Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C | 163 °F | ASTM D-648 |
Plaskolite Optix® CA - 41 FDA General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C | 163 °F | ASTM D-648 |
Plaskolite Optix® CA - 41 UVA General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C | 163 °F | ASTM D-648 |
Plaskolite Optix® CA - 41 UVT General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C | 163 °F | ASTM D-648 |
Plaskolite Optix® CA - 41 UVT LL General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C @Thickness 3.18 mm |
163 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion 6935 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C @Thickness 3.18 mm |
163 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion 85857 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C @Thickness 3.18 mm |
163 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion 8700A Polyvinyl Chloride, Rigid (PVC, Rigid) Note: Automotive OEM approval(s). Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was de.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C @Thickness 3.18 mm |
163 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion 87416 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C @Thickness 3.18 mm |
163 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion L4857 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C | 163 °F | ASTM D-648 |
Plaskolite West Optix® CA - 41 FDA General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C @Thickness 3.18 mm |
163 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion L7416 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C | 163 °F | ASTM D-648 |
Plaskolite West Optix® CA - 41 UVT LL General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C @Thickness 3.18 mm |
163 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion L9620 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C | 163 °F | ASTM D-648 |
Plaskolite West Optix® CP - 41 UVA General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C @Thickness 3.18 mm |
163 °F @Thickness 0.125 in |
Annealed; ASTM D648 |
PolyOne Edgetek® NN-35MG/000 Black v1.1 Polyamide 66 (Nylon 66) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C @Thickness 3.18 mm |
163 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Dry Blend E7755 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C | 163 °F | ASTM D-648 |
Plaskolite West Optix® CA - 41 UVA General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C | 163 °F | ASTM D-648 |
Plaskolite West Optix® CA - 41 UVT General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C | 163 °F | Unannealed; ASTM Data |
Americas Styrenics Styron® 678C Polystyrene
(discontinued **) STYRON® 678C general purpose polystyrene resin is a high flow, medium strength resin with good scuff resistance. It is typically used in thin-wall or consumer electronic applications. When used unm.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C | 163 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylac® FR134 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C | 163 °F | Unannealed (0.250"); ASTM D648 |
LTL Color Compounds ColorFast® FRA205 ABS Flame-retarded V0, high gloss ABS with superior UV stabilityAll information provided by LTL Color Compounders, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C | 163 °F | ISO 75-2/A |
ExxonMobil Exxtral™ CNU 011 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for injection molded automotive interior applications in which good surface finish and UV resistance is required. Availabilit.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C | 163 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers TR 5000 Description: Transparent ABSInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C | 163 °F | |
Aclo Accucomp ABS ABS811L Medium Impact Grade |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C | 163 °F | |
Aclo Accucomp ASA ASA001L |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C | 163 °F | |
Aclo Accutech Polypropylene Homopolymer HP0336W30L Wollastonite Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C | 163 °F | annealed; ASTM D-648 |
Axiall 3605 Rigid PVC, Extrusion, White Georgia Gulf 3605 is a special purpose compound formulated for the extrusion of thin wall profiles such as edge banding and furniture trim.Information provided by Georgia GulfGeorgia Gulf became Axi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C | 163 °F | |
Aclo Accucomp ABS ABS804L High Impact Grade |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C | 163 °F | |
Aclo Accutech Polypropylene Copolymer CP0436M40L Mica Reinforced |