Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 200 µm/m-°C | 111 µin/in-°F | DIN 53752 |
Polikim ULPOLEN® 500 UHMWPE Standard Standard Ulpolen® 1000 is the universal type primarily preferred on the condition that its technical properties meet operating environment requirements. It is more cost efficient compared to specia.. |
|||
CTE, linear | 200 µm/m-°C | 111 µin/in-°F | DIN 53752 |
Okulen® 1000 - REG PE Multicoloured coarse OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
CTE, linear | 200 µm/m-°C | 111 µin/in-°F | DIN 53752 |
Okulen® 1000 PE-UHMW, Black OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
CTE, linear | 200 µm/m-°C | 111 µin/in-°F | DIN 53752 |
Okulen® 1000 PE-UHMW, Colored OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
CTE, linear | 200 µm/m-°C | 111 µin/in-°F | DIN 53752 |
Okulen® 1000 PE-UHMW, Conductive OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
CTE, linear | 200 µm/m-°C | 111 µin/in-°F | DIN 53752 |
Okulen® 1000 PE-UHMW, Natural OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
CTE, linear | 200 µm/m-°C | 111 µin/in-°F | DIN 53752 |
Okulen® 1000 PE-UHMW, UV - stabilized OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
CTE, linear | 200 µm/m-°C | 111 µin/in-°F | DIN 53752 |
Okulen® 2000 PE-UHMW, 588 Blue OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
CTE, linear | 200 µm/m-°C @Temperature 23.0 - 100 °C |
111 µin/in-°F @Temperature 73.4 - 212 °F |
|
Quadrant EPP TIVAR® 1000 ASTL PE-UHMW + specific additives (ISO Data) TIVAR 1000 ASTL, based on a PE-UHMW grade with extremely high molecular weight, has been specifically developed for tough anti-abrasion applications. TIVAR 1000 ASTL shows a higher wear and abrasion.. |
|||
CTE, linear | 200 µm/m-°C @Temperature 23.0 - 100 °C |
111 µin/in-°F @Temperature 73.4 - 212 °F |
|
Quadrant EPP TIVAR® DS PE-UHMW + additives (ISO Data) TIVAR DS is a modified PE-UHMW with extremely high molecular weight. The latter in combination with a particular manufacturing process result in a PE-UHMW grade with superior wear and abrasion resis.. |
|||
CTE, linear | 200 µm/m-°C @Temperature 23.0 - 100 °C |
111 µin/in-°F @Temperature 73.4 - 212 °F |
|
Quadrant EPP TIVAR® Oil Filled PE-UHMW + oil (ISO Data) TIVAR Oil Filled is a self-lubricating PE-UHMW material in the real meaning of the word. Next to an enhanced wear resistance, the incorporated and evenly dispersed oil renders this material a consid.. |
|||
CTE, linear | 200 µm/m-°C @Temperature 20.0 °C |
111 µin/in-°F @Temperature 68.0 °F |
ISO 11359-2 |
Polymer Industries Polyslick UHMW Rod Polyslick UHMW Rod exhibits all of the durable qualities of our Polyslick UHMW Sheet making it perfect for the application where sheet stock is not suitable. The material is ideally suited for the m.. |
|||
CTE, linear | 200 µm/m-°C @Temperature 20.0 °C |
111 µin/in-°F @Temperature 68.0 °F |
|
3M Dyneon™ Fluorel™ FC-2123 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Excellent hot tear and compression se.. |
|||
CTE, linear | 200 µm/m-°C @Temperature 20.0 °C |
111 µin/in-°F @Temperature 68.0 °F |
|
3M Dyneon™ Fluorel™ FC-2144 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Higher viscosity version of FC-2123. .. |
|||
CTE, linear | 200 µm/m-°C @Temperature 20.0 °C |
111 µin/in-°F @Temperature 68.0 °F |
|
3M Dyneon™ Fluorel™ FC-2177 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Slower cure rate and high tear streng.. |
|||
CTE, linear | 200 µm/m-°C @Temperature 20.0 °C |
111 µin/in-°F @Temperature 68.0 °F |
ISO 11359-2 |
Polymer Industries Polyslick UHMW Profile Polyslick UHMW Profiles exhibit all of the durable qualities of our Polyslick UHMW Sheet making them perfect for use where sheet stock is not suitable. Polymer Industries offers a large variety of p.. |
|||
CTE, linear | 200 µm/m-°C @Temperature 20.0 °C |
111 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
LyondellBasell Petrothene® PR92735 Linear Low Density Polyethylene ApplicationsPETROTHENE PR 92735 is a high molecular weight, linear low density-based compound designed for cable jacketing. PR 92735 contains a nominal carbon black content of 2.6% and antioxidant .. |
|||
CTE, linear | 200 µm/m-°C @Temperature 20.0 °C |
111 µin/in-°F @Temperature 68.0 °F |
DIN 53752 |
GEHR Plastics PE-UHMW Polyethylene, Ultra High Molecular Weight The ultra high molecular weight Polyethylene has a high abrasion resistance and a high toughness at the same time. The chemical and the crack resistance are optimized in comparison to the standard P.. |
|||
CTE, linear | 200 µm/m-°C | 111 µin/in-°F | DIN 52328 |
Isoflon PEHD 500 High Density Polyethylene Products with excellent friction, anti-stick, abrasion and chemical inertia characteristicsVery good impact resistanceNo moisture regainProduct for the food industryInformation provided by Isoflon. |
|||
CTE, linear | 200 µm/m-°C @Temperature 20.0 °C |
111 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials RTV60 Silicone Rubber Compound for High Temperature, Red RTV31, RTV60 and RTV88 silicone rubber compounds are high temperature two-part silicone elastomers. They are supplied ready-to-use with a base compound and DEBT (deputy tin deflagrate) as the standa.. |
|||
CTE, linear | 200 µm/m-°C | 111 µin/in-°F | Above Tg |
Tra-Con Tra-Bond 293-14 Electrically Conductive Silver-Filled Epoxy Adhesive TRA-BOND 293-14 silver-filled, electrically conductive epoxy adhesive is designed to provide strong bonds to difficult-to-bond metals, such as nickel, copper, gold and solder. The stress-absorbing c.. |
|||
CTE, linear | 200 µm/m-°C @Temperature 20.0 °C |
111 µin/in-°F @Temperature 68.0 °F |
|
Trelleborg Emerson & Cuming Stycast® 5952 Two-Component Easy Mix Ratio Encapsulant Features and Typical ApplicationsPrimarily designed for ease of use in either meter mix or manual dispense operations. These products also offer a wide range of features including heat dissipation, .. |
|||
CTE, linear | 200 µm/m-°C | 111 µin/in-°F | Above Tg |
Epoxy Technology EPO-TEK® 337H Graphite-Filled, High Temperature Epoxy Product Description: EPO-TEK® 377H is a two component, high Tg, graphite filled epoxy designed for ESD/EMI shielding of semiconductor devices and electronics. It can be used in many electronic ind.. |
|||
CTE, linear | 200 µm/m-°C | 111 µin/in-°F | |
Hippe PTFE Good chemical resistance. High thermal stability. Flame resistance. Lowest coefficient of friction among all solid plastics. Very good dielectric properties. Very high weathering resistance.Info.. |
|||
CTE, linear | 200 µm/m-°C @Temperature 20.0 °C |
111 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
CENTROPLAST CENTROLEN PE-HD Polyethylene high density This material is a low density, easily machined plastic that can be welded and has good chemical resistance. Applications include apparatus engineering, and machines in the foodstuff industry.Infor.. |
|||
CTE, linear | 200 µm/m-°C | 111 µin/in-°F | DIN 53752 |
Okulen® 500 PE-HMW, Natural OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
CTE, linear | 200 µm/m-°C | 111 µin/in-°F | |
Resinlab® UR3010 Clear Polyurethane Potting System Resinlab™ UR 3010 Clear is a, two component, room temperature curing polyurethane potting system. It is designed to cure completely at room temperature. UR 3010 provides excellent environmental pro.. |
|||
CTE, linear | 200 µm/m-°C @Temperature 20.0 °C |
111 µin/in-°F @Temperature 68.0 °F |
|
3M Dyneon™ Fluorel™ FC-2211 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp.. |
|||
CTE, linear | 200 µm/m-°C @Temperature -40.0 - 140 °C |
111 µin/in-°F @Temperature -40.0 - 284 °F |
ASTM D696 |
Arkema Group Pebax® MX 1205 Polyether Block Amide (PEBA) Typical application: Impact modifierInformation provided by Arkema Group |