ExxonMobil Exxtral™ BNT 010 Performance Polyolefin

Category Polymer , Thermoplastic , Ethylene Butyl Acrylate
Manufacturer Exxon Chemical
Trade Name Exxtral™
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF ExxonMobil Exxtral™ BNT 010 Performance Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: A specialty thermoplastic polyolefin resin designed for automotive exterior painted parts such as bumper fascia.Availability: Africa & Middle East, Asia Pacific, Europe, South America and North America Features: Balanced Stiffness/ToughnessDuctileGood ColorabilityHigh Impact ResistanceLow Temperature Impact ResistancePaintableUses: Automotive ApplicationsAutomotive Exterior PartsAutomotive Exterior Trim Processing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 13.0 MPa
1890 psi
ISO 527-2/50
Tensile Strength, Yield 17.0 MPa
2470 psi
ISO 527-2/50
Elongation at Break >= 50 %
>= 50 %
ISO 527-2/50
Elongation at Yield 6.0 %
6.0 %
ISO 527-2/50
Flexural Modulus 0.903 GPa
131 ksi
Secant; ISO 178
Charpy Impact, Notched 1.09 J/cm²

@Temperature -30.0 °C
5.20 ft-lb/in²

@Temperature -22.0 °F
Partial Break; ISO 179
1.49 J/cm²

@Temperature 0.000 °C
7.10 ft-lb/in²

@Temperature 32.0 °F
Partial Break; ISO 179
6.51 J/cm²

@Temperature 22.8 °C
31.0 ft-lb/in²

@Temperature 73.0 °F
Partial Break; ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 43.9 °C
111 °F
ISO 75-2/A