Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 - 146 °C | 210 - 295 °F | Average value: 108 °C Grade Count:22 |
Overview of materials for Polycarbonate/ABS Alloy, NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, NCG Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | Annealed, 0.125 in bars; ASTM D648 |
PolyOne Lubri-Tech™ AS-15CF/15T Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced, PTFE Lubricated
&nb Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | Annealed, 0.125 in bars; ASTM D648 |
PolyOne Edgetek® AS-20GF/000 HI UV NAT Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **)& Description/Features:Glass Fiber ReinforcedHigh ImpactUV StabilizedNaturalUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 - 132 °C | 210 - 270 °F | Average value: 112 °C Grade Count:5 |
Overview of materials for Polytetrafluoroethylene (PTFE), Mica Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Mica Filled". Each property range of values reported is minimum and maxi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylon® N1000MDL Nylon 6/6
(discontinued **) Available in North America Additive: Molybdenum Disulfide Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedForm: Pellets Information provided by Ravago. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 - 227 °C | 210 - 440 °F | Average value: 201 °C Grade Count:13 |
Overview of materials for Nylon 610, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® PA6 ML2 Nylon 6 Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide Lubricant(2%)Features: Good Wear Resistance, Low Friction and LubricatedInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® POM CO TS20 Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%) and Silicone LubricantFeatures: Lubricated, Good Wear Resistance and CopolymerInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PC/ABS FR 1950 BK Availability: North AmericaForms: PelletsFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | Unannealed; ASTM D648 |
Techmer ES Statiblend® POM CO AS Availability: North AmericaForms: PelletsAdditive: AntistaticFeature: Antistatic and ConductiveTPCI# 60000114Information provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | Annealed; ASTM Data |
Styron Magnum™ 555 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | Annealed; ASTM Data |
Styron Magnum™ 800 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® ABS HI 350 High Impact Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Density and High Impact ResistanceProcessing Method: Injection MoldingInformation provided by .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | Unannealed; ASTM D648 |
Chase Plastics CP Pryme® A110 ABS, 10% Glass Fiber Reinforced Features: Glass fiber reinforcementInjection moldingForm: PelletsInformation provided by Chase Plastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ABS TM 25 Description: Heat Resistant Grade, Very High HeatInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | 0.125 in bar Unannealed/Conditioned 40 hours at 23°C; ASTM D648 |
Diamond Polymers ABS/PC FC-30 Description: Injection Molding Grade, High Impact, Flame RetardantInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | ASTM D648 |
Asahi Kasei Thermofil P-40TC-0158 40% Talc Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | ASTM D648 |
Quadrant EPP Sanalite® PP, Homopolymer Polypropylene Cutting Board (FDA, USDA, & NSF) (ASTM Product Data Sheet) |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | ASTM D648 |
Quadrant EPP Semitron® ESd 500 HR PTFE, static dissipative, compression molded (ASTM Product Data Sheet) |