Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 55.0 - 65.0 µm/m-°C | 30.6 - 36.1 µin/in-°F | Polykemi |
Polykemi AB POLYelast TPE HJ752 Thermoplastic Elastomer, PP/Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
CTE, linear | 55.0 - 65.0 µm/m-°C | 30.6 - 36.1 µin/in-°F | Polykemi |
Polykemi AB POLYelast TPE HJ753 Thermoplastic Elastomer, PP/Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
CTE, linear | 9.00 - 65.0 µm/m-°C | 5.00 - 36.1 µin/in-°F | Average value: 44.3 µm/m-°C Grade Count:10 |
Overview of materials for Polyetheretherketone, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
CTE, linear | 55.0 - 65.0 µm/m-°C | 30.6 - 36.1 µin/in-°F | Polykemi |
Polykemi AB POLYfill PP HJ752 Polypropylene/Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
CTE, linear | 55.0 - 65.0 µm/m-°C | 30.6 - 36.1 µin/in-°F | Polykemi |
Polykemi AB POLYfill PP HJ752 UV Polypropylene/Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
CTE, linear | 45.0 - 65.0 µm/m-°C @Temperature 20.0 °C |
25.0 - 36.1 µin/in-°F @Temperature 68.0 °F |
|
Hybrid Plastics NanoBondâ„¢ UV Curable Adhesive Generally used for dental and optical applications.Information provided by Hybrid Plastics |
|||
CTE, linear | 60.0 - 65.0 µm/m-°C | 33.3 - 36.1 µin/in-°F | |
Master Bond EP37-3FLFAN Electrically Isolating, Flexible Epoxy Description: Master Bond Polymer System EP37-3FLFAN is a two component system for high performance potting, bonding, sealing and coating that is formulated to cure at room temperature or more rapidl.. |
|||
CTE, linear | 60.0 - 65.0 µm/m-°C | 33.3 - 36.1 µin/in-°F | |
Master Bond LED401 One Component LED Curable Adhesive System Master Bond LED401 is a highly innovative, one part LED type system that cures fully upon exposure to a 405 nm wavelength light source where the presence of any UV light is minimal or incidental. In.. |
|||
CTE, linear | 60.0 - 65.0 µm/m-°C | 33.3 - 36.1 µin/in-°F | |
Master Bond LED401 White One Part, LED Curable Compound Description: Master Bond LED401 White is a one part LED type system that cures fully upon exposure to a 405 nm wavelength light source where the presence of any UV light is minimal or incidental. In.. |
|||
CTE, linear | 60.0 - 65.0 µm/m-°C | 33.3 - 36.1 µin/in-°F | |
Master Bond LED403Med USP Class VI, One Component, LED Curable System Master Bond LED403Med is a one part LED system that cures fully upon exposure to a 405 nm wavelength light that is generated by an LED source and. In fact, this material will fully cure tack-free wi.. |
|||
CTE, linear | 55.0 - 65.0 µm/m-°C | 30.6 - 36.1 µin/in-°F | |
Master Bond UV15DC80 One Component, UV and Heat Curable Epoxy System Master Bond UV15DC80 is a special dual cure epoxy based system which offers a primary cure utilizing UV light along with a secondary heat curing mechanism. This system addresses the problem of curin.. |
|||
CTE, linear | 60.0 - 65.0 µm/m-°C @Temperature 20.0 °C |
33.3 - 36.1 µin/in-°F @Temperature 68.0 °F |
|
Abatron AboCast/AboCure 8109-1 High melting point.Processing: 100/30 pbw; mix at 130-140°C (270 °F); cures in 16 h/120°C (250°F), 10 h/140°C (285°F), 8 h/160°C (320°F), 2 h/ 200°C (390°F).Applications: Heavy duty castin.. |
|||
CTE, linear | 55.0 - 65.0 µm/m-°C @Temperature 20.0 °C |
30.6 - 36.1 µin/in-°F @Temperature 68.0 °F |
|
Abatron AboCast/AboCure 8109-5 High heat resistance. Easy to use.Processing: 100/20 pbw; Potlife: 7-10 days/20°C (68°F), 5-7h/60°C (140°F); mix at RT; cures in: 4 h/100°C (212°F) + 3 h/190°C (375°F) postcure.Applications.. |
|||
CTE, linear | 55.0 - 65.0 µm/m-°C @Temperature 20.0 °C |
30.6 - 36.1 µin/in-°F @Temperature 68.0 °F |
|
Abatron AboCast/AboCure 8109-6 High heat resistance. Easy to use.Processing: 100/90 pbw; Potlife: 15-20 days/20°C (68°F), 7-10 h/120°C (250°F); mix at RT; cures in: 3 h/100°C (212°F) + 3 h/190°C (375°F) postcure.Applicat.. |
|||
CTE, linear | 60.0 - 65.0 µm/m-°C | 33.3 - 36.1 µin/in-°F | |
Abatron AboCast/AboCure 8502-1 Epoxy AboCast/AboCure 8502-1 is a solventless clear Epoxy System, used as a casting, adhesive, and impregnating resin for transformers, capacitors, coils, and other electronic components requiring a low-v.. |
|||
CTE, linear | 55.0 - 65.0 µm/m-°C | 30.6 - 36.1 µin/in-°F | Polykemi |
Polykemi AB POLYfill PP HJ752 UV2 Polypropylene/Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
CTE, linear | 55.0 - 65.0 µm/m-°C | 30.6 - 36.1 µin/in-°F | Polykemi |
Polykemi AB POLYfill PPH BF405510 VT1 Polypropylene Homopolymer, Reinforced, Heat Resistant Information provided by Polykemi AB |
|||
CTE, linear | 55.0 - 65.0 µm/m-°C @Temperature 20.0 °C |
30.6 - 36.1 µin/in-°F @Temperature 68.0 °F |
|
Abatron AboCast/AboCure 8109-7 Processing: 100/80 pbw; Potlife: 6-7 days/20°C (68°F), 12-24 h/40°C (105°F), 0.75-7 h /60°C (140°F); mix at 50-80°C (120-175°F); cures in: 1 h/100°C (212°F) + 4 h/150°C (300°F) postcure... |