Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 50.0 µm/m-°C | 27.8 µin/in-°F | |
Premix Thermoplastics PREBOARD E1026 Standard Epoxy Circuit Boards PREBOARD is a thermoplastic based PCB laminate. Low dissipation factor leads to high gain in the antennas. As a non filled laminate PREBOARD is fully homogenous so that consistant properties are ac.. |
|||
CTE, linear | 50.0 µm/m-°C @Temperature 23.0 - 100 °C |
27.8 µin/in-°F @Temperature 73.4 - 212 °F |
|
Quadrant EPP Duratron® PEI U1000 PEI, unfilled, extruded (ISO Data) Duratron U1000 PEI is an amber translucent (non-optical quality) amorphous thermoplastic material, offering high strength and heat resistance. It performs continuously to 170 °C, making it ideal fo.. |
|||
CTE, linear | 50.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
27.8 µin/in-°F @Temperature 73.4 - 140 °F |
|
Omnia Plastica PA6 GF Akulon GF - Dry Polyamide 6 reinforced with the addition of 30% glass fibre and graphite. The glass charge makes the material highly resistant to abrasion, compression and flexing. Akulon GF is particularly suitabl.. |
|||
CTE, linear | 50.0 - 70.0 µm/m-°C @Temperature 20.0 °C |
27.8 - 38.9 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Kolon Kocetal® CL704 Reinforced Grade Acetal Copolymer
(discontinued **) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
CTE, linear | 50.0 - 140 µm/m-°C | 27.8 - 77.8 µin/in-°F | Average value: 71.1 µm/m-°C Grade Count:25 |
Overview of materials for PVC, High Impact This property data is a summary of similar materials in the MatWeb database for the category "PVC, High Impact". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
CTE, linear | 50.0 µm/m-°C | 27.8 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 50-3019 Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts, even at elevated te.. |
|||
CTE, linear | 50.0 µm/m-°C @Temperature 20.0 °C |
27.8 µin/in-°F @Temperature 68.0 °F |
|
Hybrid Plastics POSS® EP 1000 Epoxy Adhesive EP1000 is a POSS® based epoxy adhesive with outstanding oxidative resistance to ozone, plasma, or atomic oxygen environments. The EP1000 POSS® Epoxy is also well-suited for peroxide and steam... |
|||
CTE, linear | 50.0 µm/m-°C | 27.8 µin/in-°F | |
MarkeTech Cesium Iodide:Thallium (CsI:Tl) Scintillator Crystal Cesium Iodide activated by thallium is a scintillation material with high absorption power and can be used as an efficient gamma ray absorber. CsI:Tl is soluble in water, but is not hygroscopic in l.. |
|||
CTE, linear | 50.0 µm/m-°C | 27.8 µin/in-°F | ASTM D696 |
Kolon SPESIN® KP213G15HIBL Impact Resistant PBT Compound resin G/F 15% + Impact resistantApplications: SwitchesInformation provided by API-Kolon. |
|||
CTE, linear | 50.0 µm/m-°C @Temperature 20.0 °C |
27.8 µin/in-°F @Temperature 68.0 °F |
Vertical Direction; ASTM D696 |
Mitsui Arlen™ C230 30% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
CTE, linear | 50.0 µm/m-°C | 27.8 µin/in-°F | ASTM D696 |
Gromax PBT 3015-201 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
CTE, linear | 50.0 - 70.0 µm/m-°C | 27.8 - 38.9 µin/in-°F | ASTM D696 |
Samyang Trirex® 3017PJ Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3017PJ is a super high flow grade.Information provided by Samyang. |
|||
CTE, linear | 50.0 - 70.0 µm/m-°C | 27.8 - 38.9 µin/in-°F | ASTM D696 |
Samyang Trirex® 3020PJ Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020PJ is a high flow grade.Information provided by Samyang. |
|||
CTE, linear | 50.0 - 70.0 µm/m-°C | 27.8 - 38.9 µin/in-°F | ASTM D696 |
Samyang Trirex® 3022R Polycarbonate with Heat Stabilizer PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3022R is a general use grade with heat stabilizers and separating materials added.Appli.. |
|||
CTE, linear | 50.0 - 55.0 µm/m-°C | 27.8 - 30.6 µin/in-°F | |
Master Bond EP21LVMed Two Component, Low Viscosity USP Class VI Epoxy Master Bond EP21LVMed is a two component, low viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulating and casting. It is formulated to cure readily at room tempera.. |
|||
CTE, linear | 50.0 - 90.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
27.8 - 50.0 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
Daikin NEOFLON EA-LR43 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
CTE, linear | 50.0 - 90.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
27.8 - 50.0 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
Daikin NEOFLON RP-5000 EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
CTE, linear | 50.0 - 90.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
27.8 - 50.0 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
Daikin NEOFLON RP-5000AS EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
CTE, linear | 50.0 µm/m-°C @Temperature 20.0 °C |
27.8 µin/in-°F @Temperature 68.0 °F |
ASTM data |
BASF Capron® 8260 HS BK-102 40% Mineral-Filled Nylon 6 (Dry)
(discontinued **) Capron 8260 HS BK-102 is a heat stabilized, pigmented black, 40% mineral reinforced nylon 6 injection molding resin. It possesses high stiffness, dimensional stability and heat resistance combined .. |
|||
CTE, linear | >= 50.0 µm/m-°C | >= 27.8 µin/in-°F | |
Epoxyset Epoxibond EB-177 Unfilled Epoxy Adhesive A two-component, unfilled, high temperature epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by Epoxyset Inc... |
|||
CTE, linear | 50.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
27.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics NORYL PX2907 PPE+PS (Asia Pacific) PPE+HIPS GF10% FR V-1 |
|||
CTE, linear | 50.0 - 70.0 µm/m-°C | 27.8 - 38.9 µin/in-°F | ASTM D696 |
Samyang Trirex® 3020R Polycarbonate with Heat Stabilizer PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020R is a high flow grade with added heat stabilizers and separating materials.Informa.. |
|||
CTE, linear | 50.0 - 70.0 µm/m-°C | 27.8 - 38.9 µin/in-°F | ASTM D696 |
Samyang Trirex® 3026B Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3026B is an extrusion grade.Applications: BottlesInformation provided by Samyang. |
|||
CTE, linear | 50.0 - 100 µm/m-°C | 27.8 - 55.6 µin/in-°F | Average value: 79.7 µm/m-°C Grade Count:13 |
Overview of materials for Polystyrene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a.. |
|||
CTE, linear | 50.0 - 60.0 µm/m-°C | 27.8 - 33.3 µin/in-°F | Average value: 51.8 µm/m-°C Grade Count:11 |
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum .. |