Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 420 °F | Annealed, 0.125 in bars; ASTM D648 |
PolyOne Lubri-Tech™ PS-30GF/15T Polybutylene Terephthalate (PBT), Glass Filled, PTFE Lubricated
(discontinued Description/Features:Glass Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 420 °F | Unannealed; ASTM D648 |
PolyOne Edgetek® ES-40CF/000 Polyethersulfone - 40% Carbon Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 420 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® PET GF15 FR 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 15% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 420 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 GF35 HS L 35% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 35% Filler by WeightAdditive: Lubricant and Heat Stabilizer Features: Lubricated and Heat StabilizedProcessi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 420 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 GF50 HS UV BK 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat StabilizerFeatures: Lubricated, Good UV Resi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 420 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 GF50 L LE 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: Low Extractables and LubricatedAppearance: Natural ColorInf.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 420 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 GF55 HS L 55% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 55% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedInformati.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 420 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® PA6 CF30 TS15 BK 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant (15%) and Silicone LubricantFeatures: LubricatedAppearance: Natural ColorPro.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 420 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® PA6 GF40 ML5 HS 12 mm 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 40% Filler by WeightAdditive: Heat Stabilized and Molybdenum Disulfide LubricantFeatures: Lubricated and Heat StabilizerAp.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 420 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® PA6 GF/M50 FR 50% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 50% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 420 °F | ASTM D648 |
A. Schulman SCHULADUR® B GF15 15% Glass Fiber Reinforced PET Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 420 °F | ASTM D648 |
A. Schulman SCHULADUR® A GF50 50% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 420 °F | Unannealed, 0.125 in bars; ASTM D648 |
PolyOne Edgetek® ES-30GF/000 PES (Polyethersulfone), 30% Glass Reinforced, Hi-Temp
(discontinued **) Information provided by PolyOne™ Corporation |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 420 °F | Unannealed; ASTM D648 |
PolyOne Edgetek® PI-40CF/000 Polyetherimide (PEI), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 420 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® PA6 GF15 FR HS L 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and Lu.. |