Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 141 °C | 285 °F | Unannealed; ASTM D648 |
Multibase Multi-Pro® 4012 X Platinum Polypropylene Glass Fiber Reinforced, 42% by weight.Forms:PelletsProcessing Methods:Injection MoldingFeatures:Appearance, Pleasing SurfaceUses:AppliancesInformation provided by Multibase |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 141 °C | 285 °F | ASTM D648 |
Owens Corning Glass Fiber Reinforced Polycarbonate, 10 wt.% glass Data provided by the manufacturer, Owens Corning. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 141 °C | 285 °F | ASTM D648 |
Oxford Polymers PC 10GF-V0 UL Listed Polycarbonate UL Listed PolycarbonateInformation provided by Oxford Polymers. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 141 °C | 285 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® PC 04008 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation provided by TP Composite.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 141 °C | 285 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® PC SS10 FR BK 10% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 10% Filler by WeightFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation pr.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 141 °C | 285 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® TPX-PC-02071 Stainless Steel Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 141 °C | 285 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP CO GF15 CC 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: CopolymerInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 141 °C | 285 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® ABS 04002 BK 16% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 16% Filler by WeightFeatures: Flame Retardant and Electromagnetic Shielding (EMI)Appearance: BlackTPCI# 7965121I.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 141 °C | 285 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® ABS SS10 FR BK 10% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 10% Filler by WeightFeatures: Flame Retardant and Electromagnetic Shielding (EMI)Appearance: BlackInformation pr.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 141 °C | 285 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® ABS SS16 FR BK 16% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 16% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Appearance: BlackInformation provided by TP Composi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 141 °C | 285 °F | ASTM D648 |
Chase Plastics CP Pryme® PC120GR Polycarbonate, 20% Glass Fiber Reinforced, Mold Release Information provided by Chase Plastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 141 °C | 285 °F | Unannealed; ASTM D648 |
Chase Plastics CP Pryme® PC130R Polycarbonate, 30% Glass Fiber Reinforced Features: Good mold releaseForm: PelletsInformation provided by Chase Plastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 141 °C | 285 °F | ASTM D648 |
Washington Penn Homopolymer Polypropylene 27% Glass Reinforced Fiberglass & mineral-reinforced polypropylene compounds provide excellent tensile and impact properties. Mold shrinkage is similar to ABS and polystyrene. Compounds also have dimensional stability. .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 141 °C | 285 °F | ASTM D648 |
Westlake Plastics Zelux® CN-SS Polycarbonate (conductive) CN-SS is filled with small non-sloughing stainless steel fibers. Has high flexural strength and good thermal stability to 275F. The CN-SS material has excellent impact strength. Information provid.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 141 °C | 285 °F | ASTM D648 |
Polymer Resources PPX-FR6 Modified PPO, UL 94 V-0 with HDT of 300 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 141 °C | 285 °F | HDT/B; ASTM D648 |
GEHR Plastics Noryl PPO-30 GF 30% Glass Filled
(discontinued **) PPO-30 GF is reinforced with 30% glass fiber for higher thermal properties and better dimensional stability. PPO belongs to the group of the amorphous materials and can be used in temperatures rang.. |