Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 81.1 °C | 178 °F | ASTM D648 |
RheTech Products F36-01 35% Mica Reinforced Polypropylene Copolymer, Black Applications: Cowl screensHVAC ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.1 °C @Thickness 6.35 mm |
178 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne LubriOne™ AT-000/18T 2S Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.1 °C | 178 °F | 0.125 in bar, Unannealed/Conditioned 48 hours; ASTM D648 |
Network Polymers NPP 808 C3WW Description: Polycarbonate AlloyInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.1 °C | 178 °F | 0.125 in bar, Unannealed/Conditioned 48 hours; ASTM D648 |
Network Polymers NPP 808 C5WW Description: Polycarbonate AlloyInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.1 °C | 178 °F | Annealed; ASTM D648 |
Network Polymers NPS 90-0802 Polystyrene Description: Injection Molding Grade, High ImpactInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.1 °C | 178 °F | Annealed; ASTM D648 |
Network Polymers NPS 90-0827 Polystyrene Description: Injection Molding Grade, High ImpactInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.1 °C | 178 °F | ASTM D648 |
Oxford Polymers INJ-FR Glass Fiber Reinforced ABS, Flame Retardant Glass Fiber Reinforced ABS, Flame RetardantInformation provided by Oxford Polymers. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.1 °C | 178 °F | ASTM D648 |
Network Polymers 702 Polystyrene Description: Ignition RetardantInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.1 - 121 °C | 178 - 250 °F | Average value: 103 °C Grade Count:14 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant". Each property range of valu.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.1 °C | 178 °F | ASTM D648 |
I. Stern 550 High Impact Polystyrene Features:Good process propertiesExcellent toughness and environmental stress crackingApplicationsStructural foamDisplaysSmall appliancesAgency RatingsFDA Title 21 CFR 177.1640UL File E220962Informat.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.1 °C | 178 °F | ASTM D648 |
Ineos Styrenics 473D High-Impact Polystyrene Resin (NAFTA) Description: High-impact, high-flow grade for a wide variety of applications, including appliance components, consumer electronics housings, magnetic and optical media, building and construction, pa.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.1 °C | 178 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® ABS FR Availability: North AmericaForms: PelletsFeatures: Flame RetardantTPCI# 1039121Information provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.1 °C | 178 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® ABS FR BK Availability: North AmericaForms: PelletsFeatures: Flame RetardantAppearance: BlackTPCI# 9224121Information provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.1 °C | 178 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® ABS FR UV Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame RetardantUL File Number: E157318Information provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.1 °C | 178 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® ABS FR UV BK Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame Retardant and Good UV ResistanceUL File Number: E157318Appearance: BlackTPCI# 9224121Information provided by TP Compos.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.1 °C | 178 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® ABS FR V2 BK Availability: North AmericaForms: PelletsFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.1 °C | 178 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS E Availability: North AmericaForms: PelletsFeatures: High ViscosityProcessing Method: Blow Molding and ExtrusionInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.1 °C | 178 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS HH BK MB Availability: North AmericaForms: PelletsFeatures: High Gloss and High Heat ResistanceAppearance: BlackProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.1 °C | 178 °F | Annealed; ASTM D648 |
American Polymers API 650-21 Polystyrene API 650-21 has been developed for injection molding applications that need a higher degree of toughness and gloss than conventional polystyrene. This polymer approaches ABS type properties.Applicat.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.1 °C | 178 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ASA S140 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.1 °C | 178 °F | ASTM D648 |
Clariant 6602-L BK-02 Nylon 66, Lubricated, Nucleated, Weather Resistant, Black Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.1 °C | 178 °F | ASTM D648 |
Clariant BRU2000 Nylon 66, Lubricated, Nucleated, Weather Resistant, Black Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.1 °C | 178 °F | ASTM D648 |
Clariant Renol 6602-L Nylon 66, Internally Lubricated Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.1 °C | 178 °F | |
Aclo Accutech Polypropylene Homopolymer HP0336M40L Mica Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.1 °C | 178 °F | ASTM D648 |
Americas Styrenics EA6740 High Impact Polystyrene Product CharacteristicsVery good printabilityMatte surface finishHigh heat distortion temperatureGood low temperature toughnessFood Contact CompliantTypical ApplicationsPackaging and one-time use it.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.1 °C | 178 °F | |
Aclo Accutech Polypropylene Homopolymer HP0339M40L Mica Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.1 °C | 178 °F | ASTM D648 |
Americas Styrenics STYRON® 487 High Impact Polystyrene Product CharacteristicsGood TrimmabilityToughnessHeat resistanceFood Contact CompliantUL Classification 94HBTypical ApplicationsLidsAppliancesPackaging/disposablesHousewaresInformation provided by A.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.1 °C | 178 °F | Annealed; ASTM D648 |
American Polymers API 550 Polystyrene API 550 is a high impact grade of polystyrene. It is characterized by good impact and processability.Applications: API 550 is widely used in housewares, toys, containers, appliance parts, speaker h.. |