Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 115 °C | 239 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYblend 85H PC/ABS-Blend Information provided by Polykemi AB |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 115 °C | 239 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Lexan® BFL4000U PC (Asia Pacific) Lexan* BFL4000U Polycarbonate resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating and good impact/flow balance. Designed fo.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 115 °C | 239 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Lexan® BFL4000U PC (Europe-Africa-Middle East) Lexan* BFL4000U Polycarbonate resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating and good impact/flow balance. Designed fo.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 115 °C | 239 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Lexan® HFD1034 PC Copolymer (Asia Pacific) 7 MFR LEXAN HFD Copolymer UV-stabilized, available in transparent colors only |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 115 °C @Thickness 3.20 mm |
239 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® HFD1034 PC Copolymer (Europe-Africa-Middle East) 7 MFR LEXAN HFD Copolymer UV-stabilized, available in transparent colors only |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 115 °C | 239 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Lexan® HFD1232 PC Copolymer (Asia Pacific) 18 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 115 °C | 239 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Lexan® HFD1711 PC Copolymer 25 MFR LEXAN High Flow Ductile Copolymer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 115 °C | 239 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Lexan® ML6413 PC Lexan* ML6413 resin is an impact modified, flame retardant polycarbonate grade with Br- & Cl-free FR systems. It features improved light shielding capability with good flow, impact and thermal prope.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 115 °C | 239 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Lexan® SLX2432D PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 115 °C | 239 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Lexan® SLX2432D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East reg.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 115 °C | 239 °F | STN EN ISO 75/A |
Plastcom SLOVALEN PH 49 GF 10 Polypropylene Homopolymer, 10% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 10% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 115 °C @Thickness 3.20 mm |
239 °F @Thickness 0.126 in |
annealed; ASTM D648 |
SABIC Innovative Plastics Lexan® BFL4000U PC Lexan* BFL4000U Polycarbonate resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating and good impact/flow balance. Designed fo.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 115 °C | 239 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Lexan® HFD1212 PC Copolymer (Asia Pacific) 18 MFR LEXAN High Flow Ductile Copolymer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 115 °C @Thickness 6.40 mm |
239 °F @Thickness 0.252 in |
ASTM D648 |
Kingfa JH960 6610 Non-halogenated Flame Retardant PC/ABS Alloy Features:Halogen free flame retardant, V-0/1.5mmExcellent balance propertiesHigh heat resistanceGood chemical resistanceGood hydrolysis resistanceSuit for paint and electo-platingDrop down resistanc.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 115 °C @Thickness 6.40 mm |
239 °F @Thickness 0.252 in |
ASTM D648 |
Kingfa PBT-T30 30% Mineral Filled PBT Features:Excellent size stabilityLow tendency to wrapLow abrasionGood surfaceApplications:Injection moldingApplication partsE & E partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 115 °C | 239 °F | ISO 75-1,-2 |
Ineos ABS Lustran® ABS 150G22 20% Glass Fiber Reinforced Grade |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 115 °C @Thickness 6.40 mm |
239 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL STN15HF PPE+PS (Asia Pacific) Automotive interiors. Improved flow characteristics/overall processing economy. 240F DTUL. High impact/good property retention after heat ageing. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 115 °C | 239 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 CM40 6122 BK 40% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackProcessing Method: Injection Mol.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 115 °C | 239 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics NORYL LTA5020 PPE+PS Noryl* LTA5020 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 115 °C | 239 °F | ASTM D648 |
Shinkong Synthetic Fibers Shinite® PP4210 PP, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 115 °C | 239 °F | ASTM D648 |
Denka MALECCA K-400 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 115 °C | 239 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® TR 90 LS PAMACM12 Product description: Grilamid TR 90 LS natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 90 LS natural contains a processing a.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 115 °C | 239 °F | |
Aclo Accutech Polypropylene Homopolymer HP0334G15M15CL Glass/Mineral Reinforced Coupled |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 115 °C | 239 °F | ISO 75 |
Azoty Tarnow™ TARNOFORM 300 M POM Tribological modified grade with addition of molybdenum disulphide, which causes decreased coefficient of friction and wear, especially for applications requiring high load at low sliding speed.Info.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 115 °C @Thickness 6.40 mm |
239 °F @Thickness 0.252 in |
Method A; ASTM D648 |
Bhansali Engineering Abstron KU660 ABS Heat Resistant Ultra Super High heat ResistantInformation provided by Bhansali |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 115 °C | 239 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer 40 MFR LEXAN High Flow Ductile Copolymer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 115 °C | 239 °F | ISO 75-1/-2 |
Mitsubishi Xantar® MX 1004 Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 115 °C | 239 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer (Europe-Africa-Middle East) 25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized |