Shakespeare Isocorâ„¢ SVP4011 high viscosity PA-6/69

Category Polymer , Thermoplastic , Nylon , Nylon 6/69
Manufacturer Shakespeare Company
Trade Name Isocor™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shakespeare Isocorâ„¢ SVP4011 high viscosity PA-6/69.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Isocorâ„¢ 4011 is a high viscosity PA-6/69. This resin is specifically suited for applications requiring superior toughness and abrasion resistance. Isocorâ„¢ 4011 is also used in applications requiring good electrical insulation properties using conventional techniques. Used for cable jacketing, film extrusions, monofilaments / bristles, impact modifier, electrical connectors, and trimmer line.Information provided by Shakespeare Company.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ASTM D 792
Water Absorption 3.7 %
3.7 %
24 hour immersion; ASTM D 570
Linear Mold Shrinkage 0.014 cm/cm

@Thickness 3.17 mm
0.014 in/in

@Thickness 0.125 in
Mechanical Properties Metric English Comments
Hardness, Shore D 79
79
ASTM D 2240
Tensile Strength at Break 39.3 MPa
5700 psi
ASTM D 638
Elongation at Break 300 %
300 %
ASTM D 638
Flexural Modulus 0.634 GPa
92.0 ksi
ASTM D 790
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D 256
Thermal Properties Metric English Comments
Melting Point 200 °C
392 °F
DSC
Deflection Temperature at 0.46 MPa (66 psi) 141 °C
286 °F
ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 42.0 °C
108 °F
ASTM D 648