Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 43.9 °C | 111 °F | Unannealed; ISO 75A-1, -2 |
LyondellBasell Hifaxâ„¢ ETA3081HS Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ ETA3081HS medium melt flow, 800 MPa flexural modulus, paintable thermoplastic elastomeric olefin (TEO) resin has balanced physical properties, moldability and paintability. .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 43.9 °C | 111 °F | Unannealed; ISO 75A-1, -2 |
LyondellBasell Hifaxâ„¢ RTA3263EUV/1 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ RTA3263EUV/1 fractional melt flow, 1,700 MPa flexural modulus, UV-stabilized, mineral-filled, extrusion grade thermoplastic elastomeric olefin (TEO) resin has an excellent b.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 43.9 °C | 111 °F | ISO 75-2/A |
ExxonMobil Exxtral™ BNT 010 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for automotive exterior painted parts such as bumper fascia.Availability: Africa & Middle East, Asia Pacific, Europe, South A.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 43.9 °C | 111 °F | ISO 75-2/A |
ExxonMobil Exxtral™ BNT 011 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin with good UV resistance designed for automotive exterior parts such as bumper fascia.Availability: Africa & Middle East, Asia Pacific,.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 43.9 °C | 111 °F | |
Aclo Accucomp Polyethylene HD0202L High Density |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 43.9 °C | 111 °F | |
Aclo Accucomp Polypropylene CPO407L Copolymer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 43.9 - 92.8 °C | 111 - 199 °F | Average value: 57.1 °C Grade Count:47 |
Overview of materials for Ethylene Butyl Acrylate This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Butyl Acrylate". Each property range of values reported is minimum and maximum values of approp.. |