Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 18.0 µm/m-°C @Temperature 100 °C |
10.0 µin/in-°F @Temperature 212 °F |
ASTM E-831 (TMA) |
Technetics Group Amicon™ PEEK 30% Carbon
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
CTE, linear | 18.0 µm/m-°C | 10.0 µin/in-°F | MD, below Tg; ASTM D696 |
Victrex® APTIV® 1103-050 Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, Mineral Filled
(Unve Description: APTIV® 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance a.. |
|||
CTE, linear | 18.0 - 40.0 µm/m-°C | 10.0 - 22.2 µin/in-°F | Average value: 28.8 µm/m-°C Grade Count:9 |
Overview of materials for Polycarbonate, Carbon + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + PTFE Filled". Each property range of values reported is minimum and maximum valu.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 °C |
10.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Solvay Specialty Polymers Ixef® 1501/0003 Polyarylamide, 30% Glass Fiber, DAM
(discontinued **) The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
CTE, linear | 18.0 - 140 µm/m-°C | 10.0 - 77.8 µin/in-°F | Average value: 63.7 µm/m-°C Grade Count:163 |
Overview of materials for PVC, Rigid Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
CTE, linear | 18.0 - 39.0 µm/m-°C @Temperature 100 - 200 °C |
10.0 - 21.7 µin/in-°F @Temperature 212 - 392 °F |
Average value: 28.5 µm/m-°C Grade Count:4 |
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced". Each property range of values repor.. |
|||
CTE, linear | 18.0 µm/m-°C | 10.0 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1-RG 1 Polyamide 66, with PAN-carbon fiber, RG-standard Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 - 200 °C |
10.0 µin/in-°F @Temperature 68.0 - 392 °F |
|
Materion Beryllium Copper Alloy 10 Plate & Rolled Bar; H (TD04) Temper; up to 76 mm Thickness (UNS C17500) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 - 200 °C |
10.0 µin/in-°F @Temperature 68.0 - 392 °F |
|
Materion Beryllium Copper Alloy 10 Plate & Rolled Bar; HT (TH04) Temper; up to 76 mm Thickness (UNS C17500) Treatment required for max strength: 2 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 - 200 °C |
10.0 µin/in-°F @Temperature 68.0 - 392 °F |
|
Materion Brush 1915â„¢ Hard Temper Wire, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 - 200 °C |
10.0 µin/in-°F @Temperature 68.0 - 392 °F |
|
Materion Brush 60™ HT Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation afte.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 21.1 - 204 °C |
10.0 µin/in-°F @Temperature 70.0 - 400 °F |
|
Materion BrushCAST® 165CT Fine Grain Casting Alloy (As Cast) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 21.1 - 204 °C |
10.0 µin/in-°F @Temperature 70.0 - 400 °F |
|
Materion BrushCAST® 275CT Fine Grain Casting Alloy (As Cast & Aged) Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 °C |
10.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Techmer ES Electrafil® J-50/CF/30 Polycarbonate, 30% Carbon Fiber Reinforced Carbon Fiber Reinforced |
|||
CTE, linear | 18.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
10.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM E831 |
A. Schulman POLYPUR™ FPU 1156 Thermoplastic Polyurethane Information provided by A. Schulman. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 °C |
10.0 µin/in-°F @Temperature 68.0 °F |
|
Williams Advanced Alloys WS226 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 - 300 °C |
10.0 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 210 Gilding Metal, Annealed CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 - 300 °C |
10.0 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 210 Gilding Metal, Spring CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 - 300 °C |
10.0 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 70265 XP175, Hard Information provided by Eagle Brass Company |
|||
CTE, linear | 18.0 µm/m-°C | 10.0 µin/in-°F | |
CLAL-MSX NICLAL 48 Copper Alloy Description: Niclal 48 is a precision resistance alloy, with moderate Resistivity, low Temperature coefficient of resistance and low thermal EMF versus Copper. With high stability of electrical resi.. |
|||
CTE, linear | 18.0 µm/m-°C | 10.0 µin/in-°F | y, before Tg; IPC TM-650 2.4.24 |
Arlon 25FR Low-Cost Ceramic Hydrocarbon High Frequency, Low Loss Thermoset Laminate and Prepreg for Double-sided, Multilayer and Mixed Dielectric Printed Circuit BoardsLow loss ceramic-filled thermoset resinTight dielectric tolerance cont.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 °C |
10.0 µin/in-°F @Temperature 68.0 °F |
|
Armstrong X-6/E Epoxy Adhesive Thixotropic.Information provided by Ellsworth Adhesives. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 - 200 °C |
10.0 µin/in-°F @Temperature 68.0 - 392 °F |
|
Materion Beryllium Copper Alloy 3 Wire; AT (TF00) Temper; 1.3-12.7 mm Diameter (UNS C17510) Treatment required for max strength: 3 hrs @ 480-495°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials .. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 - 200 °C |
10.0 µin/in-°F @Temperature 68.0 - 392 °F |
|
Materion Beryllium Copper Alloy 3 Wire; HT (TH04) Temper; 1.3-12.7 mm Diameter (UNS C17510) Treatment required for max strength: 2 hrs @ 480-495°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials .. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
10.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM E831 |
A. Schulman POLYPUR™ FPU 1156 Thermoplastic Polyurethane Information provided by A. Schulman. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 - 200 °C |
10.0 µin/in-°F @Temperature 68.0 - 392 °F |
|
Materion Beryllium Copper Alloy 3 Strip; HT (TH04) Temper (UNS C17510) Treatment required for max strength: 2-3 hrs @ 480ºC or Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation after 1000 hrs @ 200°C: 75%Formability Ratio.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 - 200 °C |
10.0 µin/in-°F @Temperature 68.0 - 392 °F |
|
Materion Beryllium Copper Alloy 3 Tube; AT (TF00) Temper; All Sizes (UNS C17510) Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc... |