Oxford Polymers PC 10GF-V0 UL Listed Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Molded
Manufacturer Oxford Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Oxford Polymers PC 10GF-V0 UL Listed Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
UL Listed PolycarbonateInformation provided by Oxford Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.28 g/cc
1.28 g/cc
ASTM D792
Water Absorption 0.15 %
0.15 %
ASTM D570
Linear Mold Shrinkage 0.0035 cm/cm
0.0035 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 58.6 MPa
8500 psi
ASTM D638
Elongation at Break 7.0 %
7.0 %
ASTM D638
Flexural Modulus 3.24 GPa
470 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm

@Temperature 23.0 °C
2.00 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 141 °C
285 °F
ASTM D648