Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 100 µm/m-°C | 55.6 µin/in-°F | ASTM D-696 |
Plaskolite West Optix® CA - 927 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
CTE, linear | 100 µm/m-°C @Temperature 20.0 °C |
55.6 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Rochling Engineered Plastics Polystone® XL Cross linked (UHMW-PE) Polystone® M is a highly versatile polymer that features: Low coefficient of friction Excellent abrasion resistance High-impact strength Chemical resistance Complies with FDA regulations under the .. |
|||
CTE, linear | 100 - 130 µm/m-°C | 55.6 - 72.2 µin/in-°F | Average value: 120 µm/m-°C Grade Count:28 |
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m.. |
|||
CTE, linear | 100 µm/m-°C @Temperature 20.0 °C |
55.6 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Asahi Kasei Tenac® LT805 Acetal Homopolymer, Low Friction Grade
(discontinued **) Excellent friction and wear on metals.Applications: Keyboard parts, bearings for office machines, gears.This product is not a part of the standard product line dated 2003. |
|||
CTE, linear | 100 µm/m-°C @Temperature 20.0 °C |
55.6 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Asahi Kasei Tenac®-C 4510 Acetal Copolymer, General Purpose
(discontinued **) General-purpose grade, characterized by balanced flowability and mechanical properties.Applications: Gears, cams, hose joints, clips, switches, mechanical parts of audio and video equipment.This pro.. |
|||
CTE, linear | 100 µm/m-°C @Temperature 20.0 °C |
55.6 µin/in-°F @Temperature 68.0 °F |
TMA; ASTM E831 |
LNP Stat-Kon® PDX-S-90398 Polyamide 12, Stainless Steel Fiber
(discontinued **) Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |
|||
CTE, linear | 100 µm/m-°C @Temperature 23.0 - 55.0 °C |
55.6 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2; Parallel to Flow |
Ineos ABS Lustran® M210TF ABS Pellets Lustran® ABS M210TF is used in general applications for toy and food contact. It meets European standard EN 71, part 3 and ASTM F 963. It has standard impact strength, high gloss, and is easy flo.. |
|||
CTE, linear | 100 µm/m-°C | 55.6 µin/in-°F | ASTM E831 |
Lucite International Diakon® CRG800 Acrylic Polymer, Toughened Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
CTE, linear | 100 µm/m-°C | 55.6 µin/in-°F | ASTM E831 |
Lucite International Diakon® ST25H8 Toughened Acrylic Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by.. |
|||
CTE, linear | 100 µm/m-°C | 55.6 µin/in-°F | ISO 11359 |
Styrolution PS 2710 HIPS Styrolution PS 2710 is a high impact grade of polystyrene with improved stress crack resistance, developed for extrusion and thermoforming applications, especially for the refrigerator industry.Impr.. |
|||
CTE, linear | 100 µm/m-°C @Temperature -30.0 - 80.0 °C |
55.6 µin/in-°F @Temperature -22.0 - 176 °F |
Borealis Method |
Borealis EE002AE Polypropylene Elastomer Modified EE002AE is a reactor elastomer modified polypropylene compound intended for injection molding. The product is available in natural color. This material has excellent balanced mechanical properties.. |
|||
CTE, linear | 100 µm/m-°C @Temperature 20.0 °C |
55.6 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Total PPH 3281 Polypropylene, Extrusion Grade Low melt flow homopolymer for sheet extrusion, strapping, and in-line thermoforming applicationsMelt Strength – The high melt strength of FINA 3281 allows uniform drawdown during processing, result.. |
|||
CTE, linear | 100 µm/m-°C | 55.6 µin/in-°F | Above Tg |
Tra-Con Tra-Bond 77-1S One Component SMD Adhesive TRA-BOND 77-1S one component, solvent-free, insulating epoxy adhesive is designed specifically for attaching surface mounted devices (SMDs) to printed circuit boards prior to wave solder. TRA-BOND 7.. |
|||
CTE, linear | 100 µm/m-°C | 55.6 µin/in-°F | Above Tg |
Tra-Con Tra-Bond 933-1 Moisture Resistant Chip Encapsulant TRA-BOND 933-1 one component, highly filled, electrically insulating epoxy encapsulant is designed for encapsulating microelectronic chips. This epoxy provides excellent environmental and mechanical.. |
|||
CTE, linear | 100 µm/m-°C | 55.6 µin/in-°F | ISO 11359-2 |
Unitika ET2025 PA6, Conditioned High-impact nylonInformation provided by Unitika Ltd. |
|||
CTE, linear | 100 µm/m-°C @Temperature 23.0 - 60.0 °C |
55.6 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
Daikin POLYFLON MG-1040F PTFE 20% Glass Fiber Filled Molding Powder, High Apparent Density, Free Flow 20% glass fiber filled. High apparent density and free-flowing properties. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Availabl.. |
|||
CTE, linear | 100 µm/m-°C @Temperature 23.0 - 60.0 °C |
55.6 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
Daikin POLYFLON MG-6030 PTFE 15% Carbon Fiber Filled Molding Powder 15% carbon fiber filled. High wear resistance, high load resistance, high bend resistance.Applications: Mechanical service (e.g. bearings, mechanical seals and bearing pads)Information provided by .. |
|||
CTE, linear | 100 µm/m-°C @Temperature 23.0 - 60.0 °C |
55.6 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
Daikin POLYFLON MG-6030F PTFE 15% Carbon Fiber Filled Molding Powder, High Apparent Density, Free Flow 15% carbon fiber filled. High apparent density and free-flowing properties. High wear resistance, high load resistance, high bend resistance.Applications: Mechanical service (e.g. bearings, mechan.. |
|||
CTE, linear | 100 µm/m-°C @Temperature 23.0 - 60.0 °C |
55.6 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
Daikin POLYFLON MG-6050 PTFE 25% Carbon Fiber Filled Molding Powder 25% carbon fiber filled. High wear resistance, high load resistance, high bend resistance.Applications: Mechanical service (e.g. bearings, mechanical seals and bearing pads)Information provided by .. |
|||
CTE, linear | 100 µm/m-°C | 55.6 µin/in-°F | |
Hippe PA 12 Nylon 12 Maintenance-free bearing and gear components under water, insulated components, seals, gear wheels. Parts for pumps and household units. Application in the electrical sector - less water absorptio.. |
|||
CTE, linear | 100 µm/m-°C | 55.6 µin/in-°F | ASTM E831 |
Addiplast Addinyl B2 R Nylon 6 High impact resistanceInformation provided by Addiplast. |
|||
CTE, linear | 100 µm/m-°C | 55.6 µin/in-°F | ISO 11359-2 |
Unitika ET2025 PA6, Dry High-impact nylonInformation provided by Unitika Ltd. |