advanced Engineering Plastics |