Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C @Thickness 3.20 mm |
289 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® 4504 PPC (Asia Pacific) High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported wit.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylex® P1310G10 HB Polycarbonate, 10% Fiberglass Reinforced, UV Stabilized Information provided by Ravago. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C @Thickness 3.20 mm |
289 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® HPH4504HEU PPC (Europe-Africa-Middle East) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C @Thickness 6.40 mm |
289 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® LGK5030 PC (Asia Pacific) Glass reinforced. Flame retardant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C @Thickness 3.20 mm |
289 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone, 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubrica.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C @Thickness 3.20 mm |
289 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP DFL14 PC (Asia Pacific) LNP* LUBRICOMP* DFL14 is a compound based on Polycarbonate resin containing PTFE, Glass Fiber. Added features of this material include: Internally Lubricated. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP STAT-KON DE0069F PC LNP* STAT-KON* DE0069F is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Superior Molding. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP STAT-KON DX06500 PC (Asia Pacific) LNP* Stat-kon* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP DC006 PC (Asia Pacific) LNP THERMOCOMP* DC006 is a compound based on Polycarbonate resin containing Carbon Fiber.This product is also known as Thermocomp* DC-1006. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP DC006H PC (Asia Pacific) LNP* Thermocomp* DC006H is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP DF006 PC (Europe-Africa-Middle East) LNP* Thermocomp* DF1006 is a compound based on Polycarbonate resin containing Glass Fiber. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C @Thickness 6.40 mm |
289 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK5030 PC LNP* Thermocomp* Lexan_LGN5030 compound is a glass reinforced. Flame retardant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C @Thickness 6.40 mm |
289 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK5030 PC (Asia Pacific) Glass reinforced. Flame retardant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C @Thickness 6.40 mm |
289 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK5030 PC (Europe-Africa-Middle East) LNP* Thermocomp* Lexan_LGK5020 compound is a glass reinforced, flame retardant material. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | Annealed; ASTM D648; ISO 75-2/A |
Styron CALIBREâ„¢ 200-3 Polycarbonate Resin Overview: CALIBREâ„¢ 200-3 polycarbonate resin is produced in compliance with the US Food and Drugs Administration (FDA) and EU food contact regulation. This resin provides excellent impact resis.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | Annealed; ISO 75-2/A |
Styron CALIBREâ„¢ 201-6 Polycarbonate Resin Overview: CALIBREâ„¢ 201-6 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistance.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | annealed; ASTM D648 |
Styron EMERGEâ„¢ 8702 Polycarbonate EMERGEâ„¢ PC 8702 advanced resin is an ignition-resistant, 20% glass reinforced, polycarbonate resin. This resin contains no bromide, chloride, or phosphate additives. It is a medium flow PC re.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | ASTM D648 |
A. Schulman ComAlloy® E-14961 30% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | ASTM D648 |
A. Schulman ComAlloy® E-14961 30% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | unannealed; ISO 75 |
Chi Mei Wonderlite® PC-115 Polycarbonate Low Viscosity |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | unannealed; ISO 75 |
Chi Mei Wonderlite® PC-122 Polycarbonate High Flow |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | 0.125";; ASTM D648 |
Diamond Polymers NPP30-2000 GF30 30% Glass Filled Homopolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | ASTM D648 |
Adell BH-18 Nylon 6, 40% Mineral Filled Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | ASTM D648 |
A. Schulman ComAlloy Hiloy® 511 Polycarbonate, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.10% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | ASTM D648 |
A. Schulman ComAlloy Hiloy® 512 Polycarbonate, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | Heat Distortion temperature |
Cosmic Plastics 224 Dacron Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | ASTM D648 |
Ashley Polymers Ashlene® P1420 Polycarbonate, 20% Glass Reinforced A 20% glass reinforced polycarbonate for increased mechanical strength and thermal properties. P1423: with UV stabilizer.Data provided by the manufacturer |