Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 57.0 - 170 µm/m-°C @Temperature 30.0 - 300 °C |
31.7 - 94.4 µin/in-°F @Temperature 86.0 - 572 °F |
Average value: 95.7 µm/m-°C Grade Count:9 |
Overview of materials for Polytetrafluoroethylene (PTFE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v.. |
|||
CTE, linear | 50.0 - 170 µm/m-°C | 27.8 - 94.4 µin/in-°F | Average value: 102 µm/m-°C Grade Count:13 |
Overview of materials for Nylon 612, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp.. |
|||
CTE, linear | 110 - 170 µm/m-°C @Temperature 20.0 °C |
61.1 - 94.4 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite 105E3V36327 Acetate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
CTE, linear | 110 - 170 µm/m-°C | 61.1 - 94.4 µin/in-°F | ASTM D696 |
Eastman Tenite 285E0V16304 Cellulose Acetate Butyrate, Clear, Trsp Applications:DisplaysProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T.. |
|||
CTE, linear | 110 - 170 µm/m-°C @Temperature 20.0 °C |
61.1 - 94.4 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite 307A4000015 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
CTE, linear | 110 - 170 µm/m-°C @Temperature 20.0 °C |
61.1 - 94.4 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite 307A4000018 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
CTE, linear | 110 - 170 µm/m-°C @Temperature 20.0 °C |
61.1 - 94.4 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite 307E0V16310 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
CTE, linear | 110 - 170 µm/m-°C @Temperature 20.0 °C |
61.1 - 94.4 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite 307E4000018 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
CTE, linear | 110 - 170 µm/m-°C | 61.1 - 94.4 µin/in-°F | ASTM D696 |
Eastman Tenite 350A4861313 Cellulose Acetate Propionate, Clear, Trsp Applications:Blood TherapyDrug DeliveryIV ComponentsMedical DevicesSurgical InstrumentsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughne.. |
|||
CTE, linear | 110 - 170 µm/m-°C @Temperature 20.0 °C |
61.1 - 94.4 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite 360A4000012 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
CTE, linear | 110 - 170 µm/m-°C | 61.1 - 94.4 µin/in-°F | ASTM D696 |
Eastman Tenite 360A4861307 Cellulose Acetate Propionate, Clear, Trsp Applications:Blood TherapyDrug DeliveryIV ComponentsMedical DevicesSurgical InstrumentsKey Attributes:Chemical resistance to most medical solvents including lipids and IPAEase of processingGamma and.. |
|||
CTE, linear | 110 - 170 µm/m-°C @Temperature 20.0 °C |
61.1 - 94.4 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite 360A4861316 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
CTE, linear | 110 - 170 µm/m-°C | 61.1 - 94.4 µin/in-°F | ASTM D696 |
Eastman Tenite 360E0096914 Cellulose Acetate Propionate, Natural, Trsp Applications:ProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T.. |
|||
CTE, linear | 110 - 170 µm/m-°C | 61.1 - 94.4 µin/in-°F | ASTM D696 |
Eastman Tenite 360E2R30016 Cellulose Acetate Propionate, Natural, Trsp Applications:AppliancesPersonal Care and CosmeticsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss.. |
|||
CTE, linear | 110 - 170 µm/m-°C @Temperature 20.0 °C |
61.1 - 94.4 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite 360E3V45512 Propionate Water Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
CTE, linear | 110 - 170 µm/m-°C @Temperature 20.0 °C |
61.1 - 94.4 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite 360E3V45516 Propionate Water Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
CTE, linear | 110 - 170 µm/m-°C | 61.1 - 94.4 µin/in-°F | ASTM D696 |
Eastman Tenite 371A2R30008 Cellulose Acetate Propionate, Natural, Trsp Applications:Consumer-Personal CareToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, c.. |
|||
CTE, linear | 110 - 170 µm/m-°C | 61.1 - 94.4 µin/in-°F | ASTM D696 |
Eastman Tenite 371A4000012 Cellulose Acetate Propionate, Clear, Trsp Applications:OphthalmicsOral HygienePen/stationary suppliesToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, st.. |
|||
CTE, linear | 110 - 170 µm/m-°C | 61.1 - 94.4 µin/in-°F | ASTM D696 |
Eastman Tenite 380A4000015 Cellulose Acetate Propionate, Clear, Trsp Applications:OphthalmicsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel.. |
|||
CTE, linear | 110 - 170 µm/m-°C | 61.1 - 94.4 µin/in-°F | ASTM D696 |
Eastman Tenite 383A4000011 Cellulose Acetate Propionate, Clear, Trsp Applications:AppliancesFloor carePersonal care and cosmeticsProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, stren.. |
|||
CTE, linear | 110 - 170 µm/m-°C | 61.1 - 94.4 µin/in-°F | ASTM D696 |
Eastman Tenite 485E3720008 Cellulose Acetate Butyrate, Clear, Trsp Applications:Toys/Sporting goodsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties including toughness, hardness, strength, surface gloss, clarity,.. |
|||
CTE, linear | 110 - 170 µm/m-°C @Temperature 20.0 °C |
61.1 - 94.4 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite 485E3720023 Butyrate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
CTE, linear | 110 - 170 µm/m-°C | 61.1 - 94.4 µin/in-°F | ASTM D696 |
Eastman Tenite 550E3V45510 Cellulose Acetate Butyrate, Water Clear, Trsp Applications:AppliancesConsumer-Personal careProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gl.. |
|||
CTE, linear | 19.8 - 170 µm/m-°C | 11.0 - 94.4 µin/in-°F | Average value: 88.1 µm/m-°C Grade Count:36 |
Overview of materials for Nylon 6, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
CTE, linear | 60.0 - 170 µm/m-°C | 33.3 - 94.4 µin/in-°F | Average value: 104 µm/m-°C Grade Count:3 |
Overview of materials for Nylon, Flexible Alloy This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Flexible Alloy". Each property range of values reported is minimum and maximum values of appropri.. |
|||
CTE, linear | 11.0 - 170 µm/m-°C | 6.11 - 94.4 µin/in-°F | Average value: 83.8 µm/m-°C Grade Count:53 |
Overview of materials for Cellulose Acetate Propionate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Propionate, Molded". Each property range of values reported is minimum and maximum val.. |
|||
CTE, linear | 11.0 - 170 µm/m-°C | 6.11 - 94.4 µin/in-°F | Average value: 76.9 µm/m-°C Grade Count:12 |
Overview of materials for Cellulose Acetate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr.. |
|||
CTE, linear | 11.0 - 170 µm/m-°C | 6.11 - 94.4 µin/in-°F | Average value: 44.8 µm/m-°C Grade Count:36 |
Overview of materials for Cellulose Acetate Butyrate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Butyrate, Molded". Each property range of values reported is minimum and maximum value.. |
|||
CTE, linear | 110 - 170 µm/m-°C @Temperature 20.0 °C |
61.1 - 94.4 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite 550E3V45510 Butyrate Water Clear, Trsp
(discontinued **) Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
CTE, linear | 110 - 170 µm/m-°C @Temperature 20.0 °C |
61.1 - 94.4 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite 360A4861301 Propionate Clear, Trsp
(discontinued **) Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |