Thermal Properties Metric English Comments
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
DIN.52612
Omnia Plastica PEEK Polyetheretherketone
Semicrystalline polymer. Material with high mechanical and thermal properties, up to 240°C. It resists to creep under load and to wear, its friction coefficient is low. The temperature resistance w..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
Premix Premi-Glas® 8101 Glass Reinforced Polyester BMC
Description: Premi-Glas® 8101 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits: Ex..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
ASTM C 177
SABIC Innovative Plastics Cycoloy® LG8002 PC+ABS (Asia Pacific)
Automotive. Low gloss, high impact and ductility at 73F and -22F. UV-stable colors.This data was supplied by SABIC-IP for the Asia Pacific region.
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
Quadrant EPP Ketron® 1000 PEEK unfilled, extruded (ISO Data)
Ketron PEEK-1000 stock shapes are produced from virgin polyetheretherketone resin and offer the highest toughness and impact strength of all Ketron PEEK grades. Both Ketron PEEK-1000 natural & black..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
ASTM C177
SABIC Innovative Plastics Lexan® 221R PC (Asia Pacific)
17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release.
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
ASTM C 177
SABIC Innovative Plastics Lexan® 223 PC
17.5 MFR, for small, intricate parts. Improved flame retardance. UV stabilized.This data was supplied by SABIC-IP for the Americas region.
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
ASTM C177
SABIC Innovative Plastics Lexan® LUX2114G PC (Asia Pacific)
18 MFR. Improved flame retardance. Internal mold release. UV stabilized.
Thermal Conductivity 0.251 W/m-K
1.74 BTU-in/hr-ft²-°F
Quadrant EPP Ketron® LSG PEEK-CLASSIX Biocompatibility tested (ASTM Product Data Sheet)
KETRON® PEEK-CLASSIX LSG white stock shapes are produced from Invibio® PEEK-CLASSIX White resin. This material exhibits a unique combination of mechanical properties, temperature and chemical re..
Thermal Conductivity >= 0.250 W/m-K
>= 1.74 BTU-in/hr-ft²-°F
ASTM C177
LG Chemical LUCON PO-5300M Electrically Conductive Thermoplastic
LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
DIN 52612
Lehmann & Voss LUVOCOM® 1105/RD7405 PEEK, unreinforced
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
DIN 52612
Schwartz Technical Plastics LAMIGAMID® 309 Cast Polyamide 6, Oil Filled, Conditioned
Application: slippers, inserts for coupling boxes, wear linersInformation provided by Schwartz Technical Plastics GmbH
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
ISO 8302
SABIC Innovative Plastics Valox® 420SE0U PBT
PBT, 30% Glass Reinforced, Flame Retardant UL94 V-0/5VA rated, UV-Stabilized
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
ASTM C177
Eastman Tenite Butyrate 485A2R30023 Natural, Trsp Cellulose Acetate Butyrate
Plasticizer 23%. Weight loss on heating = 1.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
ASTM C177
Eastman Tenite Butyrate 485E2R30010 Natural, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
ASTM C177
Eastman Tenite Butyrate 550E2R30010 Natural, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
ASTM C177
Eastman Tenite Butyrate 565A2R30016 Natural, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
ASTM C177
Eastman Tenite Propionate 371A2R30012 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 18%. Weight loss on heating = 1% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pro..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
ASTM C177
Eastman Tenite Propionate 376E4000012 Clear, Trsp Cellulose Acetate Propionate
Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
ASTM C177
Eastman Tenite Propionate 381E4000015 Clear, Trsp Cellulose Acetate Propionate
Plasticizer 15%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
ASTM C177
Eastman Tenite Propionate 383A2R30007 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 7%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
Per ATM E1530-93 on 1.4 g/cc compressed paper; density equivalent to crystallized yarn.
DuPont™ Nomex® 430 1200 Denier Aramid Yarn
A high crystallinity natural filament yarn of NOMEX with higher strength and chemical resistance than staple spun yarns. Type 430 is used where the aesthetics and properties of a filament yarn are ..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
ASTM C177
Daikin POLYFLON MG-1241F PTFE 20% Glass Fiber and 5% Graphite Filled Molding Powder, High Apparent Density, Free Flow
20% glass fiber and 5% graphite filled. High apparent density and free-flowing properties. High wear resistance, low friction, high creep resistance.Applications: Mechanical and chemical service (..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
ASTM C177
Daikin POLYFLON MG-6030 PTFE 15% Carbon Fiber Filled Molding Powder
15% carbon fiber filled. High wear resistance, high load resistance, high bend resistance.Applications: Mechanical service (e.g. bearings, mechanical seals and bearing pads)Information provided by ..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
ASTM C177
Daikin NEOFLON NP-20 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Wire and cable coatings, films,..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
Azoty Tarnow™ TARFLEN SM-2 PTFE
Non Free Flowing suspension powder for standard compression molding and compounding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
Ashley Polymers Ashlene® 528LW Nylon 66
General purpose injection molding grade.Data provided by the manufacturer
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
DIN 52612
BASF Ultramid® KR 4355 G5 25% Glass Filled PA6/6T (Conditioned)
Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
CENTROPLAST CENTROMID 12 Polyamide 12
This extruded material has good impact resistance, low moisture absorption and good chemical resistance. It is used in precision elements, drive parts, cases and housingsInformation provided by CEN..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
ASTM C177
Eastman Tenite Butyrate 465E2R30008 Natural, Trsp Cellulose Acetate Butyrate  (discontinued **)
Plasticizer 8%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..