Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ASTM D495 |
Nylene® PX3422 Nylon 6, Impact Extrusion Grade Dry as molded. Film Grade. Nylene PX3422 is a heat stabilized, high impact modified nylon resin designed for maximum toughness with minimum sacrifice in tensile strength and melting point. PX3422 .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ISO 75-1/-2 |
Quadrant EPP Borotron® UH PE-UHMW + boron based additive (ISO Data) Borotron UH and Borotron HM are boron loaded PE-(U)HMW grades, specifically developed for neutron shielding purposes in nuclear installations. The high hydrogen content of PE-(U)HMW makes it very su.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ISO 75 method A |
Quadrant EPP Cestidur™ Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ISO 75 method A |
Quadrant EPP Cestilene™ HD 1000 Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | 120°C/h; ISO 75/1 |
Polykemi AB SCANFILL BOTTLE BY45C2 Blow Molding Grade Information provided by Polykemi AB |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ISO 75-1/-2 |
Quadrant EPP TIVAR® Burnguard PE-UHMW + flame retardant + other additives (ISO Data) TIVAR Burnguard is a PE-UHMW grade containing a very effective non-halogenated flame retardant. Specifically developed to improve the poor flammability behaviour of straight forward virgin polyethyl.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ISO 75-1/-2 |
Quadrant EPP TIVAR® Cleanstat PE-UHMW + specific additives (ISO Data) TIVAR CleanStat is a PE-UHMW grade for use in food processing and pharmaceutical industries. It exhibits static dissipative properties and has a food contact compliant composition. Very good wear an.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ISO 75-1/-2 |
Quadrant EPP TIVAR® DS PE-UHMW + additives (ISO Data) TIVAR DS is a modified PE-UHMW with extremely high molecular weight. The latter in combination with a particular manufacturing process result in a PE-UHMW grade with superior wear and abrasion resis.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ISO 75-1/-2 |
Quadrant EPP TIVAR® MD PE-UHMW + metal detectable additive (ISO Data) This PE-UHMW grade with extremely high degree of polymerisation contains a metal detectable additive which does hardly affect the inherent PE-UHMW key properties. TIVAR MD presents excellent toughne.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ISO 75-1/-2 |
Quadrant EPP TIVAR® SuperPlus PE-UHMW + specific additives (ISO Data) TIVAR SuperPlus is a wear optimised, partially cross-linked PE-UHMW material with extremely high degree of polymerisation for use in most demanding applications and environments. When used for drain.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ISO 75-1/-2 |
Quadrant EPP TIVAR® TECH PE-UHMW + MoS2 (ISO Data) This PE-UHMW grade with extremely high degree of polymerisation contains molybdenum disulphide, resulting in a material with improved wear resistance and sliding properties over TIVAR 1000. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ISO 75-1/-2 |
Polymer Industries Polyslick UHMW Rod Polyslick UHMW Rod exhibits all of the durable qualities of our Polyslick UHMW Sheet making it perfect for the application where sheet stock is not suitable. The material is ideally suited for the m.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | Compression Molded; ASTM D648 |
NOVA Chemicals Surpass® RMs539-U Octene sMDPE Rotational Molding Film Features: Octene copolymerExceptional low temperature impact propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Stan.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ISO 75-1/-2 |
Polymer Industries Polyslick UHMW Profile Polyslick UHMW Profiles exhibit all of the durable qualities of our Polyslick UHMW Sheet making them perfect for use where sheet stock is not suitable. Polymer Industries offers a large variety of p.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ASTM D 648 |
NOVA Chemicals Novapol® TR-0535-UIG Hexene MDPE Rotational Molding Resin TR-0530-UIG complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. TR-0530-UIG is .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 - 47.0 °C | 108 - 117 °F | Average value: 44.3 °C Grade Count:51 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | |
LyondellBasell Lupolen® 5261 ZS HDPE, Blow Molding Grade Relatively high viscosity blow molding grade (similar to Lupolen 5261 Z), but more resistant to stress cracking) for rigid, stackable and highly shock resistant containers for packaging all types of.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ISO 75 |
GEHR Plastics PE-UHMW Polyethylene, Ultra High Molecular Weight The ultra high molecular weight Polyethylene has a high abrasion resistance and a high toughness at the same time. The chemical and the crack resistance are optimized in comparison to the standard P.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ASTM D 648 |
Shakespeare Isocorâ„¢ SVP4011 high viscosity PA-6/69 Isocorâ„¢ 4011 is a high viscosity PA-6/69. This resin is specifically suited for applications requiring superior toughness and abrasion resistance. Isocorâ„¢ 4011 is also used in applicat.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 - 43.0 °C | 108 - 109 °F | UV Postcure; ASTM D648-98c |
DSM Somos® WaterClear® Ultra 10122 Optically Clear, Colorless, Rigid, Stereolithography Resin DescriptionDSM Somos® WaterClear Ultra 10122 is a next generation optically clear resin with ABS like properties and good temperature resistance. It produces colorless, functional, accurate parts .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ISO-R 75 Method A |
Hippe PE 1000 Polyethylene Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 - 49.0 °C | 108 - 120 °F | ISO-R 75 Method A |
Hippe PE 300 Polyethylene Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ASTM D648 |
3D Systems Accura® Xtreme White 200 Plastic Ultra tough white plastic to replace CNC Machined polypropylene and ABS articles FeaturesExceptionally tough and durableUsed for challenging functional assembliesUsed for snap fit assembl.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ASTM D648 |
ExxonMobil Escorene® HD-8760 HDPE, Rotational Molding Pellets
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated UV-8 type protection, Higher stiffness, Good flowUses: Recreational products, Industrial components, RV tanks |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ASTM D648 |
ExxonMobil Escorene® HD-8660 LHDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.HD-8600 series are linear high density polyethylene resins that provide outstanding environmental stress crack resistance. HD-8660 is fully formula.. |