Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 65.0 µm/m-°C @Temperature 20.0 °C |
36.1 µin/in-°F @Temperature 68.0 °F |
DIN 53328 |
Polycasa PC QUINN PC sheets have excellent optical properties and a brilliant surface. The QUINN PC range contains sheets that are easy to fabricate and show exceptional performance at both low and high tempera.. |
|||
CTE, linear | 65.0 µm/m-°C | 36.1 µin/in-°F | Polykemi |
Polykemi AB POLYelast TPE HJ-75 UV Thermoplastic Elastomer, PP/Elastomer/Mineral, UV-Stabilized, Low CLTE Information provided by Polykemi AB |
|||
CTE, linear | 65.0 µm/m-°C | 36.1 µin/in-°F | |
Resinlab® CYNERGY CA6401 Adhesive Description: The CYNERGY 6400 SERIES are clear, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa.. |
|||
CTE, linear | 65.0 µm/m-°C | 36.1 µin/in-°F | |
Resinlab® CYNERGY CA6403 Adhesive Description: The CYNERGY 6400 SERIES are clear, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa.. |
|||
CTE, linear | 65.0 µm/m-°C | 36.1 µin/in-°F | |
Resinlab® CYNERGY CA6404 Adhesive Description: The CYNERGY 6400 SERIES are clear, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa.. |
|||
CTE, linear | 65.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
36.1 µin/in-°F @Temperature -22.0 - 176 °F |
ASTM E228 |
Solvay Engineered Polymers SEQUEL® 1485 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 1485 engineered polyolefin material is designed for large automotive exterior applications that require ductile impact properties at low temperatures, improved scratch and mar .. |
|||
CTE, linear | 65.0 - 80.0 µm/m-°C | 36.1 - 44.4 µin/in-°F | Average value: 73.8 µm/m-°C Grade Count:29 |
Overview of materials for Polyphenylene Ether, Heat Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Heat Resistant". Each property range of values reported is minimum and maximum valu.. |
|||
CTE, linear | 65.0 µm/m-°C @Temperature 23.0 - 100 °C |
36.1 µin/in-°F @Temperature 73.4 - 212 °F |
|
Quadrant EPP Quadrant PC 1000 extruded (ISO Data) Quadrant Engineering Plastic Products is marketing non-UV-stabilized polycarbonate stock shapes under the trade name Quadrant PC 1000. It is a natural, “non-optical” industrial quality (clear, tra.. |
|||
CTE, linear | 65.0 - 70.0 µm/m-°C | 36.1 - 38.9 µin/in-°F | Average value: 69.5 µm/m-°C Grade Count:29 |
Overview of materials for Polycarbonate, High Heat This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, High Heat". Each property range of values reported is minimum and maximum values of appro.. |
|||
CTE, linear | 65.0 - 180 µm/m-°C | 36.1 - 100 µin/in-°F | Average value: 103 µm/m-°C Grade Count:13 |
Overview of materials for Polytetrafluoroethylene (PTFE), Bronze Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Bronze Filled". Each property range of values reported is minimum and ma.. |
|||
CTE, linear | 65.0 µm/m-°C | 36.1 µin/in-°F | DIN 52328 |
Isoflon PC Polycarbonate Good impact resistance among transparent materialsInformation provided by Isoflon. |
|||
CTE, linear | 65.0 - 100 µm/m-°C | 36.1 - 55.6 µin/in-°F | ASTM D696 |
Guarniflon PTFE G455 Polytetrafluoroethylene 35% Carbographite PTFE G Special Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high w.. |
|||
CTE, linear | 65.0 µm/m-°C @Temperature 23.0 - 85.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 185 °F |
ASTM E831 |
Solvay Technyl® B 50H1 Nylon 66/6, Flame Retardant, EH0 Flame retardant copolyamide 66/6, unreinforced, heat stabilized, for injection molding.This phosphorus and halogen free flame retardant grade, UL 94 VO (0.4 mm), offers excellent filling qualities a.. |
|||
CTE, linear | 65.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
36.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics NORYL EXT130 PPE+HIPS (Asia Pacific) PPE+PS for auto exterior, High heat |
|||
CTE, linear | 65.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
36.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics NORYL PX2637 PPE+HIPS (Asia Pacific) |
|||
CTE, linear | 65.0 µm/m-°C | 36.1 µin/in-°F | |
Master Bond EP21LV35Med Two Component, Flexible USP Class VI Epoxy System Master Bond Polymer System EP21LV3/5Med is a two part, low viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulation and casting that cures flexible. It cures readil.. |
|||
CTE, linear | 65.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
36.1 µin/in-°F @Temperature -22.0 - 176 °F |
Borealis Method |
Borealis Daplen™ EF005AE Polypropylene TPO Compound Daplen™ EF005AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, give.. |
|||
CTE, linear | 65.0 µm/m-°C @Temperature 40.0 - 130 °C |
36.1 µin/in-°F @Temperature 104 - 266 °F |
TMA; ASTM E831 |
Plenco 4548 Phenolic, Granular, Transfer Molded PLENCO 04548 is a heat resistant mineral filled phenolic molding compound, offering fast cure rates and hot rigidity. Type ASTM 5948 CFG, and UL recognized under component file E40654. 04548 is avai.. |
|||
CTE, linear | 65.0 µm/m-°C @Temperature 20.0 °C |
36.1 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
A. Schulman POLYTROPE™ TPP 518 Injection Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 518 is an injection grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal expansion i.. |
|||
CTE, linear | 65.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 53752 |
CP-Polymer-Technik Wellamid® 6600 GS 20 HWCP 20% Glass Sphere Filled Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
CTE, linear | 65.0 µm/m-°C @Temperature 20.0 °C |
36.1 µin/in-°F @Temperature 68.0 °F |
ASTM E 831 |
Azoty Tarnow™ TARFLEN SM-S15 PTFE 15% glass fiber reinforced for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
CTE, linear | 65.0 µm/m-°C @Temperature 20.0 °C |
36.1 µin/in-°F @Temperature 68.0 °F |
ASTM E 831 |
Azoty Tarnow™ TARFLEN SM-S15G2 PTFE Tarflen SM1 reinforced with 15% glass fibers and 2% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
CTE, linear | 65.0 µm/m-°C @Temperature 20.0 °C |
36.1 µin/in-°F @Temperature 68.0 °F |
ASTM E 831 |
Azoty Tarnow™ TARFLEN SM-S25 PTFE Tarflen SM1 reinforced with 25% glass fiber for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
CTE, linear | 65.0 µm/m-°C @Temperature 20.0 °C |
36.1 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
CENTROPLAST CENTROLYTE ZX Polyethylene terephthalate with lubricant This material's solid lubricant additive has good sliding properties, and is well suited for high load, dry running situations. Possible uses include precision plain bearings, plug connectors, r.. |
|||
CTE, linear | 65.0 µm/m-°C @Temperature -30.0 - 60.0 °C |
36.1 µin/in-°F @Temperature -22.0 - 140 °F |
ASTM D696 |
Asahi Kasei Xyron® X9108 Modified Polyphenylene Ether High-Heat ResistantInformation provided by Asahi Kasei |
|||
CTE, linear | 65.0 µm/m-°C @Temperature 20.0 °C |
36.1 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
A. Schulman POLYTROPE™ TPP 518 Injection Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 518 is an injection grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal expansion i.. |
|||
CTE, linear | 65.0 µm/m-°C @Temperature 20.0 °C |
36.1 µin/in-°F @Temperature 68.0 °F |
ASTM E 831 |
Azoty Tarnow™ TARFLEN SM-B60 PTFE Tarflen SM1 reinforced with 60% bronze for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
CTE, linear | 65.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
36.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics NORYL 115 PPE+HIPS (Asia Pacific) PPE+PS, 115 oC HDT |
|||
CTE, linear | 65.0 µm/m-°C @Temperature 20.0 °C |
36.1 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
CENTROPLAST CENTROCARB Polycarbonate CENTROCARB is a transparent or semi-transparent plastic with high strength and impact resistance. It is dimensionally rigid and has very good electrical insulating properties. It is used in contain.. |