Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer |
Manufacturer | Aclo Compounders |
Trade Name | Accucomp |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | Aclo Accucomp Polypropylene CPO407L Copolymer.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D792 |
Linear Mold Shrinkage | 0.012 cm/cm | 0.012 in/in | MD; ASTM D955 |
Melt Flow | 20 g/10 min | 20 g/10 min | ASTM D1238 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Rockwell R | 60 | 60 | ASTM D785 |
Tensile Strength at Break | 13.0 MPa | 1890 psi | ASTM D638 |
Tensile Strength, Yield | 18.0 MPa | 2610 psi | ASTM D638 |
Elongation at Break | 60 % | 60 % | ASTM D638 |
Elongation at Yield | 6.0 % | 6.0 % | ASTM D638 |
Tensile Modulus | 0.800 GPa | 116 ksi | ASTM D638 |
Flexural Strength | 21.0 MPa | 3050 psi | ASTM D790 |
Flexural Modulus | 0.800 GPa | 116 ksi | ASTM D790 |
Izod Impact, Notched | 6.73 J/cm | 12.6 ft-lb/in | ASTM D256 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 62.8 °C | 145 °F | ASTM D648 |
Deflection Temperature at 1.8 MPa (264 psi) | 43.9 °C | 111 °F |