| Category | Polymer , Thermoplastic , Polycarbonate (PC) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Lexan® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics Lexan® LGK5030 PC (Asia Pacific).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.61 g/cc | 1.61 g/cc | ASTM D792 |
| Water Absorption | 0.14 % <br>@Time 86400 sec |
0.14 % <br>@Time 24.0 hour |
ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.00050 - 0.0025 cm/cm <br>@Thickness 3.20 mm |
0.00050 - 0.0025 in/in <br>@Thickness 0.126 in |
SABIC Method |
| Linear Mold Shrinkage, Transverse | 0.0010 - 0.0030 cm/cm <br>@Thickness 3.20 mm |
0.0010 - 0.0030 in/in <br>@Thickness 0.126 in |
SABIC Method |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 142 MPa | 20600 psi | Type I, 50 mm/min; ASTM D638 |
| Elongation at Break | 4.0 % | 4.0 % | Type I, 50 mm/min; ASTM D638 |
| Flexural Strength | 186 MPa | 27000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
| Flexural Modulus | 10.7 GPa | 1550 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| Izod Impact, Notched | 1.22 J/cm | 2.29 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 21.6 µm/m-°C <br>@Temperature -30.0 - 30.0 °C |
12.0 µin/in-°F <br>@Temperature -22.0 - 86.0 °F |
ASTM D696 |
| CTE, linear, Transverse to Flow | 39.6 µm/m-°C <br>@Temperature -30.0 - 30.0 °C |
22.0 µin/in-°F <br>@Temperature -22.0 - 86.0 °F |
ASTM D696 |
| Deflection Temperature at 1.8 MPa (264 psi) | 143 °C <br>@Thickness 6.40 mm |
289 °F <br>@Thickness 0.252 in |
unannealed; ASTM D648 |
| Flammability, UL94 | V-1 <br>@Thickness 1.47 mm |
V-1 <br>@Thickness 0.0579 in |
UL 94 |
| V-0 <br>@Thickness 2.79 mm |
V-0 <br>@Thickness 0.110 in |
UL 94 | |
| 5VA <br>@Thickness 3.60 mm |
5VA <br>@Thickness 0.142 in |
UL 94 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength | 16.3 kV/mm <br>@Thickness 3.20 mm |
414 kV/in <br>@Thickness 0.126 in |
in oil; ASTM D149 |