Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 37.8 °C | 100 °F | ASTM D648 |
RheTech Products FT1100-689UV Thermoplastic Polyolefin, UV Stabilized, Light Natural Beige Applications: Pillar plugsAirbag doorsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
ExxonMobil LL 8455.24 Rotational Molding Resin
(discontinued **) LL 8450 is a linear low density butene copolymer designed to offer excellent processability, whiteness and fast grinding rate. This resin is ideally suited for applications that require excellent di.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
ExxonMobil LLP8455.24 Rotational Molding Resin
(discontinued **) LL 8450 is a linear low density butene copolymer designed to offer excellent processability, whiteness and fast grinding rate. This resin is ideally suited for applications that require excellent di.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
ExxonMobil Escorene® LL-8555 LLDPE, Rotational Molding Pellets
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated, UV-4 type protection, High flowUses: Consumer items, Toys, Food storage bins |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
ExxonMobil Escorene® LL-8556 LLDPE, Rotational Molding Powder
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated, UV-4 type protection, High flowUses: Consumer items, Toys, Food storage bins |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
ExxonMobil HD 6605.29 Injection Molding Resin
(discontinued **) HD 6605 is a narrow molecular weight hexene copolymer designed for a wide range of injection molding applications, offering excellent ESCR with good stiffness-toughness balance. Ideally suited for .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
ExxonMobil HD 6714.17 Injection Molding Resin
(discontinued **) HD 6714 is a narrow molecular weight hexene copolymer designed for outstanding processability to maximize injection molding productivity. This resin is ideally suited for thin wall multicavity part.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
NOVA Chemicals Novapol® TR-0338-UI Hexene MDPE Rotational Molding Resin Excellent low temperature impact properties, Excellent ESCR, Good stiffness, Wide processing windowApplications: General purpose custom molding, Chemical containers, IBCs, Fish boxes, Septic tanks, .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
ExxonMobil Escorene® LX-0252 LMDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A linear medium density polyethylene providing an excellent processing window for molding toys and consumer items. The resin is formulated to provi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | |
LyondellBasell Lupolen® 3821 D MDPE Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 37.8 °C | 100 °F | ASTM D648 |
Spartech PP7210 Calcium Carbonate Filled High Impact Copolymer Provides the highest level of impact of all copolymers and are useful in applications where improved processing and stiffness are required versus unfilled copolymer materials.Information provided by.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C @Thickness 3.20 mm |
100 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP TH0300A PUR LNP THERMOCOMP* TH0300A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
ExxonMobil HD 6719.17 Injection Molding Resin Product Description: HD 6719 is a narrow molecular weight hexane copolymer designed for a wide rage of injection molding applications, combining easy processability with good toughness properties. I.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
ExxonMobil HD 6719.62 Injection Molding Resin Product Description: HD 6719 is a narrow molecular weight hexane copolymer designed for a wide rage of injection molding applications, combining easy processability with good toughness properties. I.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
ExxonMobil LL 8450.31 Rotational Molding Resin Product Description: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. They are ideally suited for applications that require.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
ExxonMobil LL 8555.24 Rotational Molding Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
ExxonMobil LL 8555.25 Rotational Molding Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 37.8 °C | 100 °F | ASTM D648 |
ExxonMobil LLDPE LLP 8555.24 Linear Low Density Polyethylene Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 37.8 °C | 100 °F | ASTM D648 |
ExxonMobil LLDPE LLP 8555.25 Linear Low Density Polyethylene Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
ExxonMobil LLP8450.31 Rotational Molding Resin LProduct Description: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. They are ideally suited for applications that requir.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
ExxonMobil LLP8555.24 Rotational Molding Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 37.8 °C | 100 °F | ASTM D648 |
Clariant 6008 L Nylon 6, High Impact, Injection Molding Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
ExxonMobil HD 6605.70 Injection Molding Resin Product Description: HD 6605.70 is a narrow molecular weight hexane copolymer designed for a wide range of injection molding applications, offering excellent ESCR with good stiffness-toughness balan.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
ExxonMobil HD 6733.17 Injection Molding Resin Product Description: HD 6733 is a narrow molecular weight hexane copolymer designed to maximize injection molding speed and productivity in thing wall articles. Lower processing temperatures enable .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 - 55.0 °C | 100 - 131 °F | ASTM D648 |
Arkema Group KYNAR FLEX® 2850 Black Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 - 55.0 °C | 100 - 131 °F | ASTM D648 |
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 - 101 °C | 100 - 214 °F | Average value: 67.4 °C Grade Count:4 |
Overview of materials for Low Density Polyethylene (LDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
ExxonMobil Escorene® LL-8556 LMDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A linear medium density polyethylene having improved flow characteristics vs. LL-8300's series resins, yet retaining outstanding whiteness and a goo.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 37.8 - 125 °C | 100 - 257 °F | Average value: 61.7 °C Grade Count:22 |
Overview of materials for Polypropylene with 10% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |